Microstructure and Properties of Self-Lubricating Wear-Resistant Cladding by Droplet-Free Arc Hot-Wire GTAW

Overview of the Literature

This paper, published in Surface Technology (2020, Vol. 49, No. 7), investigates the use of a novel welding process, droplet-free arc hot-wire GTAW, for depositing a self-lubricating wear-resistant cladding containing graphite. The authors, from Tianjin Sino-German University of Applied Sciences and Jiamusi University, designed a flux-cored wire containing nickel-coated graphite powder, and compared the droplet-free arc hot-wire GTAW process with conventional GMAW. The results show that the droplet-free arc hot-wire GTAW process effectively reduces the dilution of the base metal, ensures the transition of the graphite phase, and increases the deposition rate. The cladding layer forms a Fe-Cr-B wear-resistant matrix with a large number of granular graphite phases distributed at the grain boundaries. In friction and wear tests, the cladding layer has a friction coefficient as low as about 0.65, which decreases with time, and the worn surface is smooth and black, indicating self-lubrication. In contrast, the conventional GMAW cladding has a friction coefficient of about 1.4, which increases with time. The paper concludes that the droplet-free arc hot-wire GTAW process is suitable for cladding applications, especially where the chemical composition of the wire must be preserved.

Why Self-Lubricating Cladding Matters

In many industrial applications, such as bearings, gears, and sliding components, the surfaces are subjected to friction and wear. Conventional lubricants can be used, but they may not be suitable in high-temperature, vacuum, or other demanding environments. Self-lubricating materials, which contain solid lubricants such as graphite, MoS2, or BN, offer an alternative. The challenge is to incorporate these solid lubricants into a wear-resistant matrix while maintaining the integrity of the cladding layer.

Graphite is a common solid lubricant, but it is difficult to incorporate into a cladding layer because it tends to burn off during welding due to the high temperature. The paper addresses this challenge by using nickel-coated graphite powder in the flux-cored wire and by using a low-heat-input welding process.

Droplet-Free Arc Hot-Wire GTAW Process

The droplet-free arc hot-wire GTAW process is a variation of the conventional hot-wire GTAW process. In conventional hot-wire GTAW, the filler wire is preheated by resistance heating before entering the weld pool. In the droplet-free process, the wire is heated to a temperature just below its melting point, so that it enters the weld pool in a semi-solid state without forming droplets. This reduces the heat input and the dilution of the base metal, while increasing the deposition rate.

The key process parameters are:

Parameter Typical Value Notes
Welding current (GTAW) 150–250 A Controls the heat input and the size of the weld pool
Wire feed speed 1–3 m/min Determines the deposition rate
Wire heating current 50–150 A Controls the preheating of the wire
Arc voltage 10–15 V Maintained to ensure a stable arc
Travel speed 10–30 cm/min Adjusted to achieve the desired bead width and thickness
Shielding gas Argon, 10–15 L/min Provides protection for the weld pool and the heated wire

The paper reports that the droplet-free arc hot-wire GTAW process can achieve a deposition rate of up to 5 kg/h, which is significantly higher than conventional GTAW. The dilution rate is reduced to less than 10%, compared to 20–30% for conventional GMAW.

Microstructure and Properties of the Cladding Layer

The cladding layer produced by the droplet-free arc hot-wire GTAW process has a Fe-Cr-B wear-resistant matrix, with a large number of granular graphite phases distributed at the grain boundaries. The graphite phases are retained because the low heat input and the nickel coating protect them from burning off.

The friction and wear tests show that the cladding layer has a friction coefficient of about 0.65, which decreases with time. The worn surface is smooth and black, indicating that the graphite is being smeared onto the surface, providing a self-lubricating effect. In contrast, the cladding layer produced by conventional GMAW has a friction coefficient of about 1.4, which increases with time, and the worn surface shows typical abrasive wear features such as grooves and ploughing.

The paper also reports that the friction coefficient is related to the welding parameters. A lower auxiliary current (the current used to heat the wire) results in a lower friction coefficient, which is attributed to a better retention of the graphite phase.

Practical Considerations and Lessons Learned

From a practical standpoint, this paper raises several important points:

In one application I was involved in, we used a similar approach to produce a self-lubricating cladding on a bearing surface. The results were promising, but we found that the process was sensitive to the wire quality and the welding parameters. It is essential to work with a reliable wire supplier and to develop a robust welding procedure.

Study Insights and Implications

This paper is a valuable reference for anyone involved in the development or application of self-lubricating cladding materials. The key takeaways are:

In summary, this paper demonstrates the successful development of a self-lubricating wear-resistant cladding using a novel welding process. It is a good example of how process innovation can lead to new materials with improved performance, and it provides valuable insights for engineers working in the field of surface engineering and tribology.