Multi-Functional Roll Body Surfacing Device: A Veteran's Review of Its Application in Rolling Mills
Overview of the Device and Its Role
The 2005 paper from Baosteel Meishan Iron and Steel, published in Welding, describes a multi-functional roll body surfacing device that integrates preheating, surfacing, interlayer temperature control, and post-weld heat treatment in a single compact unit. This is a significant development for rolling mills, where rolls are subject to severe wear and thermal fatigue. The device was applied at the Meishan rolling mill and reported to perform well, requiring only a modest investment. From my perspective, the key value of this device is not just the surfacing capability, but the integration of the thermal management functions that are essential for producing a sound, crack-free hardfaced layer on a large roll body.
Key Technical Features and Process Integration
The device addresses the three critical thermal challenges in roll surfacing: preheating to reduce the temperature gradient and prevent cracking, interlayer temperature control to maintain a consistent deposition temperature and avoid overheating, and post-weld heat treatment to relieve residual stresses and temper the hardfaced layer. The integration of these functions into one unit eliminates the need for separate equipment, reduces handling, and ensures that the thermal cycle is controlled from start to finish. The paper does not provide detailed specifications, but based on typical designs, the device likely uses induction heating for preheating and post-weld heat treatment, and resistance or induction heating for interlayer temperature maintenance. The surfacing process itself is likely submerged arc welding or electroslag surfacing, both of which are well suited to large roll bodies.
| Function | Purpose | Typical Parameters |
|---|---|---|
| Preheating | Reduce thermal gradient, prevent cold cracking | 150 to 300°C, depending on roll material and diameter |
| Surfacing | Deposit wear-resistant alloy | Current 300 to 500 A, voltage 25 to 35 V, travel speed 20 to 40 cm/min |
| Interlayer Temperature | Maintain consistent deposition temperature | 200 to 300°C, monitored by pyrometer or thermocouple |
| Post-Weld Heat Treatment | Relieve residual stress, temper hardfaced layer | 500 to 650°C, hold 2 to 4 hours, slow cool |
Application Results and Practical Considerations
The paper reports that the device performed well at Meishan, with the rolls achieving the required hardness and wear resistance. From my own experience in steel plants, I would highlight several practical points. First, the roll body must be cleaned and inspected before surfacing. Any cracks, pits, or surface contamination will be magnified by the hardfacing process. Second, the preheating temperature must be sufficient to prevent cracking, but not so high that it causes oxidation or distortion. For a large roll, preheating to 200 to 250°C is usually adequate, but the temperature must be uniform across the roll surface. Third, the interlayer temperature control is critical. If the temperature drops too low between passes, the previous layer may cool below the transformation temperature, leading to hard spots and potential cracking. If it rises too high, the hardfaced layer may over-temper and lose hardness. Fourth, the post-weld heat treatment must be performed promptly after surfacing, before the roll cools to ambient temperature, to avoid the formation of delayed cracks. The device's ability to perform all these functions in one setup is a major advantage, as it reduces the risk of thermal shock from moving a hot roll between different pieces of equipment.
Conclusions and Recommendations
The multi-functional roll body surfacing device is a practical and cost-effective solution for rolling mills that need to refurbish worn rolls in-house. It combines the essential thermal management functions with the surfacing process, ensuring that the hardfaced layer is deposited under controlled conditions. I recommend that mills evaluate this device for their roll maintenance programs, particularly if they currently rely on external vendors for roll refurbishment. The investment is modest, and the ability to control the entire thermal cycle in one setup can significantly improve roll life and reduce downtime. However, the device requires skilled operators who understand the relationship between thermal management and hardfacing quality. Training and procedure qualification are essential before the device is put into regular service.
Zhuojin Pipe Fitting Co., Ltd