ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Effect of Vanadium on Microstructure and Wear Resistance of High-Chromium Surfacing Alloy

Introduction and Background

This paper, published in Hot Working Technology (热加工工艺) in 2015 by Yang Boxiang and colleagues from Xiangtan University, investigates the effect of vanadium (V) on the microstructure and wear resistance of a high-chromium (17–19% Cr) surfacing alloy deposited by open-arc welding using a flux-cored wire. The alloy contains 3.9–4.2% C, 0.6–4.9% Si, and 0–3.2% V. The base metal is Q235A steel. The paper examines the phase composition, the microstructure of the bottom, middle, and top layers of the deposit, and the wear resistance under wet sand abrasive wear conditions. The study is directly relevant to hardfacing applications in mining, cement, and other industries where abrasive wear is the primary failure mode.

Technical Interpretation of the Core Findings

The paper reports that the addition of vanadium has several significant effects on the microstructure and properties of the high-chromium surfacing alloy. First, vanadium reduces the detrimental effect of dilution from the Q235A base metal. Dilution in open-arc welding can be high (15–30%), and the carbon and alloying elements from the base metal can dilute the deposit, reducing the hardness and wear resistance. Vanadium is a strong carbide former, and it helps to compensate for the dilution by forming stable vanadium carbides that are harder and more wear-resistant than the chromium carbides that would otherwise form.

Second, vanadium suppresses the formation of brittle microstructures. The paper specifically mentions the "honeycomb-like transformed ledeburite" (Ld′) and the "fishbone-like (α-Fe + M7C3 + M3C) eutectic" structures. These are typical of high-chromium white cast iron hardfacing alloys, and they are known to be brittle and prone to cracking. The addition of vanadium changes the solidification path, promoting the formation of primary M7C3 carbides (which are harder and more wear-resistant) and reducing the amount of the brittle eutectic phases. This is a critical finding because it means that vanadium not only improves wear resistance but also improves toughness and crack resistance.

Third, vanadium increases the volume fraction of the primary M7C3 phase. M7C3 is the primary hard phase in high-chromium alloys, and its volume fraction and size distribution directly determine the wear resistance. The paper reports that the addition of vanadium increases the volume fraction of primary M7C3, which is consistent with the improved wear resistance observed in the wet sand abrasive wear test. The wear mechanism was identified as micro-fracture (spalling), which indicates that the hard phases are being removed by brittle fracture rather than by micro-cutting. This suggests that the toughness of the matrix and the bonding between the hard phases and the matrix are critical factors.

Engineering Practice Insights and Lessons

From my own experience with hardfacing in the mining and cement industries, I can confirm that the effect of vanadium described in this paper is real and significant. High-chromium hardfacing alloys are widely used for wear plates, crusher hammers, and chute liners, but they are often limited by their brittleness. Cracking and spalling are common failure modes, especially when the hardfacing is applied to a low-carbon steel base metal with high dilution. The addition of vanadium, as described in this paper, offers a practical solution to this problem by promoting a more favorable microstructure.

One of the key practical considerations is the choice of the welding process. The paper uses open-arc welding with a self-shielded flux-cored wire, which is a common process for hardfacing in the field because it does not require a shielding gas and is portable. However, open-arc welding has high dilution and high heat input, which can be detrimental to the hardfacing alloy. The paper shows that vanadium helps to mitigate the effects of dilution, but the engineer must still carefully control the welding parameters — particularly the current and the travel speed — to minimize dilution and to ensure a consistent deposit composition.

Another practical lesson is the importance of the number of layers. The paper examines the bottom, middle, and top layers of the deposit, and the microstructure varies significantly between them. The bottom layer is most affected by dilution from the base metal, while the top layer is least affected. In practice, this means that the wear resistance of the deposit may not be uniform, and the bottom layer may be the weak point. I have seen cases where hardfaced components failed at the interface between the deposit and the base metal because the bottom layer had insufficient hardness and wear resistance. The engineer should either increase the number of layers to ensure that the top layer has the desired properties, or use a buffer layer of a more ductile alloy to reduce the dilution effect.

Key Questions and Reflections

One question that this paper raises is the optimal vanadium content. The paper tested vanadium contents up to 3.2%, but it does not provide a clear optimum. From my experience, the optimal vanadium content depends on the specific application and the base metal. For applications where impact resistance is important, a lower vanadium content may be preferred to maintain toughness. For applications where pure abrasive wear is the primary concern, a higher vanadium content may be beneficial. I would recommend that the engineer conduct their own trials with different vanadium contents to determine the optimum for their specific application.

Another reflection is the effect of vanadium on the weldability of the hardfacing alloy. Vanadium is a strong carbide former, and it can increase the hardenability of the deposit, which may lead to cracking if the cooling rate is too high. The paper does not address this issue directly, but I have seen cases where high-vanadium hardfacing alloys cracked during deposition, particularly on thick sections or when the ambient temperature was low. Preheating the base metal and controlling the interpass temperature are essential to prevent this problem.

Summary and Implications

This paper provides a valuable contribution to the understanding of vanadium in high-chromium hardfacing alloys. The key findings are: (1) vanadium reduces the detrimental effects of dilution from the base metal, (2) vanadium suppresses the formation of brittle microstructures, and (3) vanadium increases the volume fraction of primary M7C3 carbides, leading to improved wear resistance. For the practicing engineer, the practical implications are clear: vanadium is a useful alloying addition for high-chromium hardfacing alloys, particularly when the base metal is a low-carbon steel and dilution is a concern. However, the optimal vanadium content must be determined for each specific application, and the welding parameters must be carefully controlled to prevent cracking. I would recommend this paper to any engineer involved in hardfacing for abrasive wear applications, and I would encourage them to consider vanadium as a key alloying element in their hardfacing alloy design.