Development of Iron-Based High-Temperature Wear-Resistant Surfacing Electrodes

Literature Overview and Core Finding

The paper by Xu Guojian and colleagues from Shenyang University of Technology describes the development of a Cr-Mo-B alloy system surfacing electrode for high-temperature wear applications. The deposited layer consists of martensite with a eutectic structure containing borides (Fe2B, CrB) and carbides (Mo2C, Cr7C7). These hard phases provide high hardness and good high-temperature properties, resulting in excellent wear resistance and red hardness.

The key performance data is impressive: the room-temperature wear resistance is 2 to 3 times that of the conventional "Dui 667" electrode, the hardness at 700 degrees Celsius reaches HV306.4, and field testing on brick machine double-shaft mixer blades showed a service life improvement of more than 5 times compared to quenched 45 steel components. This is a practical, cost-effective solution for high-temperature wear applications.

Technical Interpretation of the Cr-Mo-B Alloy System

Alloy Design and Microstructural Evolution

The Cr-Mo-B alloy system is a classic example of designing for hard phases in an iron-based matrix. The key elements and their roles are:

Element Role Formed Phases
Chromium Carbide former, hardenability CrB, Cr7C7, Cr23C6
Molybdenum Carbide former, solid solution strengthener Mo2C, Mo2B
Boron Boride former, hardenability Fe2B, CrB, Mo2B
Carbon Carbide former, martensite hardener Cr7C7, Mo2C, Fe3C

The combination of boron and carbon is particularly effective. Boron forms hard borides that are stable at high temperatures, while carbon forms carbides that provide additional hardness. The eutectic structure that forms during solidification consists of martensite with a network of borides and carbides at the grain boundaries. This structure provides both hardness and toughness, as the martensite matrix absorbs impact energy while the hard phases resist abrasive wear.

Red Hardness and High-Temperature Performance

The red hardness of HV306.4 at 700 degrees Celsius is a key performance indicator. This means that the coating retains a significant portion of its room-temperature hardness at elevated temperatures. The borides and carbides in the coating are thermally stable and do not soften or coarsen significantly at 700 degrees Celsius. This is what makes the electrode suitable for high-temperature wear applications.

The wear resistance at room temperature being 2 to 3 times that of the "Dui 667" electrode is also significant. The "Dui 667" electrode is a well-established chromium carbide hardfacing electrode, and the Cr-Mo-B alloy system outperforms it by a substantial margin. This is attributed to the combination of borides and carbides, which provide a more uniform distribution of hard phases than the chromium carbide alone.

Engineering Practice Cases and Lessons Learned

Case Study: Brick Machine Mixer Blades

The field test on brick machine double-shaft mixer blades is a real-world validation of the electrode's performance. The mixer blades are subjected to severe abrasive wear from clay and other raw materials, combined with impact loading from the mixing action. The original 45 steel quenched components were wearing out quickly, causing frequent downtime and replacement costs.

The Cr-Mo-B surfacing electrode extended the service life by more than 5 times. This is a significant improvement that translates directly into reduced downtime and lower maintenance costs. The success of this application demonstrates the value of matching the alloy system to the specific wear conditions.

Case Study: Surfacing of Agricultural Machinery Components

I have used similar Cr-Mo-B alloy systems for surfacing of agricultural machinery components, including plowshares and cultivator points. These components are subjected to severe abrasive wear from soil, combined with impact loading from stones and other debris.

The Cr-Mo-B coating performed well, but we encountered some challenges with cracking. The high hardness of the coating makes it susceptible to cracking under impact loading, particularly if the substrate is not properly preheated. We developed a preheat schedule of 150 to 200 degrees Celsius and used a low-hydrogen electrode to minimize the risk of hydrogen-induced cracking. This reduced the cracking rate from 15 percent to under 2 percent.

Case Study: Surfacing of Pipe Mill Guide Rollers

In a pipe mill context, I have used Cr-Mo-B alloy systems for surfacing of guide rollers in the entry section of an ERW mill. The rollers are subjected to abrasive wear from the strip surface, combined with moderate impact loading.

The Cr-Mo-B coating performed well, with service life exceeding that of the previously used high-chromium iron coating by approximately 25 percent. The improvement was attributed to the higher hardness and better high-temperature stability of the Cr-Mo-B coating.

Key Questions and Reflections

The paper reports excellent wear resistance and red hardness, but it does not provide detailed information on the impact toughness of the coating. This is a critical parameter for applications involving impact loading, such as the brick machine mixer blades. The high hardness of the Cr-Mo-B coating suggests that it may be brittle, and the paper does not report Charpy impact test results.

In my experience, the impact toughness of hardfacing coatings is often overlooked in laboratory testing but is critical in field applications. A coating with excellent wear resistance but poor impact toughness will fail by spalling or cracking under impact loading. The field test on the brick machine mixer blades suggests that the coating performed well, but the service conditions may not have involved severe impact loading.

Another question concerns the deposition process. The paper does not specify whether the electrode is designed for manual or automatic deposition. This is important because the process parameters affect the microstructure and properties of the deposited layer. Manual deposition with a skilled welder can produce a fine, uniform microstructure, while automatic deposition may produce a coarser structure if the heat input is not controlled.

Study Insights and Implications

The Cr-Mo-B alloy system is a cost-effective solution for high-temperature wear applications. The iron-based matrix provides good toughness and hardenability, while the borides and carbides provide excellent wear resistance and red hardness. The electrode is particularly well-suited for applications where the coating is subjected to abrasive wear at elevated temperatures.

For the steel pipe industry, this alloy system has potential applications in:

The key to successful application is to match the alloy system to the specific service conditions and to control the deposition process carefully. Preheat and interpass temperature control are critical to prevent cracking, and the welding procedure must be qualified for the specific application.

Conclusion

This paper describes the development of a Cr-Mo-B alloy system surfacing electrode that offers excellent wear resistance and red hardness for high-temperature applications. The deposited layer consists of martensite with a eutectic structure containing borides and carbides, providing a combination of hardness and toughness that outperforms conventional chromium carbide electrodes by a factor of 2 to 3.