ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Microstructure and Wear Resistance of Hypoeutectic Fe-Cr-B-C Hardfacing Alloys

Literature Overview and Core Findings

This paper by Wang Shenglin, Cui Li, He Dingyong, Zhou Zheng and Jiang Jianmin, published in Hot Working Technology in 2016, investigates the microstructure and wear resistance of hypoeutectic Fe-Cr-B-C hardfacing alloys prepared by flux-cored wire gas shielded arc welding. The authors prepared alloys with carbon contents ranging from 0.8% to 1.6% by mass fraction and used optical microscopy, scanning electron microscopy and X-ray diffraction to analyse the microstructure and phase composition. The key findings are that the microstructure is hypoeutectic, consisting of primary γ-Fe dendrites and a eutectic structure of borocarbides plus a eutectic matrix; that carbon significantly increases the amount of eutectic structure and the size of the eutectic matrix; and that the wear resistance is mainly influenced by the amount and morphology of the eutectic structure, which acts as a wear-resistant skeleton. Specifically, the 0.8%C alloy has a relatively low amount of eutectic structure and a relative wear performance of only 9.1; when the carbon content increases to 1.2%, the amount of eutectic structure increases significantly and the wear performance rises to 17.2; but when the carbon content is further increased to 1.6%, although the amount of eutectic structure is the highest, the size of the eutectic matrix is too large and the wear performance drops significantly to 11.4.

Interpretation of Technical Points

The Metallurgy of Hypoeutectic Fe-Cr-B-C Alloys

The Fe-Cr-B-C system is a complex alloy system that has been developed for applications requiring high wear resistance, such as in the mining, cement and steel industries. The alloy design is based on the formation of hard borocarbides, such as (Fe,Cr)2B and (Fe,Cr)7(B,C)3, which provide a wear-resistant skeleton. The hypoeutectic composition is chosen to ensure that the alloy has a certain amount of toughness, which is provided by the primary γ-Fe dendrites. The eutectic structure, consisting of borocarbides and a eutectic matrix, fills the spaces between the dendrites and provides the wear resistance.

The effect of carbon on the microstructure is critical. Carbon promotes the formation of the eutectic structure, increasing its amount. However, it also increases the size of the eutectic matrix. This is because carbon increases the volume fraction of the eutectic, but it also coarsens the eutectic structure. The optimal carbon content is therefore a balance between the amount of eutectic structure and its morphology. The paper shows that 1.2%C gives the best combination, with a high amount of eutectic structure and a relatively fine morphology.

The Relationship Between Microstructure and Wear Resistance

The wear resistance of these alloys is not simply a function of hardness. It is a function of the amount and morphology of the wear-resistant skeleton. The eutectic structure acts as a skeleton that supports the wear surface and prevents the removal of material. If the skeleton is too sparse, the wear resistance is low because the soft matrix is exposed. If the skeleton is too coarse, the wear resistance is also low because the individual borocarbide particles are large and can be easily fractured or pulled out. The optimal microstructure is one with a high amount of eutectic structure and a fine, well-distributed morphology.

This is a key insight that I have seen confirmed in practice. In many hardfacing applications, the temptation is to increase the carbon content to increase the hardness and wear resistance. However, this paper shows that there is a limit to this approach. Beyond a certain carbon content, the coarsening of the eutectic structure leads to a decrease in wear resistance, even though the hardness may continue to increase.

Integration with Engineering Practice

Practical Implications for Hardfacing Applications

The findings of this paper have direct implications for the selection of hardfacing alloys for applications such as mining equipment, cement plant components, and steel mill rolls. In these applications, the wear resistance is critical, but the alloy must also have sufficient toughness to withstand impact and thermal cycling. The paper shows that the carbon content must be carefully controlled to achieve the optimal balance between wear resistance and toughness.

In my experience, the most common mistake in hardfacing is to focus only on the hardness of the deposit and to neglect the microstructure. A hardfacing alloy with a high hardness but a coarse, brittle microstructure will have poor wear resistance in practice because the hard particles will be easily fractured or pulled out. The paper confirms this: the 1.6%C alloy has the highest amount of eutectic structure, but its wear resistance is lower than the 1.2%C alloy because the eutectic matrix is too large.

The Role of Welding Process Parameters

The paper used flux-cored wire gas shielded arc welding, which is a common process for hardfacing. The process parameters, such as the welding current, voltage, and travel speed, have a significant effect on the microstructure. In particular, the heat input affects the cooling rate and hence the size of the primary dendrites and the eutectic structure. A higher heat input will result in a coarser microstructure, while a lower heat input will result in a finer microstructure. The fabricator must therefore control the heat input to achieve the desired microstructure.

