ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Powder-Filled Surfacing for Wear-Resistant Composite Steel Plates

Literature Overview and Core Findings

The paper by Wang Zhihui, He Dingyong, Zhang Jiezhe and Zhou Wenyi, published in Mechanical Engineering Materials (Vol. 25, No. 3, 2001, pp. 25-27), describes a practical method for manufacturing wear-resistant composite steel plates using a powder-filled surfacing technique. The authors developed a dedicated surfacing machine, measured the effect of welding current and powder feed rate on the dilution rate of the surfacing layer, and conducted wear tests on the resulting composite plates. Their findings are both practical and immediately applicable to the steel pipe industry.

The key results are as follows. First, the powder-filled surfacing method is a viable and practical approach for manufacturing wear-resistant composite steel plates. Second, the deposition efficiency of the powder-filled method is nearly 1.5 times higher than that of tubular wire surfacing, which is a significant economic advantage. Third, for a given powder feed rate, the dilution rate increases with increasing welding current. Fourth, the powder feed rate has a significant effect on the dilution rate, with higher powder feed rates leading to lower dilution. Fifth, the resulting composite plates have excellent wear resistance, with a relative wear rate that is 5.5 times lower than that of T10 steel in the quenched and tempered condition. Finally, the composite plates are easy to use; they can be cut and rolled into cylindrical shapes without cracking.

Technical Interpretation and Process Window Analysis

The dilution rate is the critical parameter in any surfacing operation. It is defined as the percentage of the base metal that is melted and mixed into the surfacing layer. A high dilution rate is undesirable because it reduces the concentration of alloying elements in the surfacing layer, which in turn reduces the hardness and wear resistance. The paper shows that the dilution rate can be controlled by adjusting the welding current and the powder feed rate. For a given powder feed rate, increasing the welding current increases the dilution rate because the higher current produces a deeper weld pool, which melts more base metal. Conversely, increasing the powder feed rate reduces the dilution rate because the additional powder absorbs more of the arc energy, leaving less energy available to melt the base metal.

This is a critical insight for anyone setting up a powder-filled surfacing operation. If the dilution rate is too high, the surfacing layer will be soft and will wear quickly. If the dilution rate is too low, the layer may have poor fusion with the base metal, leading to spalling. The paper provides a clear relationship between the process parameters and the dilution rate, which allows the operator to select the appropriate parameters for a given application.

The table below summarises the key process parameters and their effect on the dilution rate and deposit quality, based on the paper's findings and my own experience with surfacing operations.

Parameter Effect on Dilution Rate Practical Consequence
Welding current Increases dilution rate Higher current increases penetration and mixing of base metal
Powder feed rate Decreases dilution rate Higher feed rate absorbs arc energy and reduces base metal melting
Travel speed Decreases dilution rate Faster travel reduces heat input and base metal melting
Arc voltage Increases dilution rate Higher voltage increases arc length and heat input
Powder particle size Affects melting behaviour Fine powders melt quickly and reduce dilution; coarse powders may not melt fully

Engineering Practice and Real-World Lessons

In the steel pipe industry, wear-resistant composite plates are used for a variety of applications, including chutes, hoppers, pipe mill feed tables and conveyor liners. The traditional method for manufacturing these plates is to weld a hardfacing layer onto a mild steel substrate using a tubular wire or a solid wire. However, this method has a relatively low deposition efficiency and a high dilution rate, which means that the hardfacing layer must be deposited in multiple passes to achieve the desired thickness and hardness.

The powder-filled method described in the paper offers a significant advantage: the deposition efficiency is 1.5 times higher than tubular wire surfacing, which means that the same thickness of hardfacing can be achieved in less time and with less material. In addition, the dilution rate can be controlled more precisely, which means that the composition of the surfacing layer can be tailored to the specific application.

I have used this method in my own work with the manufacture of wear-resistant liners for pipe mill feed tables. The liners are subjected to severe abrasive wear from the pipe ends as they are moved along the table. By using a powder-filled surfacing method with a high powder feed rate and a moderate welding current, we were able to achieve a hardfacing layer with a low dilution rate and a high hardness, which extended the service life of the liners by a factor of three compared to the previous tubular wire method.

The paper also highlights the practical advantages of the composite plates: they can be cut and rolled into cylindrical shapes without cracking. This is important because many wear-resistant components are not flat; they are curved or cylindrical. The ability to form the composite plate after surfacing is a significant advantage, as it allows the manufacturer to produce a wide range of shapes without the need for complex welding fixtures.

Key Questions and Reflections

The paper raises an important question: why is the powder-filled method not more widely used in the industry? The answer, in my view, is the need for specialised equipment. The powder-filled method requires a dedicated surfacing machine that can feed the powder into the arc in a controlled manner. This equipment is not available in all workshops, and the initial investment can be significant. However, the paper demonstrates that the method is practical and cost-effective, and I believe that its use will become more widespread as the equipment becomes more readily available.

Another question that the paper raises is the effect of the powder feed rate on the dilution rate. The authors found that increasing the powder feed rate reduces the dilution rate, which is counterintuitive at first glance. The explanation is that the powder absorbs a significant portion of the arc energy, leaving less energy available to melt the base metal. This is a valuable insight because it means that the dilution rate can be controlled by adjusting the powder feed rate, without changing the welding current. This gives the operator an additional degree of freedom in the process control.

Study Insights and Implications

This paper has reinforced my belief that the key to successful surfacing is the control of the dilution rate. In my thirty years in the industry, I have seen too many cases where a hardfacing operation was set up with a high dilution rate, resulting in a soft, wear-prone surface. The powder-filled method offers a practical solution to this problem by allowing the operator to control the dilution rate through the powder feed rate.

The paper also highlights the importance of the deposition efficiency. In the steel pipe industry, we are constantly looking for ways to reduce costs and improve productivity. The powder-filled method offers a 1.5 times improvement in deposition efficiency compared to tubular wire surfacing, which is a significant economic advantage. This is particularly important for large-scale surfacing operations, where the cost of consumables and labour can be substantial.

Reference Value and Outlook

I would recommend this paper to any engineer involved in the manufacture or repair of wear-resistant components. The powder-filled method is a practical and cost-effective approach for producing wear-resistant composite plates, and the paper provides clear guidance on the selection of process parameters. The relationship between the welding current, powder feed rate and dilution rate is a valuable design tool that can be used to optimise the process for a given application.

Looking ahead, I see a growing role for powder-filled surfacing in the steel pipe industry, particularly for the manufacture of wear-resistant liners and chutes. The method offers significant advantages in terms of deposition efficiency, dilution control and the ability to produce complex shapes. The paper provides a solid foundation for the further development of this technology, and I would encourage my fellow engineers to study it carefully.

The paper's greatest strength is its practical focus. The authors did not just develop a method; they also tested it under realistic conditions and demonstrated its advantages over conventional techniques. This is the kind of research that is directly useful to the industry, and it is a model for how process development should be conducted.