ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Effect of Magnetic Field Current on the Microstructure and Mechanical Properties of Fe5 Overlay: A Practical Review

Literature Overview and Core Problem

This 2010 paper from the Liaoyang Boiler and Pressure Vessel Inspection Institute and Shenyang University of Technology addresses the use of a transverse DC magnetic field during plasma arc surfacing of Fe5 self-fluxing alloy. The authors introduced a magnetic field to the arc and the molten pool, and they studied the effect of the magnetic field current on the microstructure and mechanical properties of the overlay. They found that the overlay with a magnetic field had higher hardness and better wear resistance than the overlay without a magnetic field. The best performance was achieved at a magnetic field current of 3 A, where the wear resistance was the best and the hardness was the highest. This is a research paper, but it has practical implications. The use of an external magnetic field to control the weld pool is a well-known technique, and the authors have applied it to a specific alloy system.

Technical Points and Metallurgical Interpretation

The Fe5 Self-Fluxing Alloy

Fe5 is a self-fluxing alloy, which is a nickel-based or iron-based alloy with boron and silicon as the fluxing elements. The boron and silicon lower the melting point and provide the self-fluxing property. The alloy is used for hardfacing applications where high hardness and good wear resistance are required. The typical composition of Fe5 is shown in the table below.

Element Content (wt.%) Function
Carbon 0.5% - 1.0% Increases hardness and wear resistance.
Chromium 15% - 20% Increases hardness and corrosion resistance.
Boron 2% - 4% Forms hard borides, increases hardness.
Silicon 2% - 4% Fluxing agent, lowers melting point.
Iron Balance Matrix element.

The Effect of the Magnetic Field

The magnetic field affects the arc and the molten pool in several ways. First, the magnetic field exerts a force on the charged particles in the arc, which causes the arc to rotate or to oscillate. This can improve the arc stability and the distribution of the heat. Second, the magnetic field induces a stirring effect in the molten pool. The stirring action breaks up the dendrites, refines the grain size, and distributes the hard particles more uniformly. Third, the magnetic field can affect the solidification direction, which can change the orientation of the grains. The authors found that the hardness and the wear resistance increased with the magnetic field current up to 3 A, and then decreased. The decrease at higher currents is likely due to excessive stirring, which can cause turbulence and entrapment of gas and slag. The table below summarises the effect of the magnetic field current on the properties.

Magnetic Field Current (A) Hardness (HRC) Wear Resistance Microstructure
0 55 - 58 Baseline Coarse dendrites, non-uniform distribution of hard particles.
1 58 - 60 Improved Finer dendrites, more uniform distribution.
2 60 - 62 Improved Further refinement, more uniform distribution.
3 62 - 64 Best Fine equiaxed grains, uniform distribution of hard particles.
4 60 - 62 Decreased Excessive stirring, some porosity and slag entrapment.

The Practical Concerns

The most important practical concern is the control of the magnetic field. The magnetic field must be uniform and stable, and the current must be precisely controlled. The magnetic field is generated by a coil, and the current is controlled by a power supply. The position of the coil relative to the arc is critical. If the coil is not properly positioned, the magnetic field will not be uniform, and the effect will be inconsistent. The authors used a transverse DC magnetic field, which means the field is perpendicular to the welding direction. This is the most effective configuration for stirring the molten pool.

Integration with Engineering Practice

The Application to Hardfacing

The use of an external magnetic field in hardfacing is not new, but it is not widely used in industry. The reason is that the equipment is additional, and the process is more complex. However, the benefits are significant. The refinement of the microstructure and the improvement of the wear resistance can extend the life of the hardfaced component by a significant margin. For a component that is subject to severe wear, such as a crusher roll or a shovel tooth, the improvement can be the difference between a component that lasts one season and a component that lasts two seasons. The authors have demonstrated the effect on a specific alloy, and the results are clear.

The Process Window

The process window for the magnetic field current is narrow. The authors found that the optimum current is 3 A, and the performance decreases at higher currents. This means that the power supply must be capable of holding the current within a narrow tolerance. In a production environment, this is a challenge. The magnetic field current must be monitored and controlled, and the coil must be shielded from the effects of the welding current. The table below summarises the process window for the magnetic field.

Parameter Range Practical Notes
Magnetic field type Transverse DC The field is perpendicular to the welding direction.
Magnetic field current 2 A - 4 A The optimum is 3 A.
Coil position 10 mm - 20 mm from the arc Must be precisely positioned.
Welding current 150 A - 250 A Must be matched to the strip or wire size.
Welding speed 100 mm/min - 300 mm/min Must be matched to the deposition rate.

Key Questions and Reflections

The paper raises a question that I have often asked myself: why is this technique not used more widely in industry? The answer is that the equipment is additional, and the process is more complex. However, the benefits are significant. The refinement of the microstructure and the improvement of the wear resistance can extend the life of the hardfaced component by a significant margin. My own reflection is that the use of a magnetic field is a promising technique, but it requires a high level of process control. The process window is narrow, and the equipment must be reliable. For a young engineer, the lesson is to understand the interaction between the magnetic field and the welding arc. For a veteran like me, the paper is a reminder that the best results come from a thorough understanding of the physics of the process.

Study Insights and Implications

The most important insight from this paper is that the magnetic field can be used to control the microstructure and the properties of a hardfacing overlay. The authors have demonstrated that the magnetic field current has a significant effect on the hardness and the wear resistance, and that the optimum current is 3 A. The mechanism is the refinement of the grain size and the uniform distribution of the hard particles. This is a valuable finding for the hardfacing industry. For a young engineer, the lesson is to understand the effect of the process parameters on the microstructure and the properties. For a veteran like me, the paper is a confirmation of the importance of process control. The reference value of this paper is that it provides a quantitative relationship between the magnetic field current and the properties of the overlay. It is a valuable reference for any engineer involved in hardfacing or surface engineering.