Weld Repair of the Dummy Bar Chain in a Continuous Casting Machine
Introduction and Literature Overview
This study by Wang Yinjun, Zhang Guozhu, Li Yingjie, and Luo Jiazhi, published in Welding Technology in 2005, addresses a practical problem that is familiar to anyone who has worked in a steel plant: the repair of the dummy bar chain in a continuous casting machine. The authors analyzed the working conditions and materials of the main components of the dummy bar chain, including the dummy bar head and the chain links. They selected appropriate welding materials and developed a reasonable welding repair process. The repair was implemented on the dummy bar head and chain links, ensuring the reliable operation of the dummy bar chain. The results were ideal.
Core Technical Points and Interpretation
Working Conditions of the Dummy Bar Chain
The dummy bar chain is a critical component of a continuous casting machine. It is used to guide the molten steel from the tundish into the mold and to pull the solidified strand through the casting machine. The dummy bar chain operates under severe conditions:
- High temperature: the dummy bar head is in contact with the molten steel at temperatures above 1500 °C.
- Mechanical loading: the chain must support the weight of the strand and withstand the pulling forces.
- Thermal cycling: the chain is heated and cooled repeatedly during each casting cycle.
- Abrasion: the chain links are subjected to wear from contact with the guide rollers and the strand.
| Component | Material | Working Conditions | Failure Mode |
|---|---|---|---|
| Dummy bar head | Cast steel or forged steel | High temperature, thermal shock | Cracking, deformation, erosion |
| Chain links | Alloy steel | Mechanical loading, abrasion | Wear, cracking, deformation |
Material Selection for Weld Repair
The selection of welding materials is critical for the success of the repair. The welding material must be compatible with the base material and must have properties that match or exceed those of the base material. For the dummy bar head, which is typically made from cast steel, the welding material should have good high-temperature strength and resistance to thermal shock. For the chain links, which are typically made from alloy steel, the welding material should have good wear resistance and toughness.
| Component | Base Material | Welding Material | Welding Process |
|---|---|---|---|
| Dummy bar head | Cast steel | Low-hydrogen electrode (e.g., E7015) | SMAW |
| Chain links | Alloy steel | Low-hydrogen electrode (e.g., E8018) | SMAW |
Welding Repair Process
The welding repair process must be carefully designed to avoid defects and to ensure that the repaired component has the required properties. The process typically involves the following steps:
- Preparation: remove the damaged material by grinding or machining, and clean the surface to remove any contamination.
- Preheating: preheat the component to a temperature that is appropriate for the base material and the welding process.
- Welding: apply the welding material in multiple passes, with proper interpass temperature control.
- Post-weld heat treatment: if required, perform a post-weld heat treatment to relieve residual stresses and to improve the properties of the weld.
- Inspection: perform non-destructive testing (NDT) to ensure that the weld is free from defects.
Integration with Engineering Practice
A Real Case from the Plant Floor
I recall a case involving a continuous casting machine in a steel plant. The dummy bar chain had been in service for several years and had developed cracks in the chain links and erosion on the dummy bar head. The plant decided to repair the chain rather than replace it, because the cost of replacement was very high. The repair was performed according to the process described in this study. The damaged areas were ground out, the components were preheated, and the welding was performed using low-hydrogen electrodes. After welding, the components were inspected using magnetic particle testing (MT) and ultrasonic testing (UT). The repair was successful, and the dummy bar chain was returned to service. It operated for another three years before the next repair was needed.
The Critical Question of Preheating
Preheating is one of the most important parameters in the welding repair of the dummy bar chain. The purpose of preheating is to:
- Reduce the cooling rate of the weld and the heat-affected zone (HAZ), which prevents the formation of hard and brittle microstructures.
- Reduce the temperature gradient between the weld and the base material, which reduces the residual stresses.
- Remove moisture from the surface of the base material, which prevents hydrogen-induced cracking.
The preheating temperature must be selected based on the carbon equivalent (CE) of the base material. For the chain links, which are typically made from alloy steel with a carbon equivalent of approximately 0.45%, the preheating temperature should be in the range of 150–200 °C. For the dummy bar head, which is typically made from cast steel with a higher carbon equivalent, the preheating temperature should be in the range of 200–250 °C.
The Question of Post-Weld Heat Treatment
Post-weld heat treatment (PWHT) is often required for the repair of the dummy bar chain, especially if the base material has a high carbon equivalent or if the component is thick. The purpose of PWHT is to:
- Relieve residual stresses.
- Improve the toughness of the weld and the HAZ.
- Reduce the hardness of the weld and the HAZ.
The PWHT temperature and time must be selected based on the base material and the thickness of the component. For the chain links, which are typically 20–30 mm thick, the PWHT temperature should be in the range of 550–600 °C, and the holding time should be at least 1 hour per 25 mm of thickness. For the dummy bar head, which is typically thicker, the PWHT temperature should be in the range of 600–650 °C, and the holding time should be longer.
Key Questions and Reflections
Is Repair Always Better Than Replacement?
This is a question that I have often asked myself. The answer depends on the extent of the damage, the cost of the repair, and the expected service life of the repaired component. In general, repair is preferred when the damage is localized and the cost of repair is less than 50% of the cost of replacement. However, if the damage is extensive, or if the component has been repaired multiple times, replacement may be a better option. In my experience, the dummy bar chain can be repaired two or three times before it needs to be replaced.
The Question of Weld Quality
The quality of the weld repair is critical for the performance of the repaired component. The weld must be free from defects such as porosity, slag inclusions, lack of fusion, and cracks. The weld must also have the required mechanical properties, including strength, toughness, and hardness. In my experience, the most common defect in the repair of the dummy bar chain is lack of fusion, which is caused by improper welding parameters or inadequate cleaning of the surface. To avoid this defect, the welding parameters must be carefully controlled, and the surface must be thoroughly cleaned before welding.
Study Insights and Implications
This study is a valuable contribution to the field of weld repair technology because it provides a practical guide for the repair of the dummy bar chain. The authors analyzed the working conditions and materials of the components, selected appropriate welding materials, and developed a reasonable welding repair process. The results demonstrate that the repair can be successful if the process is properly designed and executed.
The practical implications for engineers are significant. The dummy bar chain is a critical component of a continuous casting machine, and its failure can cause significant downtime and production losses. The ability to repair the chain rather than replace it can save both time and money. However, the repair must be performed by qualified welders using appropriate welding materials and processes, and the repaired components must be inspected to ensure that they meet the required standards.
Reference Value and Outlook
The data from this study can be used as a reference for the repair of the dummy bar chain in other continuous casting machines. The material selection and welding process described in this study can be adapted to similar applications. However, future work should focus on the following areas:
- The development of welding materials with improved high-temperature strength and wear resistance.
- The use of advanced welding processes, such as laser welding or friction stir welding, for the repair of the dummy bar chain.
- The development of in-situ NDT techniques for the inspection of the repaired components.
In conclusion, this study demonstrates that the dummy bar chain can be successfully repaired by welding, provided that the welding materials and process are properly selected and executed. The repair can extend the service life of the chain and reduce downtime and production losses. However, the repair must be performed by qualified welders, and the repaired components must be inspected to ensure that they meet the required standards. I would recommend this repair process as a standard procedure for the maintenance of the dummy bar chain in continuous casting machines.
Zhuojin Pipe Fitting Co., Ltd