Transfer Coefficients of Alloying Elements in Manual Arc Surfacing Electrodes
Core Findings and Experimental Scope
This 1995 study from the Welding Journal addresses a question that still troubles every shop floor that builds up worn parts: how much of the alloying element you put into the electrode coating actually ends up in the deposit. The authors conducted thermodynamic analysis of the welding metallurgical process and developed manual arc surfacing electrodes that rely on the coating to transfer alloy elements. The experimental work covered basic coating types with high and medium carbon W-Cr-Mo-V and Cr-Mo-V-Si alloy systems. The key numbers are worth memorizing: tungsten, molybdenum, chromium, vanadium and silicon achieved transfer coefficients of 0.8 to 0.9. Carbon behaved differently, with coefficients ranging from 0.32 to 0.65 depending on the morphology of graphite added to the coating. The authors also corrected the commonly used formula for electrode coating weight coefficient so it could be applied to the design of high-alloy coating electrodes.
Metallurgical Interpretation and Practical Implications
The high transfer coefficients for W, Mo, Cr, V and Si are no accident. These elements form stable oxides that are easily reduced by the deoxidizers in the coating, and they have limited affinity for nitrogen. The real lesson here is that you cannot simply add more alloy to the coating and assume linear transfer. The carbon story is the one that bites people on site. Carbon acts as a deoxidizer at welding temperatures, and its transfer depends heavily on the form of graphite. If you use flake graphite, you get one transfer behavior; if you use a different morphology, you get another. I have seen hardfacing electrodes where the specified carbon content in the deposit was wildly off from the certificate because the electrode manufacturer did not control graphite morphology. The correction of the coating weight coefficient formula is a practical gift. For high-alloy coatings, the old formula underestimated the amount of coating needed to achieve a given deposit composition. The corrected formula lets you design the electrode with confidence.
Engineering Practice and Lessons Learned
On the plant floor, this paper tells you three things. First, when you specify a hardfacing electrode for a W-Cr-Mo-V system, you can expect roughly 85 percent of the intended alloy to transfer, so design your deposit chemistry accordingly. Second, never rely on carbon as an alloying element without knowing the graphite form in the coating. Third, if you are buying electrodes from a new supplier, ask for their coating weight coefficient calculation and verify it against the corrected formula. I once rejected a batch of surfacing electrodes because the deposit hardness was 8 HRC below specification. The root cause was the supplier using a different graphite source without adjusting the coating formula. The corrected formula in this paper would have caught that discrepancy during design review.
Summary
This paper is a compact but critical reference for anyone who designs or specifies manual arc surfacing electrodes. The transfer coefficient data for W, Mo, Cr, V and Si provide a solid baseline for deposit chemistry prediction, while the carbon transfer behavior highlights a subtle but costly variable. The corrected coating weight coefficient formula is a practical tool that belongs in every electrode design manual. For the industry veteran, the real value is in recognizing that alloy transfer is not a simple linear process, and that the coating formulation must be treated as a metallurgical system in its own right.
Zhuojin Pipe Fitting Co., Ltd