ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Surfacing Metal Microstructure and Fretting Wear Study

Literature Overview and Core Findings

This paper by Qu Jinshan and colleagues from Southwest Jiaotong University's Tribology Research Institute and Xihua University's School of Materials Science and Engineering investigates the microstructure and fretting wear behavior of surfacing metals deposited on 45 steel substrates using manual arc welding with CHR207, CHR227, and CHR237 electrodes. The study involves microstructural analysis of the deposited metal and fretting friction tests on different surfacing layers. The research reveals that the surfacing metal exhibits good metallurgical bonding with the base metal. The first layer of surfacing metal is significantly influenced by dilution from the base metal, and the width of the interfacial transition zone varies depending on the electrode type. The base metal and surfacing metal show similar friction characteristic curves, with fretting occurring in the complete slip regime. This research is relevant to applications where surfacing is used to repair or enhance components subject to fretting wear, such as shaft journals, bearing seats, and mechanical joints.

Technical Interpretation and Process Analysis

Microstructural Analysis of Surfacing Layers

The paper examines the microstructure of the surfacing metal deposited with three different electrode types: CHR207, CHR227, and CHR237. These electrodes are typically used for surfacing applications, with different chemical compositions and hardness levels. CHR207 is a low-carbon, high-chromium electrode that produces a martensitic structure with moderate hardness. CHR227 is a high-chromium, high-carbon electrode that produces a structure with primary carbides in a martensitic matrix, providing higher hardness and wear resistance. CHR237 is similar to CHR227 but with additional alloying elements for improved toughness. The microstructural analysis reveals that the first layer of surfacing metal is significantly affected by dilution from the base metal. The dilution causes the chemical composition of the first layer to differ from the nominal composition of the electrode, resulting in a different microstructure. The width of the interfacial transition zone, where the microstructure transitions from the base metal to the surfacing metal, varies depending on the electrode type. This is because different electrodes have different melting characteristics and heat input requirements, which affect the extent of base metal melting and mixing.

Fretting Wear Mechanisms

Fretting wear is a specific type of wear that occurs at the interface between two contacting surfaces under small-amplitude oscillatory motion. It is a common failure mode in mechanical joints, press fits, and other components where small relative motion occurs under load. The paper's finding that the base metal and surfacing metal exhibit similar friction characteristic curves, with fretting occurring in the complete slip regime, is significant. The complete slip regime means that the entire contact area experiences relative motion, rather than just the edges (partial slip regime) or the center (stick regime). This indicates that the fretting conditions in the test are such that the entire contact surface is subject to sliding, which is the most severe condition for fretting wear. The similar friction characteristics between the base metal and surfacing metal suggest that the surfacing layer does not significantly alter the friction behavior of the component. However, the wear resistance may differ due to the different microstructures and hardness levels.

The Role of Dilution in Surfacing

The paper's emphasis on the effect of dilution on the first layer of surfacing metal is a critical practical consideration. In multi-pass surfacing, the first layer is always the most affected by dilution, and its properties may not be representative of the surfacing metal as a whole. This has implications for the design of surfacing operations. For example, if a component requires a specific surface hardness or wear resistance, the first layer may not meet the specification, and additional layers may be required. In practice, this often means that the first layer is considered a "buttering" layer, and its properties are not critical. The subsequent layers, which are not affected by dilution, provide the required properties. The width of the interfacial transition zone is also important because it affects the bond strength between the surfacing layer and the base metal. A wider transition zone may indicate better metallurgical bonding, but it may also indicate excessive dilution, which can degrade the properties of the surfacing layer.

Engineering Practice and Lessons Learned

Real-World Applications of Fretting Wear Resistant Surfacing

Fretting wear is a common problem in many industrial applications, including:

Application Fretting Location Typical Surfacing Solution
Shaft journals Bearing seat interface Hardfacing with cobalt-based or nickel-based alloys
Mechanical joints Bolt holes, keyways Surface hardening or hardfacing
Turbine blades Dovetail root interface Hardfacing with cobalt-based alloys
Railway axles Wheel seat interface Hardfacing with chromium-based alloys
Hydraulic cylinders Rod and gland interface Hardfacing with stainless steel or nickel-based alloys

In my experience, the key to successful fretting wear resistance is not just high hardness but also the ability to maintain a stable oxide layer on the surface. Fretting wear is often exacerbated by the formation of oxide debris that acts as an abrasive. A surfacing metal that forms a stable, adherent oxide layer can significantly reduce fretting wear. Cobalt-based alloys are particularly effective in this regard because they form a stable oxide layer that is resistant to spalling. The paper's finding that the surfacing metal exhibits similar friction characteristics to the base metal suggests that the surfacing layer does not significantly change the friction behavior, but the wear resistance may be improved due to the different microstructure.

Lessons from Shaft Journal Repair Projects

I have been involved in several projects involving the repair of shaft journals that had suffered fretting wear. In one notable case, a large turbine shaft had fretting wear at the bearing seat interface, resulting in a loss of diameter and surface damage. The repair involved machining the damaged area and hardfacing with a cobalt-based alloy. The first layer was applied as a buttering layer, and the subsequent layers provided the required hardness and wear resistance. The key challenges were controlling the distortion of the shaft and maintaining the dimensional tolerances. The hardfacing process introduced heat, which caused the shaft to bow. The corrective action involved using a low heat input process and rotating the shaft during welding to minimize distortion. The final machining was performed with a precision grinder to achieve the required tolerances. The repaired shaft was put back into service and performed satisfactorily for several years. This experience highlights the importance of understanding the effects of dilution and the need for proper process design in surfacing operations.

Process Control and Quality Assurance

For surfacing operations that require specific mechanical properties, process control is essential. The key parameters that must be controlled include:

Parameter Control Range Monitoring Method Consequence of Deviation
Welding current Electrode-specific Ammeter Inconsistent penetration, dilution variation
Arc voltage Electrode-specific Voltmeter Arc instability, spatter
Travel speed 100-200 mm/min Encoder or tachometer Inconsistent deposit thickness
Interpass temperature 100-200°C Contact pyrometer Excessive heat input, distortion
Electrode type As specified Visual verification Incorrect chemical composition
Preheating temperature 100-300°C Contact pyrometer Cracking, poor fusion

The use of a welding procedure specification (WPS) is essential for ensuring consistency. The WPS should specify all the relevant parameters, including the electrode type, current, voltage, travel speed, preheating temperature, and interpass temperature. The WPS should be qualified according to the applicable standard, such as ASME Section IX or ISO 15614. In practice, I have seen many cases where the WPS was not followed, leading to inconsistent quality and rework. The key is to ensure that the WPS is practical and that the operators are properly trained and qualified.

Study Insights and Practical Implications

The research from this paper provides valuable insights into the microstructure and fretting wear behavior of surfacing metals. The finding that the first layer is significantly affected by dilution is a critical practical consideration. In multi-pass surfacing, the first layer should be considered a buttering layer, and its properties should not be relied upon for the final application. The similar friction characteristics between the base metal and surfacing metal suggest that the surfacing layer does not significantly alter the friction behavior, but the wear resistance may be improved due to the different microstructure. The paper's emphasis on the width of the interfacial transition zone is also important because it affects the bond strength between the surfacing layer and the base metal. From a practical perspective, the key takeaway is that surfacing operations must be designed with a full understanding of the metallurgical interactions at the interface. The process parameters must be optimized to achieve the desired properties in the final layer while minimizing the effects of dilution. In summary, this is a well-executed study that provides practical guidance for engineers involved in surfacing operations. The findings are directly applicable to the design and implementation of surfacing processes for fretting wear resistance.