ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Study on the Relationship Between Temperature Field and Microstructure-Property in CNC Surfacing Additive Manufacturing

Literature Overview and Core Concept

This paper, published in Welding journal by Zhang Yu, Luo Zhen, Li Yang, and Bi Jing from Tianjin University, presents a finite element analysis of the temperature field distribution and thermal cycling characteristics during CNC surfacing additive manufacturing of thin-walled components. The work is supported by a doctoral fund from the Ministry of Education, indicating its fundamental research nature. The authors established a three-dimensional heat transfer model to simulate the temperature field and thermal cycles during the build-up process, and correlated the results with the observed microstructure and mechanical properties.

Additive manufacturing using welding arcs as the heat source (wire arc additive manufacturing, WAAM) has gained significant attention in recent years as a cost-effective method for producing large metal components. The process involves depositing weld metal layer by layer to build up a three-dimensional shape. The thermal history of each layer is complex: each new layer reheats the previously deposited layers, creating a unique thermal cycle that affects the final microstructure and properties.

Technical Interpretation of Thermal Cycles and Microstructure Evolution

The paper's key finding is that during the stacking process, previously deposited weld metal is repeatedly reheated, with the peak temperature decreasing as the heat source moves away. This thermal cycling has a profound effect on the microstructure. The authors found that in the interior of the workpiece, the peak temperature of the thermal cycle reaches above the complete austenitization temperature of the material, causing complete recrystallization during subsequent cooling. This results in a fine, uniform microstructure consisting of fine ferrite and intergranular pearlite.

In contrast, the end regions of the workpiece, which experience fewer thermal cycles and different peak temperatures, show a different microstructure consisting of proeutectoid ferrite and lath martensite. This is because the thermal cycle in these regions does not reach the complete austenitization temperature, so the original microstructure is not fully transformed.

The difference in microstructure between the interior and the end regions has significant implications for mechanical properties. The fine, uniform microstructure in the interior should provide good strength and toughness, while the lath martensite in the end regions may be harder but more brittle. This inhomogeneity is a concern for additive manufacturing, where the goal is to achieve uniform properties throughout the component.

Practical Implications for Additive Manufacturing

From a practical standpoint, this paper highlights the importance of understanding thermal history in additive manufacturing. The thermal cycles determine the final microstructure, which in turn determines the mechanical properties. If the process parameters (heat input, deposition rate, layer thickness, interlayer temperature) are not carefully controlled, the resulting component will have non-uniform properties, which can lead to premature failure in service.

The key process parameters that affect the thermal history are:

  1. Heat input: Higher heat input increases the peak temperature and the size of the heat-affected zone, but also increases distortion and residual stress.
  2. Interlayer temperature: The temperature of the workpiece before each new layer is deposited determines the cooling rate and the resulting microstructure. A higher interlayer temperature reduces the cooling rate, which can lead to coarser grains and softer material.
  3. Layer thickness: Thicker layers reduce the number of thermal cycles but increase the heat input per layer, which can cause excessive grain growth.
  4. Travel speed: Faster travel speed reduces the heat input per unit length, but can cause lack of fusion or porosity.

Engineering Practice Insights and Lessons Learned

In my experience with welding-based additive manufacturing, the most critical factor is controlling the interlayer temperature. If the interlayer temperature is too low, the cooling rate is too fast, which can cause hard, brittle microstructures and cracking. If it is too high, the material becomes soft and the grains grow excessively.

I recall a project where we were building up a large valve body using WAAM with a low-alloy steel wire. The initial trials produced a component with acceptable surface quality, but the mechanical properties were inconsistent. Tensile tests showed significant scatter, and some samples failed at the layer boundaries. We investigated the microstructure and found that the layer boundaries had coarse grains and some porosity, which was caused by inadequate fusion between layers.

The solution was to implement a controlled interlayer temperature using a thermocouple and an interlayer cooling system. We also adjusted the travel speed and the wire feed rate to achieve better fusion. After these changes, the mechanical properties became more consistent, and the failure mode changed from brittle fracture at layer boundaries to ductile fracture in the base material.

This experience underscores the importance of the thermal management approach described in this paper. The finite element model can be used to predict the thermal history and optimize the process parameters before actual deposition, saving time and material.

Summary and Reflection

This paper provides valuable insight into the relationship between thermal history and microstructure in welding-based additive manufacturing. The finding that the interior of the workpiece undergoes complete recrystallization due to repeated thermal cycling, while the end regions show a different microstructure, is important for understanding the property variations in additively manufactured components.

From my perspective, the practical implication is clear: to achieve uniform properties in additively manufactured components, the thermal history must be carefully controlled. This requires a thorough understanding of the heat transfer during deposition, which can be obtained through finite element modeling. The paper's approach of correlating the simulated temperature field with the observed microstructure provides a solid foundation for process optimization.

I would recommend that any engineer involved in welding-based additive manufacturing invest in developing a reliable thermal model for their specific process and material combination. This model can then be used to optimize process parameters and ensure consistent, high-quality components.