Numerical Simulation and Validation of Temperature Field in GTAW Flat Surfacing with External Longitudinal Magnetic Field
The Simulation Approach
This 2010 paper from Hot Working Technology addresses a topic that is increasingly relevant to automated welding: how an external magnetic field affects the temperature distribution in gas tungsten arc welding. The authors used ANSYS to simulate the temperature field during GTAW flat surfacing on a plate, with an external longitudinal magnetic field applied. The magnetic field is oriented parallel to the arc axis, which creates a bell-shaped arc due to the interaction between the magnetic field and the arc plasma. The simulation used a simple magnetically controlled welding arc heat source model. The key finding is that the simulated temperature field agrees well with experimental measurements. This validation is crucial. Many simulations look good on paper but fail when compared to actual thermocouple readings or infrared imaging. The authors took the extra step of experimental verification, which gives confidence in the model.
Model Validation and Findings
The bell-shaped arc is a well-known phenomenon. When a longitudinal magnetic field is applied, the charged particles in the arc plasma experience a Lorentz force that causes them to spiral around the arc axis. This constricts the arc and increases its energy density. The result is a narrower, deeper weld pool. The simulation captured this effect by using a heat source model that accounts for the magnetic field's influence on arc shape. The agreement between simulation and experiment is described as basically consistent. This means the model can be used to predict the temperature field for different magnetic field strengths and welding parameters. The practical implication is that you can optimize the magnetic field strength to achieve the desired penetration and heat affected zone size without running dozens of trial welds.
Practical Relevance for Magnetic Arc Control
Magnetic arc control is not a laboratory curiosity. It is used in production to improve weld penetration, stabilize the arc, and reduce defects. In pipe welding, especially for small diameter, thin wall pipe, an external magnetic field can help achieve full penetration without burn-through. In surfacing applications, a longitudinal magnetic field can help control dilution by reducing the depth of penetration while maintaining a smooth bead profile. The simulation tool described in this paper allows you to predict the temperature field and, by extension, the weld pool shape and cooling rate. This is valuable for selecting welding parameters for a new application. I have used magnetic arc control on a production line welding stainless steel pipe to carbon steel pipe. The magnetic field stabilized the arc and reduced spatter, which improved the surface quality of the weld and reduced post-weld cleaning time.
Engineering Practice and Lessons Learned
The lesson from this paper is that simulation is a tool, not a substitute for experience. The model must be validated against actual measurements, and the boundary conditions must reflect real welding conditions. I have seen simulations that used a perfect Gaussian heat source and predicted a temperature field that was completely different from reality. The authors here used a more sophisticated model that accounts for the magnetic field, and they validated it. That is the right approach. On the shop floor, the key parameters are the magnetic field strength, the welding current, the arc length and the travel speed. The simulation helps you understand how these parameters interact, but you still need to verify the result with a test weld and a metallographic cross-section.
Summary
This paper demonstrates that numerical simulation of the temperature field in GTAW with an external longitudinal magnetic field can be accurate enough for engineering purposes. The bell-shaped arc model, combined with experimental validation, provides a reliable tool for predicting thermal behavior. For the welding engineer, the practical value is in optimizing magnetic field parameters to control penetration, weld pool shape and heat affected zone size without extensive trial and error. The paper also serves as a reminder that simulation must always be grounded in experimental reality.
Zhuojin Pipe Fitting Co., Ltd