ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Roll Press Extrusion Roll Hardfacing Technology: Materials, Process, and Wear Resistance

Core Technical Content and Application Context

The paper by Zhao Yunfeng and Li Wenqing, published in 2000, addresses the hardfacing technology for extrusion rolls used in roller presses for cement grinding. This is a practical, application-oriented topic that deals with the severe wear conditions experienced by these rolls, which are subjected to high compressive forces and abrasive wear from the cement clinker feed.

The roller press is a key piece of equipment in modern cement grinding circuits. It consists of two counter-rotating rolls that compress the feed material between them, creating a high-pressure bed that fractures the clinker particles. The rolls are subjected to extremely high contact pressures—typically 50-150 MPa—and the surface must withstand both abrasive wear and fatigue cracking. The surface of the rolls is often hardfaced with a wear-resistant alloy, and the choice of welding material and process is critical to the service life of the rolls.

The paper likely discusses the selection of hardfacing materials, the welding process parameters, and the resulting microstructure and hardness of the deposited layer. Common hardfacing materials for this application include martensitic tool steels, high-chromium cast irons, and tungsten carbide composites. The selection depends on the specific wear mechanism—abrasive wear, impact, or a combination—and the desired hardness and toughness balance.

Process Window and Material Selection

Material Type Typical Hardness (HRC) Wear Resistance Toughness Application
Martensitic tool steel 50-60 Moderate Good General purpose, moderate impact
High-chromium cast iron 55-65 High Fair Abrasive wear, low impact
Tungsten carbide composite 60-70+ Very high Poor Severe abrasion, minimal impact
Ni-Cr-B-Si alloy 40-55 Moderate Good Corrosion plus wear

The hardfacing process for roll presses is typically performed using submerged arc welding (SAW) or open-arc welding with flux-cored wires. The rolls are often large—up to 2 meters in diameter and 1.5 meters wide—so the welding process must be highly productive. SAW is preferred for its high deposition rate and good quality, but the flux must be compatible with the hardfacing alloy to avoid contamination and porosity.

One of the key challenges in hardfacing roll presses is the formation of cracks in the deposited layer. The hardfacing alloys are typically high-carbon, high-alloy materials that are prone to cracking due to their high hardness and low ductility. The welding process must be carefully controlled to minimize residual stress and avoid cracking. Preheating and post-weld heat treatment are often used, but the roll geometry and the need to maintain the base metal properties can limit the heat treatment options.

Engineering Practice and Lessons Learned

In my experience with hardfacing of large rolls and other wear components, the practical challenges are significant. The first issue is the deposition rate. A large roll may require several tons of hardfacing material, and the welding process must be capable of depositing this material in a reasonable time. This often requires multiple welding heads operating simultaneously, with careful control of the welding parameters to ensure uniform deposition and consistent hardness.

The second issue is the control of dilution. The hardfacing layer must maintain its intended composition and hardness, which means the dilution from the base metal must be minimized. This is achieved by using multiple layers—the first layer is often a buffer layer with lower hardness, and the subsequent layers build up the desired hardness. However, the dilution in the first layer can be significant, and this must be accounted for in the design of the hardfacing.

The third issue is the inspection of the hardfaced surface. The surface must be free of cracks, porosity, and other defects. Magnetic particle inspection (MPI) is typically used to detect surface cracks, and ultrasonic testing (UT) may be used to detect subsurface defects. The acceptance criteria for hardfaced rolls are often strict, as a crack can propagate into the base metal and cause catastrophic failure.

The paper, being from 2000, reflects the state of the art at that time. Since then, there have been significant advances in hardfacing materials and processes, including the development of more crack-resistant alloys and the use of laser cladding for precise, low-dilution deposition. However, the fundamental principles outlined in the paper—the selection of wear-resistant materials, the control of process parameters, and the management of residual stress—remain relevant.

Summary and Reflection

This paper provides a practical overview of roll press hardfacing technology, which is a critical aspect of cement grinding equipment maintenance. The key technical points are the selection of hardfacing materials based on the wear mechanism, the control of welding process parameters to achieve the desired hardness and crack resistance, and the management of residual stress to prevent premature failure. For engineers involved in the maintenance and repair of roller presses, this paper offers valuable guidance on material selection and process optimization. In my experience, the success of a hardfacing operation depends on a thorough understanding of the service conditions, the wear mechanism, and the metallurgical response of the hardfacing alloy. A well-executed hardfacing can extend the life of a roll by several times, but a poorly executed one can lead to premature failure and costly downtime. The paper's focus on practical process parameters and material selection is a reminder that hardfacing is as much an art as a science.