Roller Press Roll Surface Hardfacing Repair: Technology and Application

Introduction: The Wear Problem in Roller Presses

Roller presses are used in cement and mineral processing to grind raw materials. The rolls are subjected to extreme abrasive wear, and the surface must be periodically repaired or replaced. The paper by Shi Liyan et al. (2007) discusses the technology and application of hardfacing repair for roller press rolls. This is a high-wear application, and the repair technique must be robust and cost-effective. The paper correctly identifies that the key to a successful repair is the selection of the hardfacing material and the welding procedure. I have seen roller press rolls that were repaired multiple times, and the quality of the repair determines the service life of the roll.

Core Technical Points: Hardfacing Material and Welding Procedure

The paper discusses the working principle of the roller press and the repair technology. The hardfacing material is typically a high-chromium iron-based alloy, deposited using a flux-cored wire or a submerged arc welding process. The welding procedure must be carefully controlled to avoid cracking and to achieve the desired hardness and wear resistance. I have summarized the key technical points below.

Technical Aspect Recommended Practice Practical Significance
Hardfacing material High-chromium iron-based alloy, e.g., 25–30% Cr, with carbide-forming elements (Mo, Nb, V) The chromium carbides provide excellent abrasive wear resistance. The hardness should be in the range of 55–65 HRC.
Welding process Flux-cored arc welding (FCAW) or submerged arc welding (SAW) These processes provide high deposition rates and good weld quality. SAW is preferred for large rolls because of its high efficiency.
Welding pattern Strip or "wavy" pattern, with overlapping passes The pattern must ensure uniform coverage and avoid unfused zones. A "wavy" pattern is often used to distribute the residual stress.
Preheat and interpass temperature Preheat to 150–200°C, interpass temperature ≤300°C Reduces the risk of cracking in the hardfacing layer and the HAZ. The roll is a large component, so the preheat must be uniform.
Post-weld treatment Slow cooling, possibly with a stress-relief heat treatment Reduces residual stress and prevents delayed cracking. For a large roll, controlled cooling is often the only practical option.

The paper also discusses the precautions to be taken during the repair. The most important of these is to ensure that the roll surface is properly prepared before welding. The worn surface must be ground or machined to remove any cracks or defects. If the surface is not properly prepared, the new hardfacing layer will not bond to the base metal, and the repair will fail.

Practical Insights and Lessons from the Field

I have seen roller press rolls repaired many times, and the success of the repair depends on several factors that the paper does not fully address:

  1. The repair should be planned as a complete operation. The roll must be removed from the press, the surface prepared, the hardfacing applied, and the roll inspected. Each step must be carried out with care, and the roll should not be put back into service until it has passed inspection.
  2. The hardfacing layer should be applied in multiple passes. A single thick pass will have high residual stress and may crack. The layer should be built up in multiple passes, with each pass overlapping the previous one.
  3. The hardness of the hardfacing layer must be checked. A hardness test on the finished surface will confirm that the hardfacing material has been deposited correctly. If the hardness is too low, the roll will wear quickly; if it is too high, the hardfacing may be brittle and crack.
  4. The roll must be balanced after repair. The hardfacing process will add material to the roll surface, which may cause an imbalance. The roll must be balanced before it is put back into service, otherwise it will vibrate and cause damage to the press.

Summary and Outlook

The paper by Shi Liyan et al. provides a good overview of the technology and application of hardfacing repair for roller press rolls. The authors correctly identify that the key to a successful repair is the selection of the hardfacing material and the welding procedure. The paper is a useful reference for any engineer involved in the repair of wear components. However, I would recommend that the paper be supplemented with more detailed information on the welding parameters and the inspection requirements. From my perspective, the most important lesson is that the repair must be planned as a complete operation, from surface preparation to final inspection. A roller press roll is a critical component, and a poorly executed repair will lead to premature failure and costly downtime.