ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Effect of Low-Frequency Longitudinal Magnetic Field on Hardness and Wear Resistance of Surfacing Layer

Literature Overview and Core Findings

This paper by Lu Lin and colleagues from Shenyang University of Technology investigates the effect of an external low-frequency longitudinal magnetic field on the hardness and wear resistance of a surfacing layer produced by submerged arc welding. The authors applied a magnetic field during the surfacing process and varied the excitation current and the magnetic field frequency. The key finding is that with an excitation current of 1.5 A and a magnetic field frequency of 10 Hz, electromagnetic stirring effectively reduces the columnar grain characteristics and increases the hardness of the deposited metal.

This is a classic example of using an external field to modify the solidification microstructure of a weld deposit. In our industry, we care about this because the hardness and wear resistance of a surfacing layer directly determine the service life of components such as valve seats, pump impellers, and pipe fittings that are subject to abrasive or erosive wear.

Interpretation of Technical Points

The mechanism behind the improvement is electromagnetic stirring. When a magnetic field is applied to a molten weld pool, it induces a Lorentz force that causes the liquid metal to circulate. This circulation breaks up the columnar grains that normally grow from the fusion line toward the center of the weld, and it promotes the formation of finer, more equiaxed grains. Finer grains mean more grain boundaries, which impede dislocation motion and increase hardness. The paper reports that the hardness increases with the application of the magnetic field, and the wear resistance improves correspondingly.

The optimal parameters are critical. The paper found that 1.5 A excitation current and 10 Hz frequency gave the best results. At lower currents or frequencies, the stirring effect is too weak to break up the columnar grains. At higher values, the stirring may become turbulent and cause defects such as porosity or slag entrapment. This is a narrow process window, and it requires precise control of the power supply and the coil arrangement.

I want to emphasize that the magnetic field must be longitudinal, meaning the field lines are parallel to the welding direction. A transverse field would have a different effect, possibly causing the weld pool to be pushed to one side. The authors used a longitudinal field, which is the correct approach for improving the solidification structure.

Integration with Engineering Practice

In our pipe fitting and steel pipe business, we use submerged arc welding for a variety of applications, including cladding the inside of pipes and fittings with a corrosion-resistant alloy. The conventional approach is to use a high heat input and a slow travel speed to achieve good fusion, but this often results in a coarse columnar grain structure that has poor toughness and, in some cases, a susceptibility to solidification cracking.

The application of a magnetic field could be a practical way to refine the grain structure without changing the welding parameters. However, I have to consider the practical challenges of implementing this on a production line. The magnetic coil must be positioned close to the weld pool, and it must not interfere with the welding torch or the shielding gas. The power supply for the coil adds complexity, and the coil itself may need to be water-cooled if it is operated continuously.

Another practical consideration is the effect of the magnetic field on the arc. A strong magnetic field can deflect the arc, causing the weld bead to be misplaced or the penetration to be inconsistent. The authors used a low-frequency field, which is less likely to cause arc deflection than a high-frequency field, but it is still a risk. I would want to see the results of a bead-on-plate test with the magnetic field applied, and to measure the bead width and penetration to ensure they are consistent.

Key Questions and Reflections

The most important question for me is whether the improvement in hardness and wear resistance is significant enough to justify the added complexity. The paper does not provide quantitative data on the hardness values or the wear rate, so I cannot make a direct comparison. In my experience, a 10 to 20 percent increase in hardness can translate to a significant improvement in wear life, but it depends on the specific application.

Another question is the effect of the magnetic field on the dilution of the base metal. In a cladding application, we want to minimize dilution to maintain the corrosion resistance of the deposited layer. If the magnetic field increases the stirring and promotes mixing, it might increase dilution, which would be undesirable. The paper does not address this, and I would want to see a dilution measurement before adopting this technique for a corrosion-resistant cladding application.

Study Insights and Implications

This paper is a good example of how a relatively simple modification to the welding process can have a significant effect on the properties of the deposited metal. The concept of electromagnetic stirring is well established in casting and welding, but this paper provides specific data for the submerged arc surfacing process.

For our industry, the most promising application is the hardfacing of components that are subject to abrasive wear, such as the sealing surfaces of valves or the wear plates of pipe fittings. If we can increase the hardness of the hardfacing layer by 10 to 20 percent, we can extend the service life of these components and reduce the frequency of replacement.

However, I would caution against adopting this technique without a thorough qualification program. The process window is narrow, and the equipment is more complex than a standard welding setup. I would recommend starting with a laboratory-scale test to determine the optimal parameters for the specific material and application, and then progressing to a production trial.

Reference Value and Outlook

This paper is a valuable contribution to the field of welding metallurgy and provides a practical insight into the use of magnetic fields to control the solidification structure of weld deposits. The results are specific to the materials and conditions tested, but the underlying principle is applicable to a wide range of welding processes.

In the future, I can see this technique being integrated with robotic welding and real-time process monitoring to achieve consistent quality. The key is to understand the interaction between the magnetic field and the welding arc, and to control it precisely. For now, I would recommend that any engineer considering this route start with a simple bead-on-plate test, measure the hardness and wear resistance, and then progress to a production application.