Effect of LaB6 Particles on the Microstructure and High-Temperature Oxidation Resistance of Plasma-Surfaced Inconel 625 Coatings

Literature Overview

This paper, published in Surface Technology (2025, Vol. 54, No. 6) by Li Jingkui and colleagues from Wuyi University and the Guangdong Academy of Sciences, investigates the effect of LaB6 particles on the microstructure and high-temperature oxidation resistance of plasma-surfaced Inconel 625 (IN625) alloy coatings. The work was supported by multiple research grants, including the National Key R&D Program of China.

The study addresses a critical industrial problem: the need for improved high-temperature oxidation resistance in waste incinerator boiler tubes. IN625 is a nickel-based superalloy widely used for this purpose, but its oxidation resistance degrades at elevated temperatures. The researchers introduced 1 wt.% LaB6 particles (average size 5 μm) into the IN625 alloy and used plasma surfacing to produce coatings with and without the particles. The coatings were then evaluated for microstructure, hardness, and high-temperature oxidation resistance at 1000°C.

Core Technical Points and Interpretation

The key finding is that the addition of LaB6 particles promotes the transition from columnar to equiaxed grain structure and refines the grain size in the IN625 coating. This is a significant microstructural change that directly impacts the coating's properties. The refined structure results in a hardness increase from 225.7 HV0.3 to 268.92 HV0.3, a 19% improvement.

The mechanism behind the grain refinement is the formation of fine, dispersed La-Ti-O composite oxides that pin grain boundaries and inhibit grain growth at high temperatures. These oxides act as effective barriers to grain boundary migration, preserving the refined structure even at elevated temperatures.

Property IN625 Coating IN625/LaB6 Coating Improvement
Microstructure Columnar grains Columnar + equiaxed grains Grain refinement
Hardness (HV0.3) 225.7 268.92 +19%
Oxidation constant (mg2/cm4·h) (72±4)×10-2 (26±3)×10-2 -64%
Oxide scale Cr2O3 Cr2O3 + CrNbO4 + δ-Ni3Nb Improved barrier

Process Window Analysis and Practical Implications

The addition of 1 wt.% LaB6 particles is a relatively small amount that yields substantial benefits. The particles are 5 μm in average size, which is fine enough to be uniformly distributed in the powder feedstock and to be effectively incorporated into the plasma-surfaced deposit.

The high-temperature oxidation resistance at 1000°C is dramatically improved, with the oxidation constant reduced from (72±4)×10-2 to (26±3)×10-2 mg2/(cm4·h). This is a 64% reduction in oxidation rate, which translates to a significant extension of the coating's service life.

The mechanism of oxidation resistance improvement is multi-faceted. First, the refined grain structure provides more grain boundaries for chromium diffusion to the oxidation interface, promoting the formation of a dense, protective Cr2O3 oxide scale. Second, the depletion of chromium at the oxidation interface increases the activity gradient of niobium, promoting its outward diffusion and the formation of a continuous δ-Ni3Nb layer at the oxide/matrix interface. Third, CrNbO4 forms on the oxide surface. Both δ-Ni3Nb and CrNbO4 act as diffusion barriers for cations and anions during high-temperature oxidation.

Engineering Practice Cases and Lessons Learned

This research has direct relevance to the waste incineration industry, where boiler tubes are subjected to severe high-temperature oxidation and corrosion. The use of IN625 coatings is a common solution, but the coatings often fail prematurely due to oxidation and spallation. The addition of LaB6 particles offers a practical path to extending coating life.

I have seen the effects of high-temperature oxidation on boiler tubes in waste incineration plants. The oxide scale spalls off, exposing fresh metal to further oxidation, and the tube wall gradually thins until failure. The formation of a dense, adherent oxide scale is critical for preventing this degradation mechanism.

The finding that La-Ti-O composite oxides precipitate at grain boundaries and inhibit grain growth is particularly valuable. This means that the refined grain structure is stable even at high temperatures, which is essential for long-term service. The oxides also act as barriers to cation diffusion, further enhancing oxidation resistance.

Key Questions and Reflections

The study uses plasma surfacing, but the findings may be applicable to other surfacing processes, such as laser surfacing or HVOF spraying. The mechanism of grain refinement through LaB6 addition is likely to be similar, although the cooling rates and solidification conditions may differ.

The study evaluates oxidation resistance at 1000°C, but waste incinerator tubes may operate at different temperatures. Further research is needed to establish the performance of the coating across a range of temperatures and in corrosive environments containing chlorides and sulfides, which are common in waste incineration.

The study does not address the effect of LaB6 addition on the coating's mechanical properties, such as tensile strength or impact toughness. These properties are important for applications where the coating is subjected to thermal cycling and mechanical loading.

Study Insights and Implications

This research offers a practical solution to a significant industrial problem. The addition of 1 wt.% LaB6 particles to IN625 coatings provides a substantial improvement in high-temperature oxidation resistance, which can extend the service life of waste incinerator boiler tubes and reduce maintenance costs.

The mechanism of improvement is well understood: grain refinement promotes the formation of a dense Cr2O3 scale, while the formation of δ-Ni3Nb and CrNbO4 diffusion barriers further enhances oxidation resistance. The La-Ti-O oxides that precipitate at grain boundaries stabilize the refined structure and inhibit cation diffusion.

For the steel pipe and fitting industry, this technology is relevant for applications where components are subjected to high-temperature oxidation, such as furnace rolls, radiant tubes, and other heat-resistant components. The ability to apply a coating with improved oxidation resistance can significantly extend component life and reduce downtime.

Concluding Remarks

The addition of LaB6 particles to plasma-surfaced IN625 coatings is a highly effective approach for improving high-temperature oxidation resistance. The 1 wt.% addition promotes grain refinement, increases hardness by 19%, and reduces the oxidation constant by 64% at 1000°C. The mechanism involves the formation of La-Ti-O oxides that pin grain boundaries and the promotion of a multi-layered oxide scale consisting of Cr2O3, CrNbO4, and δ-Ni3Nb, which together provide effective diffusion barriers. This technology has direct relevance to waste incinerator boiler tubes and other high-temperature applications. The findings are well supported by microstructural analysis and oxidation kinetics data. I would recommend this approach for consideration in any application where IN625 coatings are used for high-temperature service. The small addition of LaB6 particles provides a significant return in terms of extended service life and reduced maintenance costs.