Microstructure and Erosion Resistance of Martensitic Stainless Steel Hardfacing Layers

Literature Overview and Application Context

The paper by Gu Ruichao, Bao Yefeng and Yang Ke, published in Electric Welding Machine (2012, Vol. 42, No. 2, pp. 16-19), investigates the microstructure and erosion resistance of martensitic stainless steel hardfacing layers. The study used 2Cr13 and a microalloyed 1Cr13 (modified with V, Ti, Nb and N) for submerged arc hardfacing. The effects of microalloying elements and heat treatment on the microstructure and erosion resistance of the hardfacing layers were analyzed. The results show that the microalloying elements V, Ti, Nb and N form fine, dispersed stable compounds with C and N during the initial stages of austenite nucleation, which refine the grains of the hardfacing layer. After the austenite grains are stabilized, these compounds provide precipitation strengthening. After tempering, some carbides precipitate between the martensite laths, providing secondary strengthening while reducing the carbon content in the martensite, which improves the toughness of the matrix. The better combination of strength and toughness ultimately improves the erosion resistance of the material.

This is a highly relevant topic for the hydroelectric, pump and valve industries, where components are subjected to erosion by water, slurry or other fluids containing solid particles. Martensitic stainless steels such as 2Cr13 and 1Cr13 are widely used for these applications due to their good combination of strength, toughness and corrosion resistance. However, their erosion resistance is often limited by their hardness and the presence of brittle phases. The addition of microalloying elements such as V, Ti, Nb and N can significantly improve the microstructure and properties of these steels.

Microalloying Effects and Microstructural Evolution

The microalloying elements V, Ti, Nb and N play a critical role in the microstructure of the hardfacing layer. These elements are strong carbide and nitride formers, and they form fine, dispersed precipitates during the solidification and subsequent heat treatment. The authors found that these precipitates form during the initial stages of austenite nucleation, which refines the grain size of the hardfacing layer. This is a classic grain refinement mechanism, where the fine precipitates act as nucleation sites for the austenite grains, resulting in a finer, more uniform microstructure.

After the austenite grains are stabilized, the precipitates provide precipitation strengthening. This is a secondary strengthening mechanism, where the fine precipitates impede the movement of dislocations, increasing the strength and hardness of the material. The combination of grain refinement and precipitation strengthening results in a material with improved strength and toughness.

The tempering treatment is also critical. During tempering, some carbides precipitate between the martensite laths, providing secondary strengthening. This is a well-known phenomenon in martensitic steels, where the precipitation of fine carbides during tempering increases the strength and hardness. However, the precipitation of carbides also reduces the carbon content in the martensite, which improves the toughness of the matrix. This is a key point: the reduction in carbon content in the martensite reduces the lattice distortion and the tendency for brittle fracture, while the fine carbides provide strengthening. The result is a better combination of strength and toughness.

Erosion Resistance and Its Correlation