ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Strip Submerged Arc Cladding of Nuclear Reactor Pressurizer Heads: Process Development and Qualification

Literature Overview and Practical Significance

This paper by Liao Guoping from Dongfang Boiler Group describes the development and qualification of a strip submerged arc cladding process for the hemispherical heads of nuclear reactor pressurizers. The work involved the design and manufacture of special assembly tooling and auxiliary curved backing plates, the use of a 100-tonne welding positioner, and the use of ESAB welding equipment to clad the entire inner surface of the heads with an ultra-low carbon austenitic stainless steel corrosion-resistant layer.

This is a high-end application that demands the utmost attention to detail. The paper discusses the influence of current, voltage, welding speed, bead overlap, and the levelness of the workpiece on the cladding quality. The author determined the appropriate welding parameters and successfully completed the cladding of four heads for two pressurizers. This paper is a valuable reference for anyone involved in the cladding of large, curved surfaces, particularly in the nuclear industry.

Interpretation of Technical Points

Equipment and Tooling Design

The paper highlights the importance of equipment and tooling design. The hemispherical head is a large, curved component that is difficult to position and rotate. The author designed a special assembly fixture and auxiliary curved backing plates to support the head and to ensure that the cladding is applied uniformly. The use of a 100-tonne positioner allows the head to be rotated and tilted to the optimal position for each weld pass. This is a critical aspect of the process, as the position of the workpiece affects the molten pool behaviour and the bead shape.

Process Parameters and Their Effects

The paper discusses the influence of current, voltage, welding speed, and bead overlap on the cladding quality. In strip submerged arc cladding, the current is the primary factor controlling the deposition rate and the penetration. The voltage controls the arc length and the width of the bead. The welding speed affects the heat input and the bead geometry. The bead overlap is critical for ensuring a smooth, uniform surface without lack of fusion or excessive dilution.

The author also discusses the importance of the workpiece levelness. If the head is not level, the molten pool will flow to one side, causing the bead to be asymmetric and potentially leading to lack of fusion or slag entrapment. This is a practical issue that is often overlooked, but it is critical for large, curved surfaces.

Dilution Control and Corrosion Resistance

The paper emphasises the importance of controlling dilution. For a corrosion-resistant overlay on a carbon steel or low-alloy steel substrate, the dilution must be kept low to maintain the required chromium and nickel content in the first layer. The author discusses the use of multiple layers to achieve the required thickness and composition. The first layer has the highest dilution, and the subsequent layers have progressively lower dilution. This is a standard practice in the industry, and the paper provides a good example of how it is implemented in a nuclear application.

Integration with Engineering Practice

In our industry, we apply similar principles when cladding large components such as reactor vessels, heat exchangers, and pipe fittings. The key challenges are managing the geometry of the component, controlling the process parameters, and ensuring the quality of the deposit.

One of the most important lessons from this paper is the importance of trial runs. Before cladding the actual production heads, the author likely performed a series of trial runs on mock-ups or test coupons to determine the optimal parameters. This is a standard practice in our industry, and it is essential for qualifying the procedure and for ensuring that the production parts meet the specifications.

Another lesson is the importance of quality control. The cladding must be inspected using non-destructive testing methods such as ultrasonic testing, magnetic particle testing, or liquid penetrant testing to detect any defects. The chemical composition of the deposit must be verified using spectrometric analysis, and the mechanical properties must be verified using tensile and impact tests.

Key Questions and Reflections

One question that the paper does not fully address is the management of residual stresses. Cladding a large, curved surface inevitably introduces residual stresses, which can cause distortion and, in some cases, cracking. The author mentions post-weld heat treatment, but does not provide details on the specific cycle used. In our practice, we typically use a stress-relief heat treatment after cladding, but the temperature and time must be carefully selected to avoid degrading the properties of the cladding.

Another reflection concerns the use of a 100-tonne positioner. This is a significant piece of equipment, and its use requires careful planning and coordination. The positioner must be capable of handling the weight and size of the head, and it must be able to rotate and tilt the head smoothly and accurately. The paper's description of the equipment and tooling design is a valuable reference for anyone planning a similar operation.

Study Insights and Implications

This paper is a valuable case study of a high-end cladding application. It demonstrates that successful cladding of large, curved surfaces requires a combination of careful equipment design, precise process control, and thorough quality assurance.

From a practical standpoint, the key takeaways are as follows. First, invest in the right equipment and tooling. A 100-tonne positioner is expensive, but it is essential for handling large, heavy components. Second, perform trial runs on mock-ups before cladding the production parts. This allows you to optimise the parameters and to identify any potential issues. Third, control the dilution carefully to ensure that the deposit meets the required chemical composition. Fourth, use multiple layers to achieve the required thickness and to reduce the dilution in the final layer. Fifth, implement a comprehensive quality control program that includes non-destructive testing, chemical analysis, and mechanical testing.

Reference Value and Outlook

This paper is an excellent reference for engineers involved in the cladding of large pressure vessels and other critical components. It provides a detailed description of the equipment, tooling, process parameters, and quality control measures used in a nuclear application. The next step for the industry would be to develop more advanced process control systems that can automatically adjust the welding parameters based on real-time feedback from sensors monitoring the arc, the bead geometry, and the temperature.

In conclusion, this paper demonstrates that strip submerged arc cladding is a viable and reliable process for cladding large, curved surfaces. The key to success is a combination of careful planning, precise process control, and thorough quality assurance. The paper provides a valuable reference for anyone facing a similar challenge.