In-Situ Ceramic Phase Reinforced Fe-Based Hardfacing by Plasma Surfacing
Introduction
The paper by Zong Lin and Liu Zhengjun explores the use of plasma surfacing to create an in-situ ceramic phase reinforced iron-based hardfacing layer. The approach is to precoat a mixture of high carbon ferrochrome, ferrovanadium, and graphite on a carbon steel substrate, then apply plasma arc to melt the coating and the substrate surface. The result is a composite layer with hard carbides dispersed in a martensitic matrix. This is a clever way to avoid the need for expensive pre-alloyed powders.
Technical Analysis
The precoating composition determines the final microstructure. The authors used a mixture that, after melting, forms (Fe,Cr,V)7C3 and VC. The primary (Fe,Cr,V)7C3 carbides are hexagonal and relatively large, while VC particles are finer and agglomerated or spherical. The matrix is martensite with some retained austenite. The hardness distribution shows a gradient from the substrate to the surface, which is beneficial for wear resistance: the surface is hard, while the transition zone maintains some toughness.
The key parameters are the precoating thickness, the plasma arc current, and the travel speed. These affect dilution and the final carbide volume fraction. Too much dilution reduces the carbide content and hardness; too little may result in poor bonding. The paper reports good metallurgical bonding, which is essential for any hardfacing.
Practical Implications
In-situ synthesis is attractive because it uses relatively cheap raw materials and can be tailored to specific wear conditions. In my experience, this type of hardfacing is well suited for crusher hammers, mining teeth, and other components that suffer from severe abrasive wear. However, the precoating process is not always practical for complex shapes or large components. It works best on flat or simple curved surfaces.
One issue I have seen with in-situ carbide hardfacing is the formation of cracks due to the high hardness and the difference in thermal expansion between the carbides and the matrix. The paper does not discuss crack resistance, but in practice, we must control the cooling rate and possibly use a preheat or post-weld heat treatment. Also, the size and distribution of carbides are critical: coarse carbides can act as crack initiation sites, while fine, uniformly dispersed carbides give better wear resistance.
Conclusion
The in-situ synthesis of ceramic phases in an iron-based matrix is a cost-effective way to produce wear-resistant hardfacing. The paper provides a good foundation for understanding the microstructure and hardness gradient. For the shop floor, the main challenges are controlling dilution and avoiding cracking. I would recommend that any application of this process be validated with metallographic examination and wear testing on actual components, not just coupons. The hardness gradient is a positive feature, but it must be consistent across the entire surface to avoid premature failure.