This is a critical point that is often overlooked. Many fabricators assume that the alloy composition alone determines the properties, but in reality, the welding process parameters have a significant effect on the microstructure and hence the properties. The paper shows that the carbon content is not the only factor; the cooling rate, which is determined by the heat input, also plays a role.

Defect Analysis and Countermeasures

The main defect in hardfacing alloys is cracking, which can occur due to the high hardness and brittleness of the deposit. The following countermeasures are recommended:

  1. Use a hypoeutectic composition to ensure that the alloy has a certain amount of toughness.
  2. Control the carbon content to achieve the optimal balance between the amount of eutectic structure and its morphology.
  3. Use a preheat and interpass temperature to reduce the risk of cracking.
  4. Control the heat input to achieve the desired microstructure.
  5. Use a post-weld heat treatment to reduce residual stresses and temper any hard microstructures.
  6. Use a buffer layer of a softer alloy to reduce the risk of cracking at the interface.

Key Questions and Reflections

What Is the Optimal Carbon Content?

The paper shows that the optimal carbon content is around 1.2%, where the wear performance reaches a maximum of 17.2. However, this is for the specific alloy system and welding process used in the study. The optimal carbon content may vary depending on the alloy composition, the welding process, and the service conditions. The fabricator must therefore conduct trials to determine the optimal carbon content for their specific application.

How Does the Wear Mechanism Change with Carbon Content?

The paper does not provide a detailed analysis of the wear mechanism, but it is likely that the wear mechanism changes with carbon content. At low carbon contents, the wear is dominated by the removal of the soft matrix. At high carbon contents, the wear is dominated by the fracture and pull-out of the coarse borocarbide particles. At the optimal carbon content, the wear is a combination of both mechanisms, but the wear-resistant skeleton is able to support the wear surface effectively.

What Are the Limitations of the Study?

The study is limited to a specific alloy system and welding process. The findings may not be directly applicable to other alloy systems or welding processes. In addition, the study used a laboratory-scale wear test, which may not fully simulate the conditions in service. The fabricator must therefore conduct field trials to validate the findings.

Study Insights and Implications

The Importance of Microstructural Control in Hardfacing

This paper reinforces the fundamental principle that the microstructure controls the properties. In the case of hardfacing alloys, the microstructure determines the wear resistance, and the microstructure is controlled by the alloy composition and the welding process parameters. The fabricator must have a thorough understanding of the metallurgy of the alloy system and the effect of the welding process on the microstructure.

The Need for a Systems Approach

The problem of hardfacing is not just a materials problem; it is also a welding problem and a design problem. The fabricator must consider the entire system, including the base material, the hardfacing alloy, the welding process, and the service conditions. This requires a systems approach that integrates materials science, welding technology, and mechanical engineering.

The Value of Research in Optimising Hardfacing Alloys

This paper is a good example of how research can optimise hardfacing alloys. The authors systematically varied the carbon content and studied the effect on the microstructure and wear resistance. This approach is more effective than the trial-and-error approach that is often used in industry. The fabricator should use a similar approach to optimise their hardfacing alloys.

Conclusion

The paper by Wang Shenglin et al. provides a comprehensive understanding of the effect of carbon content on the microstructure and wear resistance of hypoeutectic Fe-Cr-B-C hardfacing alloys. The key findings are that the microstructure is hypoeutectic, consisting of primary γ-Fe dendrites and a eutectic structure of borocarbides plus a eutectic matrix; that carbon significantly increases the amount of eutectic structure and the size of the eutectic matrix; and that the wear resistance is mainly influenced by the amount and morphology of the eutectic structure. The optimal carbon content is around 1.2%, where the wear performance reaches a maximum. These findings have direct implications for the selection of hardfacing alloys for applications requiring high wear resistance, and they highlight the importance of microstructural control in hardfacing. The paper also demonstrates the value of research in optimising hardfacing alloys, and it provides a systematic approach that can be used by fabricators to develop and qualify hardfacing alloys for their specific applications. For the industry veteran, this paper is a reminder that the wear resistance of a hardfacing alloy is not simply a function of hardness, but is determined by the amount and morphology of the wear-resistant skeleton, and that the carbon content must be carefully controlled to achieve the optimal balance between wear resistance and toughness.