Strip Cladding Repair of Continuous Casting Machine Guide Rollers

Literature Overview and Practical Significance

The paper by Zhang Xiangfu from Jinan Iron and Steel Group addresses a practical problem that is familiar to anyone involved in steel production: the wear and failure of continuous casting machine guide rollers. These rollers operate in a harsh environment, exposed to high temperatures, thermal cycling, and abrasive wear from the steel strand. The paper describes the development of a strip cladding repair process using 0Cr13NiMoN hardfacing metal, combined with auxiliary carbon-nitrogen strengthening technology and a specific welding technique. The result is a high-quality repaired roller that can be returned to service. This is a valuable contribution because roller replacement is expensive, and repair is often more economical than replacement.

Key Technical Points and Interpretation

Working Environment and Failure Mechanism of Guide Rollers

The paper analyzes the working environment of continuous casting machine guide rollers. The rollers are exposed to high temperatures, typically in the range of 800 to 1000°C, and they are in contact with the hot steel strand. The failure mechanisms include abrasive wear from the strand, thermal fatigue from the cyclic heating and cooling, and corrosion from the cooling water and the atmosphere. The combination of these mechanisms leads to surface cracking, spalling, and dimensional loss. The paper identifies the dominant failure mechanism as abrasive wear combined with thermal fatigue.

Strip Cladding Process

The paper describes the use of strip cladding for the repair of guide rollers. Strip cladding is a process in which a strip electrode is used instead of a round wire. The strip provides a higher deposition rate and a wider weld bead, which is advantageous for covering large surfaces. The paper specifies a longitudinal strip cladding technique with an overlapping bead sequence. This technique ensures that the entire surface of the roller is covered with the hardfacing metal.

0Cr13NiMoN Hardfacing Metal

The paper selects 0Cr13NiMoN as the hardfacing material. This is a martensitic stainless steel with additions of molybdenum and nitrogen. The molybdenum increases the hardenability and the corrosion resistance, while the nitrogen increases the hardness and the strength. The material has a good combination of hardness and toughness, which makes it suitable for the abrasive and thermal fatigue conditions of the guide rollers.

Auxiliary Carbon-Nitrogen Strengthening Technology

The paper introduces an auxiliary carbon-nitrogen strengthening technology. This involves the addition of carbon and nitrogen to the hardfacing metal to increase its hardness and wear resistance. The carbon and nitrogen form hard carbides and nitrides, which are distributed in the martensitic matrix. The technology is applied during the cladding process, ensuring that the strengthening elements are uniformly distributed.

Integration with Engineering Practice

Repair vs. Replacement Decision

The paper demonstrates that repair is a viable alternative to replacement for continuous casting machine guide rollers. The cost of repair is significantly lower than the cost of a new roller, and the repaired roller can achieve a service life comparable to a new one. The decision to repair or replace depends on the extent of the damage and the availability of the repair equipment. In my experience, repair is often the preferred option when the roller is not severely damaged.

Welding Procedure Qualification

The welding procedure for the strip cladding must be carefully qualified to ensure the quality of the repaired roller. The key parameters include the welding current, voltage, travel speed, and the preheat and interpass temperatures. The paper emphasizes the importance of a reasonable welding process to achieve a high-quality weld. The procedure must be validated through testing, including hardness testing, metallographic examination, and non-destructive testing.

Quality Control and Inspection

The repaired roller must be inspected to ensure that the cladding is free of defects such as cracks, porosity, and lack of fusion. The inspection methods include visual examination, magnetic particle testing, and ultrasonic testing. The hardness of the cladding must be measured to verify that it meets the specification. The paper emphasizes that a high-quality weld is essential for the performance of the repaired roller.

Key Questions and Reflections

Why Is Strip Cladding Preferred Over Other Processes?

Strip cladding offers several advantages over other cladding processes, such as submerged arc welding with a single wire or gas metal arc welding. The strip provides a higher deposition rate, which reduces the time required to cover the roller surface. The wide weld bead also reduces the number of passes required. However, strip cladding requires specialized equipment and careful control of the welding parameters.

What Are the Challenges of Cladding a Cylindrical Surface?

Cladding a cylindrical surface, such as a guide roller, presents unique challenges. The roller must be rotated during the cladding process to ensure uniform coverage. The welding position changes as the roller rotates, which can affect the weld quality. The paper addresses this by using a longitudinal strip cladding technique, which minimizes the effect of the welding position.

How Does the Auxiliary Carbon-Nitrogen Strengthening Work?

The auxiliary carbon-nitrogen strengthening technology involves the addition of carbon and nitrogen to the hardfacing metal. The carbon and nitrogen form hard carbides and nitrides, which increase the hardness and wear resistance of the cladding. The technology is applied during the cladding process, ensuring that the strengthening elements are uniformly distributed. The result is a cladding with a higher hardness and better wear resistance than a conventional hardfacing material.

Study Insights and Implications

This paper is a practical example of how welding technology can be used to extend the service life of expensive equipment. The repair of continuous casting machine guide rollers is a cost-effective alternative to replacement, and the paper provides a detailed description of the repair process. The use of 0Cr13NiMoN hardfacing metal, combined with the auxiliary carbon-nitrogen strengthening technology, results in a repaired roller that can perform as well as a new one.

The paper also highlights the importance of understanding the failure mechanism before selecting a repair process. The guide rollers fail due to a combination of abrasive wear and thermal fatigue. The hardfacing material must have a good combination of hardness and toughness to resist both mechanisms. The 0Cr13NiMoN material provides this combination.

Reference Value and Outlook

This paper is a valuable reference for engineers involved in the maintenance and repair of continuous casting equipment. The strip cladding process described in the paper can be applied to other components that are subject to similar wear and thermal fatigue conditions. The auxiliary carbon-nitrogen strengthening technology is a useful innovation that can be applied to other hardfacing applications.

Looking ahead, the development of new hardfacing materials and processes will continue to improve the service life of continuous casting equipment. The use of advanced materials, such as metal matrix composites, and advanced processes, such as laser cladding, may offer further improvements. However, the strip cladding process described in this paper remains a practical and cost-effective solution for the repair of guide rollers.