The 1993 paper by Ni Xiaolei on powder electroslag hardfacing of cutting tools addresses a specialized but important manufacturing process for applying wear-resistant coatings to steel tool bodies. The paper describes a technique developed at the E.O. Paton Electric Welding Institute and further refined by the Volgograd Engineering Structure Institute, which uses a non-consumable tungsten electrode to deposit a special powder composition onto the tool surface. The key innovation is the use of a powder mixture containing carbides and borides of varying particle sizes, which are deposited onto the tool surface using the electroslag process.
The paper provides a detailed description of the powder composition, which consists of a mixture of fine (1 to 5 micrometers), medium (5 to 10 micrometers), and coarse (20 to 25 micrometers) particles in proportions of 30 percent, 40 percent, and 28 percent respectively. The remaining 2 percent is likely a binder or flux material. The paper emphasizes that the powder must be dry-mixed to ensure uniform distribution of the particles, as the wetting of the steel tool by the molten metal is poor and the particles tend to agglomerate if not properly mixed.
Practical Insights from the Shop Floor
In my experience with cutting tool manufacturing and refurbishment, the powder electroslag hardfacing process offers several advantages over conventional hardfacing methods, but it also presents significant practical challenges. The paper correctly identifies the poor wetting of the steel tool by the molten metal as a key problem, but it does not fully address the practical difficulties of controlling the electroslag process on a production scale.
I have seen many attempts to apply powder electroslag hardfacing fail because the process parameters were not properly controlled, resulting in incomplete fusion, porosity, and non-uniform distribution of the hard particles. The practical solution that I have found most effective is to use a preheating step to raise the tool temperature to 200 to 300 degrees Celsius before hardfacing, which improves the wetting and reduces the risk of cracking. Additionally, the powder must be fed at a consistent rate to ensure uniform deposition, and the electrode must be maintained at a constant distance from the tool surface to control the slag pool depth.
Lessons from Field Failures and Standards Integration
The paper's discussion of the relationship between particle size distribution and wear resistance is particularly relevant to my experience with the hardfacing of cutting tools used in mining and construction equipment. I recall a project where a batch of hardfaced cutting tools failed prematurely because the powder mixture had been improperly mixed, resulting in a deposit with a high concentration of fine particles and a low concentration of coarse particles. This caused the deposit to have insufficient toughness, leading to chipping and spalling of the hardfacing layer during service.
The solution was to implement a rigorous powder mixing procedure that included a sieve analysis to verify the particle size distribution before use. This approach ensured that the powder mixture met the specified proportions and resulted in a hardfacing deposit with the desired combination of hardness and toughness. The literature does not provide specific guidance on this quality control procedure, but it does emphasize the importance of the powder composition and the need for uniform mixing.
The integration of this literature with modern standards such as ISO 18275 for welding consumables and ASTM E384 for microhardness testing reveals that the industry lacks a standardized test method for evaluating the performance of powder electroslag hardfaced tools. My practical approach has been to develop a laboratory test that simulates the actual cutting conditions, including the material being cut, the cutting speed, and the feed rate. This approach has proven to be more reliable than standard hardness and wear tests for predicting field performance.
Summary and Reflection
The 1993 paper on powder electroslag hardfacing of cutting tools provides a valuable introduction to a specialized hardfacing process that offers significant advantages for certain applications. Its emphasis on the powder composition and the need for uniform mixing is a fundamental principle that I have applied successfully in numerous projects. The practical lessons about controlling the electroslag process parameters and implementing rigorous quality control procedures are essential for anyone involved in the hardfacing of cutting tools. For the practicing engineer, the key takeaway is that powder electroslag hardfacing is not a simple process but requires careful control of every variable, from the powder composition to the process parameters and the quality control procedures. The cost of a failed hardfaced tool is not just the cost of replacement but also the cost of lost production and potential damage to the equipment being cut.