Microstructure and Hardness Analysis of Stainless Steel Hardfacing Joint on Q235 Steel

Literature Overview and Core Findings

The paper by Li et al. (2013) investigates the microstructure and hardness of a 3Cr13 stainless steel hardfacing layer deposited on Q235 steel using the automatic submerged arc welding process. The authors analyzed the microstructure of the joint and measured the microhardness across the interface.

The results showed that the hardness distribution corresponds to the microstructural changes across the joint. The base metal had an average hardness of 132 HV, while the hardfacing layer had an average hardness of 432 HV. The maximum hardness of 453 HV was observed in the second layer of the hardfacing metal.

Technical Interpretation and Process Parameters

The use of 3Cr13 stainless steel for hardfacing is a common practice in the industry because it offers a good combination of hardness and corrosion resistance. The automatic submerged arc welding process is well-suited for hardfacing because it provides high deposition rates and a stable arc, and the flux provides protection from atmospheric contamination.

The hardness distribution across the joint is a key indicator of the quality of the hardfacing. The base metal hardness of 132 HV is typical for Q235 steel, which is a low-carbon structural steel. The hardfacing layer hardness of 432 HV is significantly higher, which is expected for a martensitic stainless steel. The maximum hardness of 453 HV in the second layer is interesting because it suggests that the second layer has a higher hardness than the first layer.

This is likely due to the effect of dilution. The first layer is diluted by the base metal, which reduces the carbon and chromium content and lowers the hardness. The second layer is deposited on the first layer, which is already hard, and the dilution from the base metal is less, so the second layer retains more of the intended alloy composition and achieves higher hardness.

Comparison of Microstructure and Hardness Across the Joint

The following table summarizes the hardness distribution across the joint:

Zone Average Hardness (HV) Microstructure
Base metal (Q235) 132 Ferrite + Pearlite
Heat-affected zone Intermediate Varies
First hardfacing layer Lower than second Martensite + Ferrite
Second hardfacing layer 453 (max) Martensite + Carbides

The hardness distribution is consistent with the microstructural changes. The base metal is a soft ferrite-pearlite structure, while the hardfacing layer is a hard martensitic structure. The heat-affected zone is a transition zone where the microstructure changes from ferrite-pearlite to martensite, and the hardness increases accordingly.

Engineering Practice and Lessons Learned

The hardfacing of Q235 steel with 3Cr13 stainless steel is a common practice in the steel pipe and fitting industry, particularly for components that require both wear resistance and corrosion resistance, such as pipe fittings, valve bodies, and pump components.

One lesson I have learned from working with stainless steel hardfacing is that the dilution from the base metal is a critical factor that determines the properties of the hardfacing layer. The first layer is always diluted by the base metal, which reduces the hardness and corrosion resistance. For critical applications, it is essential to deposit at least two layers to achieve the full properties of the hardfacing alloy.

The finding that the maximum hardness is in the second layer is consistent with this. In practice, this means that a single-layer hardfacing may not provide the desired performance, and a two-layer deposit is often necessary. However, a two-layer deposit also means more heat input, which can cause distortion and residual stress. The process parameters must be carefully controlled to balance these competing factors.

Another practical point is the need for proper preheating and post-weld heat treatment. 3Cr13 is a martensitic stainless steel that is prone to hydrogen-induced cracking. Preheating reduces the cooling rate and allows hydrogen to diffuse out of the weld, while post-weld heat treatment can temper the martensite and reduce the hardness, improving toughness.

Study Insights and Reflections

This paper is a straightforward but valuable contribution to the field. The hardness distribution across the joint provides a clear picture of the quality of the hardfacing, and the microstructural analysis explains the hardness variations.

From a practical standpoint, the most valuable contribution of this work is the confirmation that the second layer of hardfacing achieves higher hardness than the first layer. This is a well-known phenomenon in the industry, but it is useful to have it documented in a systematic study.

However, I would note that the paper does not address the corrosion resistance of the hardfacing layer. 3Cr13 is a martensitic stainless steel that offers moderate corrosion resistance, but the corrosion resistance is significantly affected by the microstructure and the presence of carbides. In a corrosive environment, the hardfacing layer may not provide adequate protection, and a more corrosion-resistant alloy may be required.

One gap in the study is the lack of data on the wear resistance of the hardfacing layer. The hardness is a useful indicator, but it does not directly correlate with wear resistance in all cases. A hardfacing layer with high hardness may still have poor wear resistance if the microstructure is not optimized.

Conclusion and Outlook

The analysis of the microstructure and hardness of a 3Cr13 stainless steel hardfacing layer on Q235 steel provides valuable insights into the quality of the joint. The hardness distribution is consistent with the microstructural changes, and the maximum hardness in the second layer confirms the importance of multi-layer deposition for achieving full hardfacing properties. This work has direct relevance to the hardfacing of components in the steel pipe and fitting industry, where wear and corrosion resistance are critical. The next step should be to evaluate the corrosion resistance and wear resistance of the hardfacing layer under actual service conditions to determine whether the hardfacing provides adequate protection.