ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Design of an Automatic Roll Hardfacing Machine: PLC Control and Sequence Logic

Problem Statement and Machine Design Concept

The 2014 paper by Liang Guangrui and colleagues from Guangxi Vocational and Technical College addresses a specific problem in the sugar industry: the wear of sugarcane roller press rolls. The rolls suffer from abrasive wear, which reduces the pressing efficiency and shortens the service life. The authors propose a hardfacing technique that creates a pitted surface on the roll, which improves the grip on the sugarcane and reduces the wear rate. To implement this technique consistently, they designed an automatic hardfacing machine controlled by a programmable logic controller (PLC). The use of a PLC is a significant step forward because manual hardfacing of a large roll is slow, inconsistent, and dependent on the welder's skill. The automatic machine ensures that the welding parameters and the travel speed are controlled precisely, which is essential for producing a uniform pitted pattern.

PLC Control System and Sequence Logic

The heart of the machine is the PLC control system, which follows a sequence function chart (SFC) to coordinate the rotation of the roll, the movement of the welding torch, and the initiation of the arc. The following table summarises the key sequence steps and the associated PLC outputs.

Sequence Step PLC Output Description
1 Start rotation motor The roll begins to rotate at a set speed
2 Move torch to start position The welding torch is positioned at the start of the weld path
3 Initiate welding arc The power source is energised and the arc is established
4 Start torch oscillation The torch oscillates to create the pitted pattern
5 Monitor arc voltage and current The PLC checks that the welding parameters are within tolerance
6 Stop torch oscillation and arc The weld pass is completed
7 Index roll to next position The roll is rotated to the next weld path
8 Repeat steps 3–7 The cycle continues until the roll surface is covered
9 Stop rotation and move torch to home The machine returns to the initial state

The sequence function chart provides a clear and logical method for programming the PLC. The authors report that the machine operates reliably and improves productivity. The key design point is the coordination between the rotation speed and the torch travel speed, which determines the spacing of the pitted pattern. If the rotation is too fast, the pits will be too far apart; if it is too slow, the pits will overlap and the pattern will be lost.

Practical Results and Economic Benefits

The authors report that the hardfaced roll shell hardness increased by 76%, and the wear volume was only 9.9% of that of a non-hardfaced roll. These are impressive numbers, but they need to be interpreted carefully. The hardness increase is a direct result of the hardfacing deposit, but the wear reduction is also influenced by the pitted surface, which reduces the contact area and changes the wear mechanism. The following table presents a comparison of the performance before and after hardfacing.

Parameter Before Hardfacing After Hardfacing Improvement
Surface hardness 30 HRC (typical) 53 HRC (typical) +76%
Wear volume (relative) 100% 9.9% -90.1%
Service life 3 months (typical) 12 months (typical) +300%

The economic benefit is substantial. The cost of the hardfacing consumables and the machine time is a fraction of the cost of replacing the roll. In addition, the automatic machine reduces the labour requirement and improves the consistency of the deposit. For a sugar mill, the ability to extend the roll life by a factor of three or four is a major commercial advantage.

Summary

The paper by Liang Guangrui and colleagues demonstrates the value of automation in hardfacing. The PLC-controlled machine removes the variability of manual welding and produces a consistent pitted pattern that improves the performance of the roll. The sequence function chart is a simple and effective method for programming the control logic. For a production engineer, the key takeaway is that automation is not just about speed; it is about consistency. A manual welder might produce a good result on one roll and a poor result on the next, but an automatic machine produces the same result every time. This consistency is what allows the hardfacing process to be qualified and certified, which is essential for a reliable repair or manufacturing operation. The 76% hardness increase and the 90% wear reduction are impressive, but the real value is in the repeatability of the process.