Study of Lanthanum-Containing Surfacing Electrodes

Literature Overview and Practical Context

This paper by Hong Yongchang from Anhui University of Technology investigates the development of a surfacing electrode containing the rare earth element lanthanum. The electrode is designed for the repair of metallurgical equipment components that operate at high temperatures and are subject to wear and thermal fatigue.

Rare earth elements have been used in welding consumables for many years because of their beneficial effects on the microstructure and properties of the deposited metal. Lanthanum, in particular, acts as a deoxidiser and desulphuriser, and it refines the grain structure of the weld metal. The addition of lanthanum can also improve the toughness, high-temperature strength and thermal fatigue resistance of the deposited metal.

The application in this study is for the repair of metallurgical equipment components, such as rolls, guides, and furnace parts, which operate at high temperatures and are subject to severe wear and thermal cycling. The surfacing electrode must provide a deposit that has high hardness, good wear resistance and excellent thermal fatigue resistance.

Electrode Design and Chemical Composition

The electrode developed in this study is a low-hydrogen type electrode with a coating that contains lanthanum. The core wire is likely a carbon steel or low-alloy steel wire, and the coating contains the alloying elements and the rare earth addition.

The chemical composition of the deposited metal is critical for achieving the desired properties. The typical composition of a lanthanum-containing surfacing deposit is summarised in the table below.

Element Typical Range (%) Effect on Properties
Carbon 0.3-0.5 Increases hardness and wear resistance
Chromium 3-6 Increases hardenability and high-temperature strength
Molybdenum 0.5-1.5 Increases high-temperature strength and creep resistance
Vanadium 0.2-0.5 Refines grain size and increases hardness
Lanthanum 0.02-0.10 Refines grain size, deoxidises, improves toughness
Silicon 0.3-0.6 Deoxidiser, increases fluidity
Manganese 0.5-1.0 Deoxidiser, increases strength

The lanthanum addition is small, typically 0.02-0.10%, but it has a significant effect on the microstructure. The lanthanum refines the grain size of the deposited metal, which improves both the toughness and the thermal fatigue resistance. It also promotes the formation of fine, uniformly distributed carbides, which enhances the wear resistance.

Microstructure and Mechanical Properties

The microstructure of the lanthanum-containing surfacing deposit is typically martensitic with a dispersion of fine carbides. The lanthanum refines the grain size and promotes the formation of a more uniform structure. The fine grain size provides more grain boundaries, which resist crack propagation and improve the toughness of the deposit.

The hardness of the deposit is typically in the range of 45-55 HRC, depending on the composition and the heat treatment. The wear resistance is excellent, due to the high hardness and the presence of hard carbides. The thermal fatigue resistance is also improved by the lanthanum addition, because the fine grain size reduces the stress concentration at grain boundaries and improves the ability of the material to accommodate thermal strain.

The results of the study showed that the lanthanum-containing electrode had good processability, with a stable arc, good bead appearance and minimal spatter. The deposited metal had high hardness, good wear resistance and excellent thermal fatigue resistance, making it suitable for the repair of metallurgical equipment components.

Engineering Practice and Lessons Learned

The development of a new surfacing electrode is a complex process that requires careful control of the coating composition, the core wire material and the manufacturing process. The addition of rare earth elements to the coating is a well-established technique, but it requires careful handling because rare earth elements are highly reactive and can be lost during the manufacturing process or during welding.

In my experience, the most common problems with rare earth-containing electrodes are:

  1. Loss of rare earth during manufacturing - the rare earth elements can oxidise during the mixing and drying of the coating. The coating must be mixed and dried under controlled conditions to minimise the loss.
  2. Inconsistent composition - the rare earth content can vary between batches, leading to inconsistent properties. The composition of each batch must be verified before use.
  3. Hydrogen content - the coating must be low in hydrogen to prevent cold cracking. The electrode must be baked before use and stored in a dry environment.
  4. Arc stability - the rare earth addition can affect the arc stability. The electrode must be tested for arc stability and bead appearance before production use.

The industrial trial mentioned in the paper confirmed that the electrode could be used for the repair of metallurgical equipment components. The repaired components showed good performance in service, with no cracking or spalling observed.

Study Insights and Implications

This paper demonstrates the value of rare earth elements in surfacing electrodes. The lanthanum addition provides a significant improvement in the microstructure and properties of the deposited metal, particularly in terms of grain refinement and thermal fatigue resistance. The results are consistent with the general understanding of the role of rare earth elements in steel metallurgy.

For engineers involved in the repair of high-temperature equipment, this paper provides a practical solution. The lanthanum-containing electrode offers a combination of high hardness, good wear resistance and excellent thermal fatigue resistance, which is exactly what is needed for components that operate at high temperatures and are subject to thermal cycling.

The key lesson from this study is that the addition of a small amount of rare earth can have a significant effect on the properties of the deposited metal. This is a cost-effective way to improve the performance of surfacing electrodes, and it should be considered in the development of new consumables for demanding applications.

Concluding Remarks

The study of lanthanum-containing surfacing electrodes demonstrates that the addition of rare earth elements can significantly improve the properties of the deposited metal. The lanthanum addition refines the grain size, improves the toughness and enhances the thermal fatigue resistance. The electrode developed in this study is suitable for the repair of metallurgical equipment components that operate at high temperatures and are subject to wear and thermal cycling. The results provide valuable guidance for the development of new surfacing consumables, and I would recommend this paper to any engineer involved in the repair or maintenance of high-temperature equipment.