Cavitation erosion is a serious problem in hydroelectric turbines, particularly in the runner blades of Francis and Kaplan turbines. The high-velocity water flow causes the formation and collapse of vapour bubbles, which creates high-pressure shock waves that erode the blade surface. The erosion typically occurs in the lower half of the blade, where the water velocity is highest and the pressure is lowest. Over time, cavitation erosion can significantly reduce the efficiency of the turbine and eventually lead to blade failure.

The paper by Hu Dong and Lan Jian from Wuhan University of Technology addresses the repair of cavitation-eroded 0Cr13Ni5Mo martensitic stainless steel turbine blades using RMD650 alloy wire with arc welding. The authors studied the microstructure and properties of single-layer and 15-layer hardfacing deposits, and evaluated their cavitation erosion resistance.

Welding Parameters and Process Considerations

The authors used the following welding parameters for the hardfacing:

Parameter Value
Welding voltage 18.8 V
Welding current 240 A
Torch travel speed 10 mm/s
Wire feed speed 4.5 m/min
Shielding gas Argon (typical for GMAW)

These parameters are typical for gas metal arc welding (GMAW) of stainless steel. The relatively low voltage and current suggest that the process was operated in the short-circuit transfer mode, which is suitable for thin deposits and good control of the weld pool. The travel speed of 10 mm/s is relatively fast, which results in a thin deposit per pass. This is important for controlling dilution and heat input.

From my experience, the repair of turbine blades requires careful attention to the following:

  1. The damaged area must be ground or machined to remove all cavitation-eroded material and any cracks.
  2. The base metal must be preheated to prevent cracking, especially if the blade is thick.
  3. The welding parameters must be controlled to minimise distortion.
  4. The repair must be inspected for defects before returning the turbine to service.

Microstructure Evolution in Single-Layer and Multi-Layer Deposits

The paper reports that the single-layer deposit had columnar prior austenite grains, while the 15-layer deposit had equiaxed prior austenite grains. This is an interesting finding that has implications for the mechanical properties of the deposit.

In the single-layer deposit, the solidification begins at the fusion line and grows epitaxially from the base metal. The grains grow in a columnar fashion, perpendicular to the fusion line. In the multi-layer deposit, each subsequent layer is deposited on top of the previous one, and the heat input from the subsequent layers causes recrystallisation and grain refinement. This results in an equiaxed grain structure in the top layers.

The authors also found that the cooling rate during welding affects the morphology of the prior austenite grains but has little effect on the final martensite formation and its size. This is a significant finding, as it suggests that the welding parameters can be varied to control the grain size without affecting the martensite transformation.

Hardness and Cavitation Erosion Resistance

The paper reports that the 15-layer deposit had higher hardness than the single-layer deposit. The hardness variation was attributed to changes in dislocation density, as confirmed by kernel average misorientation (KAM) analysis. The higher dislocation density in the multi-layer deposit is likely due to the repeated thermal cycles and the associated strain hardening.

The cavitation erosion test showed that the 15-layer deposit had better cavitation erosion resistance than the single-layer deposit. This is consistent with the higher hardness of the multi-layer deposit, as hardness is a key factor in cavitation erosion resistance. The harder the material, the more resistant it is to the high-pressure shock waves generated by cavitation bubble collapse.

Practical Implications for Turbine Blade Repair

The results of this study have significant practical implications for the repair of hydroelectric turbine blades. The key findings are:

  1. Multi-layer hardfacing deposits have better cavitation erosion resistance than single-layer deposits.
  2. The hardness of the deposit increases with the number of layers, due to increased dislocation density.
  3. The welding parameters can be varied to control the grain size without affecting the martensite transformation.
  4. The RMD650 wire is suitable for repairing cavitation-eroded 0Cr13Ni5Mo turbine blades.

From my experience, the repair of turbine blades is a critical operation that requires a high level of skill and quality control. The blades operate under high stress and in a corrosive environment, and a poor repair can lead to premature failure. The use of RMD650 wire and the welding parameters described in the paper provide a good starting point for the repair process.

However, there are some practical considerations that are not covered in the paper:

  1. The repair must be followed by post-weld heat treatment to relieve residual stresses.
  2. The repaired area must be inspected using non-destructive testing methods such as ultrasonic testing or dye penetrant testing.
  3. The surface finish of the repaired area must be smooth to prevent cavitation from occurring at the repair interface.

Conclusion and Lessons Learned

The paper by Hu Dong and Lan Jian provides valuable insight into the repair of cavitation-eroded martensitic stainless steel turbine blades. The key findings are that multi-layer deposits have better cavitation erosion resistance than single-layer deposits, and that the hardness of the deposit increases with the number of layers. The RMD650 wire is a suitable filler material for this application.

From a practical standpoint, the repair of turbine blades is a challenging operation that requires careful process control and quality assurance. The welding parameters described in the paper provide a good baseline, but the actual parameters must be adjusted based on the specific blade geometry and the extent of the damage. The most important lesson is that the repair must be performed by skilled welders who understand the metallurgy of the base metal and the filler material.

In the hydroelectric industry, cavitation erosion is a constant challenge, and the ability to repair damaged blades effectively is essential for maintaining turbine efficiency and extending the life of the equipment. This paper provides a solid foundation for developing a reliable repair process, and I would recommend it to any engineer involved in turbine maintenance or repair. The combination of microstructural analysis and cavitation erosion testing is particularly valuable, as it provides both theoretical understanding and practical validation of the repair process.