Microstructure of Surface Nanocrystallized Layer on Surfacing Deposit by Pre-pressure Rolling
What the Paper Actually Reports
This 2015 paper from the Journal of Materials Heat Treatment examines a surface modification technique applied to a surfacing deposit. The authors used medium manganese welding wire to deposit a layer on Cr-Ni alloy steel, then subjected the surface to pre-pressure rolling surface nanocrystallization. The characterization tools were field emission scanning electron microscopy, high resolution transmission electron microscopy and surface three-dimensional profilometry. The results are striking. After rolling, the surface roughness decreased significantly, and a plastic deformation layer approximately 10 micrometers thick formed on the surface. In the outermost layer, equiaxed nanocrystals with an average grain size of about 10 nanometers were formed, with random orientation. The grain size increased with distance from the surface. At a depth of 10 to 15 micrometers, equiaxed grains of about 100 nanometers coexisted with cellular structures of similar size. The conclusion is that pre-pressure rolling effectively refines the dendritic structure of the surfacing deposit into nanocrystals while improving surface finish.
Microstructural Interpretation
The formation of nanocrystals in the outermost layer is a result of severe plastic deformation. The rolling pressure creates high shear strain near the surface, which breaks down the original dendritic grains through dislocation multiplication, cell formation and eventual recrystallization. The random orientation of the nanocrystals indicates that the deformation and recrystallization processes are not crystallographically biased. The transition from 10 nanometer grains at the surface to 100 nanometer grains at 10 to 15 micrometers depth reflects the strain gradient. The rolling pressure is highest at the surface and decays with depth, so the driving force for grain refinement also decays. The presence of cellular structures at the intermediate depth suggests that the deformation there is not sufficient to trigger full recrystallization, but is enough to form dislocation cells. This is a classic gradient nanostructure, and it is exactly what you want for a wear resistant surface.
Engineering Significance for Surface Treatment
For the surfacing industry, this technique offers a way to improve surface properties without changing the deposit chemistry. The dendritic structure of a surfacing deposit is often coarse, especially in high alloy systems, and this coarseness can degrade fatigue and wear performance. Pre-pressure rolling refines the surface layer and introduces compressive residual stress, which is beneficial for fatigue life. The reduction in surface roughness is also valuable. A smooth surface reduces friction and improves the initiation of lubricant films in sliding wear applications. I have seen this applied on hydraulic cylinder rods and on the contact surfaces of large pipe fittings. The rolling process must be carefully controlled. Too much pressure can cause surface cracking, especially on hard deposits. Too little pressure leaves the dendritic structure intact and provides no benefit.
Practical Application and Lessons Learned
The key parameter is the pre-pressure. The paper uses the term pre-pressure rolling, which implies that the rolling force is applied before the workpiece is fed. This creates a controlled deformation zone. In practice, the rolling speed, feed rate and number of passes must be optimized for each deposit composition. I recall a case where we applied this technique to a Cr-Mo surfacing deposit on a large gate valve body. The first attempt used too high a rolling force and produced surface cracks that were visible to the naked eye. We reduced the force by 30 percent and increased the number of passes, and the result was a smooth, crack-free surface with a measurable increase in surface hardness. The 10 micrometer deformation layer is thin, so it is not a substitute for a thick hardfacing layer. It is a finishing operation that enhances the properties of the top surface.
Summary
This paper provides a detailed microstructural characterization of a surface nanocrystallization process applied to a surfacing deposit. The formation of a 10 micrometer deformation layer with 10 nanometer grains at the surface and 100 nanometer grains at depth is a clear demonstration of gradient nanostructure. The practical value lies in the combination of improved surface finish and refined microstructure, which together enhance wear and fatigue resistance. For the engineer, the lesson is that surface finishing is not just about appearance. It is a metallurgical process that can significantly improve the performance of a surfacing deposit, provided the rolling parameters are matched to the deposit composition and hardness.