Vertical Mill Roller and Table Surface Wear-Resistant Hardfacing Technology
Overview of the Literature
This 2005 paper from Kunshan Huifeng Wear-Resistant Industry Co., Ltd. addresses the wear problems of vertical mill rollers and grinding tables in cement grinding systems. The vertical mill, or roller mill, has gained widespread acceptance because of its significant energy savings compared to ball mills. However, the authors are candid about the downside: the wear of the grinding rollers and the table surface is a constant source of trouble for plant owners. The irregular wear pattern, combined with the increasing gap between the roller and the table as wear progresses, leads to declining equipment efficiency, rising energy consumption, and ultimately forced shutdown for maintenance.
Core Technical Points
Wear Characteristics of Vertical Mill Components
The paper identifies the unique wear characteristics of vertical mill grinding elements. Unlike the roller press, which has a relatively uniform wear pattern, the vertical mill roller and table experience irregular wear due to the complex motion of the material bed. The roller rotates on its own axis while the table rotates beneath it, creating a grinding zone where the material is crushed and ground. The wear pattern depends on the material being ground, the moisture content, and the operating parameters of the mill.
Hardfacing Materials and Techniques
The paper discusses the available hardfacing technologies for vertical mill components. The most common approach is to use flux-cored arc welding (FCAW) with a wear-resistant alloy wire. The alloy system is typically a high-chromium carbide type, with chromium content in the range of 15-30% and carbon content in the range of 3-6%. The microstructure consists of primary chromium carbides in a martensitic or austenitic matrix, providing excellent abrasive wear resistance.
| Hardfacing Alloy Type | Typical Hardness (HRC) | Primary Wear Mechanism | Application |
|---|---|---|---|
| High-chromium carbide | 55-65 | Abrasive wear | Raw material grinding |
| Martensitic steel | 45-55 | Impact + abrasive | Coal grinding |
| Austenitic manganese | 40-50 | Impact + work hardening | Clinker grinding |
| Composite carbide | 60-70 | Severe abrasive | Hard rock grinding |
The Gap Problem and Its Consequences
The paper highlights a critical issue: as the roller and table wear, the gap between them increases, reducing the grinding efficiency. This is a self-reinforcing problem. As the gap increases, the material bed becomes thicker, and the grinding action becomes less effective, leading to a coarser product. To maintain the same product fineness, the mill must be operated at a higher table speed or with a higher material feed rate, both of which increase energy consumption. Eventually, the wear becomes so severe that the mill must be stopped for re-hardfacing.
Repair and Re-Hardfacing Strategy
The paper outlines a practical repair strategy. When the wear reaches a critical level, the roller and table are removed from service and re-hardfaced. The process involves:
- Machining away the worn surface to sound metal.
- Inspecting the substrate for cracks and defects.
- Applying a new hardfacing layer using FCAW or SAW.
- Machining the hardfaced surface back to the original profile.
- Balancing the roller and table assembly.
Engineering Practice Insights
The Importance of Wear Monitoring
From my experience in steel plant grinding operations, I can confirm that the key to managing vertical mill wear is continuous monitoring. The paper does not provide specific monitoring intervals, but in practice, I recommend measuring the roller and table profile every 500-1000 operating hours. This allows the maintenance team to predict when the wear will reach the critical level and plan the re-hardfacing operation during a scheduled shutdown.
The Cost of Ignoring Wear
The paper correctly identifies the consequences of ignoring wear: declining efficiency, rising energy consumption, and unplanned downtime. In my experience, a vertical mill that is operated with excessive wear can consume 10-20% more energy than a well-maintained mill. Over a year of operation, this can translate into significant additional cost. More importantly, an unplanned shutdown due to catastrophic wear can cost more in lost production than the entire re-hardfacing operation.
