Effect of Longitudinal Intermittent Alternating Magnetic Field on Plasma Arc Surfacing Metal

Research Motivation

This paper investigates the effect of a longitudinal intermittent alternating magnetic field on the microstructure and properties of plasma arc surfacing metal. The motivation is to improve the mechanical properties of the weld deposit by controlling the solidification process. In plasma arc surfacing, the rapid cooling and solidification of the molten pool can result in coarse grain structures and non-uniform phase distributions, which degrade the mechanical properties.

The authors applied a longitudinal intermittent alternating magnetic field during plasma arc surfacing of Fe5 alloy powder onto low carbon steel. They used optical metallography, X-ray diffraction, microhardness testing, and wet sand rubber wheel wear testing to characterize the deposits under different magnetic field parameters.

The concept is that an external magnetic field can influence the solidification process by inducing convection in the molten pool and by affecting the nucleation and growth of grains. The intermittent nature of the magnetic field adds another level of control, allowing the solidification to be influenced in a more complex way than a steady magnetic field.

Microstructural and Property Changes

The results showed that the magnetic field can significantly affect the microstructure and properties of the deposit. Under appropriate magnetic field parameters, the number of hard phases in the deposit increased, and the growth direction of these phases was controlled. This resulted in increased hardness and wear resistance.

The mechanism is related to the effect of the magnetic field on the solidification process. The magnetic field induces convection in the molten pool, which breaks up the growing dendrites and promotes the formation of more nucleation sites. This leads to grain refinement. The magnetic field also affects the orientation of the growing grains, which can be beneficial if the hard phases are aligned in a direction that resists wear.

Magnetic Field Parameter Effect on Microstructure Effect on Properties
Field strength Controls the intensity of convection and grain refinement Higher strength generally increases refinement and hardness
Frequency Affects the oscillation of the molten pool Optimal frequency maximizes the refinement effect
Intermittent duty cycle Determines the duration of the magnetic field application Allows control of the solidification sequence
Field direction Influences the orientation of the growing grains Can align hard phases in a beneficial direction

The X-ray diffraction analysis showed that the magnetic field increased the amount of hard phases in the deposit. This is significant because the hard phases are responsible for the wear resistance. The microhardness testing confirmed that the hardness increased with the appropriate magnetic field parameters. The wet sand rubber wheel wear testing showed a corresponding increase in wear resistance.

The authors concluded that the magnetic field can improve the crystallization morphology of the deposit metal and refine the grains. This is a fundamental finding that has broad implications for plasma arc surfacing and other welding processes where solidification control is important.

Practical Implications for Surfacing

From a practical standpoint, the application of a magnetic field during plasma arc surfacing offers a way to improve the properties of the deposit without changing the chemical composition. This is particularly valuable when the composition is fixed by the application requirements, but the microstructure can be optimized through the magnetic field.

The intermittent nature of the magnetic field is an interesting innovation. By varying the duty cycle, the engineer can control the solidification sequence and tailor the microstructure to the specific application. For example, in a wear-resistant coating, the magnetic field can be adjusted to maximize the amount of hard phases and align them in the direction of wear.

The practical implementation of magnetic field control requires careful design of the magnetic field source and the control system. The magnetic field must be positioned correctly relative to the molten pool, and the field parameters must be synchronized with the welding process. This adds complexity to the surfacing operation, but the potential benefits in terms of improved properties justify the investment.

In the steel pipe industry, plasma arc surfacing is used for a variety of applications, including the application of wear-resistant coatings on rolls and other components. The ability to improve the properties of these coatings through magnetic field control is a significant advantage.

Conclusion

This study demonstrates that a longitudinal intermittent alternating magnetic field can effectively improve the microstructure and properties of plasma arc surfacing metal. The magnetic field promotes grain refinement, increases the amount of hard phases, and controls their growth direction, resulting in increased hardness and wear resistance. The practical implications are significant: magnetic field control offers a way to optimize the properties of surfacing deposits without changing the chemical composition. For engineers involved in plasma arc surfacing, this is a valuable technique that can improve product quality and extend service life. The intermittent magnetic field approach can be extended to other welding and surfacing processes, making it a versatile tool for microstructure control.