OCC-Drawn L401 Aluminum Alloy Wire for TIG Hardfacing on ZL117
1. A Different Way to Make Welding Wire
When I first read this paper, I was struck by the elegance of the approach. The authors used the Ohno Continuous Casting (OCC) process to produce a φ4 mm aluminum alloy wire with a smooth surface and a directionally solidified structure. The OCC process, developed by Professor Ohno in Japan, uses a heated mould and a cooling system that allows the molten metal to solidify in a controlled direction, producing a wire with a columnar structure aligned along the drawing direction. This is fundamentally different from conventional casting, which produces a equiaxed grain structure with more porosity and segregation.
The significance for welding is that the wire's microstructure directly affects the weld deposit. A wire with a fine, aligned structure melts more uniformly, produces a more stable arc, and results in a weld deposit with a more homogeneous structure. The authors then used this wire as filler for TIG hardfacing on ZL117, a hypereutectic Al-Si alloy used in automotive and aerospace applications where wear resistance is critical.
2. Microstructure of the OCC Wire
The OCC-drawn L401 wire (L401 is a Chinese designation for an Al-Si-Cu filler alloy, similar to ER4043 but with higher copper content) exhibited a microstructure consisting of:
- Directionally grown, nearly parallel columnar dendrites of α-Al.
- Interdendritic binary eutectic of (α-Al + Si).
- Interdendritic ternary eutectic of (α-Al + Si + CuAl₂).
The columnar structure is the hathe writing systemark of the OCC process. The dendrites grow in the direction of heat extraction, which is along the wire axis. This produces a wire with high ductility and a smooth surface, which is beneficial for wire feeding in automated welding systems.
The presence of CuAl₂ (θ phase) in the ternary eutectic is significant. Copper in aluminum alloys forms CuAl₂, which is a hard intermetallic phase. The amount and distribution of this phase determine the hardness and wear resistance of the alloy. In the OCC wire, the CuAl₂ is finely dispersed in the interdendritic regions, which is ideal for hardfacing applications.
3. Hardfacing on ZL117 and Wear Performance
The authors used the OCC-drawn L401 wire to hardface ZL117 using TIG welding. The resulting hardfacing layer was analysed with optical microscopy and XRD. The microstructure of the hardfacing layer consisted of the same phases as the wire, but with a more refined distribution due to the rapid solidification of the weld pool.
The key result was the hardness and wear resistance. The hardfacing layer had a hardness of approximately 100–120 HV, compared to the ZL117 substrate at around 60–70 HV. The wear resistance, measured by a pin-on-disc test, was 43 times higher than that of the ZL117 substrate. This is an extraordinary improvement, and it is attributed to the high volume fraction of hard CuAl₂ and Si phases in the hardfacing layer.
| Property | ZL117 Substrate | Hardfacing Layer (OCC L401) |
|---|---|---|
| Hardness (HV) | 60–70 | 100–120 |
| Relative wear resistance | 1 | 43 |
| Primary phases | α-Al + Si + CuAl₂ | α-Al + Si + CuAl₂ (refined) |
| Microstructure | Coarse, equiaxed | Fine, directionally solidified |
The 43× improvement is remarkable, but it must be interpreted carefully. The wear test conditions matter. The authors used a dry sliding wear test, which is a severe condition for aluminum alloys. In a lubricated or abrasive environment, the improvement might be different. However, the result is still a strong indication that the hardfacing layer is significantly more wear-resistant than the substrate.
4. Metallurgical Explanation
The wear resistance of Al-Si-Cu alloys is controlled by the size and distribution of the hard phases. In ZL117, the primary Si particles are coarse and blocky, which can act as stress concentrators and lead to crack initiation during wear. In the hardfacing layer, the Si particles are finer and more uniformly distributed, and the CuAl₂ phase is also finely dispersed. This combination of fine, hard phases in a ductile α-Al matrix provides a composite structure that resists wear effectively.
The OCC wire's directionally solidified structure contributes to this refinement. When the wire is melted in the TIG arc, the columnar structure breaks down, but the fine distribution of Si and CuAl₂ in the interdendritic regions is preserved in the weld pool, leading to a refined microstructure in the hardfacing layer.
5. Practical Considerations for Hardfacing Aluminum
Hardfacing aluminum alloys is notoriously difficult. The oxide layer on aluminum melts at 2050 °C, while the base metal melts at around 660 °C. This means that the oxide must be broken up or removed before the weld can wet the surface. TIG welding with AC current is the standard approach, as the reverse polarity half-cycle cleans the oxide. The authors used TIG, which is the right choice for this application.
The OCC wire has a smooth surface, which is an advantage for wire feeding. In automated TIG welding, a rough wire surface can cause feeding problems and arc instability. The smooth surface of the OCC wire ensures consistent feeding and a stable arc, which is critical for achieving a uniform hardfacing layer.
6. Lessons for the Shop Floor
This paper is a good example of how process innovation can improve weld quality. The OCC process is not widely used in the welding industry, but its potential for producing high-quality filler wires is significant. The key lessons are:
- The filler wire's microstructure matters. A directionally solidified wire melts more uniformly and produces a more homogeneous weld deposit.
- The hardfacing layer's wear resistance is a function of the hard phase distribution. Fine, uniformly distributed hard phases give better wear resistance than coarse, blocky phases.
- TIG welding with AC is the right process for aluminum hardfacing. The reverse polarity half-cycle cleans the oxide and ensures good wetting.
7. Closing Thoughts
This paper is a reminder that the quality of the filler wire is as important as the welding process itself. In my experience, many weld failures are traced back to poor filler wire quality, whether it is porosity, segregation, or surface contamination. The OCC process offers a way to produce wires with a controlled microstructure, which can improve weld quality and performance. I would encourage engineers to look beyond the standard filler wire catalogues and consider alternative production routes that can deliver better properties.
Zhuojin Pipe Fitting Co., Ltd