The Re-Hardfacing Decision: Repair vs. Replacement
The paper does not provide a definitive answer on whether to repair or replace, but the economics are clear. A new roller or table segment costs the full replacement price, while re-hardfacing typically costs 30-50% of that. However, the re-hardfaced component must be handled with care. The old hardfacing layer must be completely removed, and the substrate must be inspected for cracks. If the substrate is cracked, the component may not be repairable and must be replaced.
Welding Defects and Their Impact
The paper does not discuss welding defects in detail, but I will add from experience. The most common defects in vertical mill hardfacing are:
- Lack of fusion: caused by insufficient welding current or travel speed, leading to spalling in service.
- Porosity: caused by moisture in the flux or wire, creating stress raisers that initiate fatigue cracks.
- Cracking: if the hardfacing layer cracks, it is not always catastrophic, but cracks that propagate into the substrate are.
- Distortion: caused by excessive heat input, leading to misalignment of the roller and table.
Key Questions and Reflections
Why Does Wear Occur Irregularly?
The paper identifies irregular wear as a major problem, but does not fully explain the mechanism. In my experience, irregular wear is caused by several factors:
- Non-uniform material feed: if the material is fed unevenly, one side of the table wears faster than the other.
- Vibration: excessive vibration can cause the roller to bounce, creating a non-uniform wear pattern.
- Material segregation: if the material segregates by size, the coarser particles cause more wear on one side.
- Roller misalignment: if the roller is not properly aligned with the table, the wear pattern becomes skewed.
What Is the Role of the Hardfacing Alloy?
The choice of hardfacing alloy is critical. The paper mentions several alloy types, but the key is to match the alloy to the specific service conditions. For raw material grinding, where the material is abrasive but not particularly hard, a high-chromium carbide alloy is suitable. For clinker grinding, where the material is harder and more abrasive, a composite carbide alloy may be needed. For coal grinding, where the material is softer but has a higher impact component, a martensitic steel alloy is often the best choice.
Study Insights and Implications
The Practical Value of This Paper
This paper is a practical guide for plant engineers dealing with vertical mill wear. It provides a clear overview of the problem, the available solutions, and the maintenance strategies. The emphasis on the gap problem and its consequences is particularly valuable, as it highlights the self-reinforcing nature of wear. The paper is a good starting point for anyone who needs to understand the basics of vertical mill hardfacing.
What the Paper Does Not Say
The paper is relatively brief and does not provide detailed metallurgical data or process parameters. It also does not discuss the specific hardfacing alloys in detail. For a more complete picture, the reader should consult more detailed references on hardfacing technology, such as the AWS Welding Handbook or the ASM Handbook.
Reference Value and Outlook
Standards and Specifications
The paper does not reference specific standards, but in practice, vertical mill hardfacing is governed by the same principles as any other surfacing operation. The relevant standards include ASME Section IX for welding procedure qualification, ISO 15614 for procedure qualification, and various material standards for the hardfacing alloys.
Future Directions
The paper is from 2005, and the field has advanced considerably. Modern vertical mills often use composite rollers with a wear-resistant insert or a specially designed hardfacing alloy. Laser cladding and plasma transferred arc (PTA) welding are now used for high-precision hardfacing, offering better control of dilution and a more uniform deposit. However, the fundamental principles remain the same: match the alloy to the service conditions, control the welding parameters, and manage the wear proactively.
Summary
This paper provides a practical introduction to the wear problems of vertical mill rollers and grinding tables. It correctly identifies the irregular wear pattern and the gap problem as the key issues, and it emphasizes the importance of a systematic maintenance and repair strategy. The key takeaways for the plant engineer are: choose the hardfacing alloy based on the specific grinding conditions, monitor wear regularly, plan re-hardfacing during scheduled shutdowns, and ensure that the welding procedure is qualified before production. In my experience, plants that follow these principles achieve roller and table service lives measured in years, while those that do not are constantly fighting fires. The paper is a good starting point, but the reader should supplement it with more detailed metallurgical and process data before making a final decision on alloy selection and welding parameters.
Zhuojin Pipe Fitting Co., Ltd