Magnetic Control Technology for Stainless Steel Strip Electroslag Surfacing

The Undercut Problem

This paper addresses a persistent problem in strip electroslag surfacing: undercut and poor bead formation. When surfacing with a wide strip electrode, the electromagnetic forces generated by the welding current can cause the molten metal to be pushed away from the edges of the strip, resulting in undercut at the bead edges. This is a serious quality issue because undercut creates stress concentrations and reduces the effective cross-section of the deposit.

The authors investigated two types of magnetic control devices: a coil-type external magnetic field and a fixed-core self-induction magnetic field. The coil-type device uses an external coil to generate a magnetic field that counteracts the electromagnetic forces in the weld pool. The fixed-core device uses a ferromagnetic core to shape the magnetic field distribution. Both approaches are designed to control the molten metal flow and improve bead formation.

The authors developed and tested both types of devices, then proposed a reasonable device structure and the main process parameters. They also examined the effects of magnetic pole position, welding material, and welding parameters on the magnetic control effect. This is a systematic approach to a practical problem, and the results are directly applicable to production.

Magnetic Control Approaches

The two types of magnetic control devices have different characteristics. The coil-type external magnetic field provides a flexible and adjustable magnetic field, but it requires an external power source and is more complex to implement. The fixed-core self-induction magnetic field is simpler and more robust, but it is less flexible because the magnetic field distribution is determined by the core geometry.

Control Device Type Advantages Limitations Application Suitability
Coil-type external magnetic field Adjustable field strength and direction Requires external power source and control system Suitable for applications requiring fine control
Fixed-core self-induction magnetic field Simple, robust, no external power needed Field distribution fixed by core geometry Suitable for production where consistent conditions prevail
Magnetic pole position Determines the field distribution relative to the weld pool Must be optimized for each application Critical parameter for effective control
Welding material Affects the electromagnetic force and molten metal behavior Different materials require different magnetic parameters Must be matched to the consumable and substrate
Welding parameters Affect the heat input and molten metal volume Interacts with magnetic field strength Must be coordinated with magnetic control settings

The magnetic pole position is a critical parameter. The magnetic field must be positioned so that it counteracts the electromagnetic forces at the edges of the weld pool. If the poles are too far from the weld pool, the field strength is insufficient. If they are too close, the field may cause other defects such as arc blow. The authors found that the optimal pole position depends on the strip width and the welding current.

The welding material also affects the magnetic control effect. Different stainless steel compositions have different electrical and magnetic properties, which influence the electromagnetic forces in the weld pool. The authors found that the magnetic control parameters must be adjusted for each material to achieve the best results.

Practical Considerations for Strip Surfacing

In my experience, strip electroslag surfacing is a high-productivity process that is widely used for cladding pressure vessels, heat exchangers, and other large components. The undercut problem is a common issue that can lead to rework and extended production times. Magnetic control offers a practical solution, but it requires careful setup and optimization.

The key is to understand the interaction between the magnetic field and the weld pool. The electromagnetic forces in the weld pool are caused by the interaction between the welding current and the magnetic field generated by that current. These forces tend to push the molten metal toward the center of the strip, creating undercut at the edges. An external magnetic field can counteract these forces, but the field strength and direction must be carefully controlled.

The authors' work shows that both coil-type and fixed-core devices can be effective, but the choice depends on the application. For production where the conditions are consistent, the fixed-core device is simpler and more reliable. For applications where the conditions vary, the coil-type device offers more flexibility.

The process parameters must also be coordinated with the magnetic control settings. The welding current, voltage, and travel speed all affect the weld pool size and the electromagnetic forces. The magnetic field strength must be adjusted to match these parameters. This requires a systematic approach to process development, which the authors have demonstrated.

Conclusion

This study provides a practical solution to the undercut problem in strip electroslag surfacing. The magnetic control devices developed and tested by the authors are effective in improving bead formation and eliminating undercut. The key parameters are the magnetic pole position, the welding material, and the welding parameters, all of which must be optimized for each application. For engineers involved in strip surfacing, this is a valuable reference that can help reduce rework and improve product quality. The magnetic control approach can be extended to other surfacing processes where electromagnetic forces cause similar problems.