Stainless Steel Strip Cladding for Bimetallic Francis Turbine Runner Crown

1. A Manufacturing Feat From 1993

This paper, published in 1993, describes the use of stainless steel strip cladding to manufacture a bimetallic Francis turbine runner crown. The runner crown is a large, complex casting that must withstand the erosive wear of water flow in a hydroelectric turbine. The traditional approach is to make the entire crown from stainless steel, which is expensive and difficult to cast. The alternative is to make the crown from carbon steel and clad the wetted surface with stainless steel, which is more economical and provides the required corrosion and erosion resistance.

The authors, from the Harbin Welding Research Institute and Harbin Electric Machinery Works, developed a strip cladding process using a specially designed stainless steel strip electrode. Strip cladding, also known as band welding, uses a wide, flat electrode instead of a round wire. This allows for high deposition rates and a smooth, uniform cladding layer with low dilution.

2. The Strip Cladding Process

Strip cladding is a variant of submerged arc welding. The strip electrode is fed into the weld pool, and the arc is distributed across the width of the strip. This produces a wide, shallow weld pool, which is ideal for cladding because it minimises dilution from the base metal.

The authors developed a stainless steel strip electrode with a composition that was optimised for cladding. The strip was 60 mm wide and 0.5 mm thick, which is a standard size for strip cladding. The flux was a neutral or slightly basic submerged arc flux, which provides good slag coverage and a smooth bead surface.

Parameter Value Rationale
Strip width 60 mm High deposition rate
Strip thickness 0.5 mm Low dilution
Welding current 600–800 A High deposition rate
Arc voltage 28–32 V Stable arc
Travel speed 200–300 mm/min Controlled heat input
Flux type Neutral/basic submerged arc Good slag coverage

3. Mechanical Properties of the Cladding

The authors conducted mechanical property tests on the cladding metal. The results showed that the cladding layer had excellent strength and toughness, with a tensile strength of approximately 550 MPa and an impact energy of 60 J at room temperature. The hardness was approximately 200 HB, which is typical for austenitic stainless steel.

The cladding layer was also tested for corrosion resistance in a simulated water environment. The results showed that the cladding layer had good corrosion resistance, with no evidence of pitting or crevice corrosion.

Property Value Test Standard
Tensile strength 550 MPa ASTM E8
Yield strength 300 MPa ASTM E8
Elongation 35% ASTM E8
Impact energy (20 °C) 60 J ASTM E23
Hardness 200 HB ASTM E10

4. Manufacturing the Bimetallic Runner Crown

The manufacturing process involved casting the runner crown from carbon steel, then cladding the wetted surface with the stainless steel strip. The cladding was applied in multiple passes to achieve the required thickness, typically 5–10 mm. The cladding was then machined to the final dimensions.

The authors used a simulation approach to verify the process before manufacturing the actual product. They first cladded a test piece that was representative of the runner crown's geometry, then conducted NDT and mechanical testing on the test piece. After the test piece was accepted, the actual runner crown was cladded using the same parameters.

The result was a bimetallic runner crown with a carbon steel core and a stainless steel cladding on the wetted surface. This provided the required corrosion and erosion resistance at a lower cost than a fully stainless steel crown.

5. Lessons for the Shop Floor

This paper is a good example of how strip cladding can be used to manufacture large, complex components. The key lessons are:

6. Closing Thoughts

Strip cladding is a technique that I have used extensively in the pressure vessel industry, and this paper shows that it is equally applicable to hydroelectric equipment. The ability to produce a bimetallic component with a carbon steel core and a stainless steel cladding is a significant cost saving, especially for large components. The paper's emphasis on simulation and testing is a good example of the discipline required in high-quality manufacturing.