ZG75CrMo Hot Rolling Work Roll Hardfacing Process: A Practical Review
Literature Overview and Context
This 1999 paper from Xingtai Machinery Roll Co., Ltd. addresses a common problem in rolling mill operation: the drive-side flat head of a hot rolling work roll wears out before the roll body reaches its discard size. The authors developed a hardfacing process for the flat head using a wear-resistant and impact-resistant composite layer, which extended the roll service life. The process was successfully applied to new roll manufacturing, opening a new route for roll repair and manufacturing with significant economic benefits.
Problem Analysis
The Real Issue
In a hot rolling mill, the work roll is driven through the flat head on the drive side. The flat head transmits the torque from the coupling to the roll body. During service, the flat head experiences severe wear and impact loading. The wear is caused by the relative motion between the flat head and the coupling, which is a sliding contact under high load.
The problem is that the flat head wears out before the roll body reaches its discard size. This means the entire roll must be replaced, even though the roll body still has significant life remaining. The economic loss is substantial, especially for large rolls.
Material Selection
The roll material is ZG75CrMo, a cast steel with 0.75% carbon and chromium-molybdenum alloying. This material has good strength and wear resistance, but the flat head surface is not hard enough to resist the severe wear in the coupling contact area.
Hardfacing Process Design
Alloy Selection
The authors selected a wear-resistant and impact-resistant composite layer for the hardfacing. The alloy must have sufficient hardness to resist wear, but also sufficient toughness to withstand the impact loading from the coupling. This is a classic trade-off between hardness and toughness.
Process Parameters
The hardfacing process likely involved:
- Preheating: To prevent cracking, the roll must be preheated before hardfacing.
- Interpass temperature control: To maintain a consistent deposit quality.
- Post-weld heat treatment: To relieve residual stresses and temper the deposit.
- Multiple layers: To achieve the required thickness and hardness.
Results
The hardfaced flat head showed significantly improved wear resistance and impact resistance. The roll service life was extended, and the process was successfully applied to new roll manufacturing. The economic benefits were significant because the roll could be used for a longer period before replacement.
| Parameter | Before Hardfacing | After Hardfacing |
|---|---|---|
| Flat head wear rate | High | Significantly reduced |
| Roll service life | Limited by flat head wear | Extended |
| Impact resistance | Poor | Improved |
| Economic benefit | Baseline | Substantial savings |
Practical Implications for Roll Manufacturing and Repair
This paper demonstrates a practical approach to extending the life of expensive components. The key insight is that the failure mode is localized — the flat head wears out while the roll body is still good. By hardfacing the flat head, the entire roll can be used to its full potential.
This approach is directly applicable to other components in the pipe and fitting industry, such as:
- Rolls for pipe forming mills: The roll surfaces can be hardfaced to extend their life.
- Mandrels for seamless pipe production: The mandrel surface can be hardfaced to resist wear.
- Guide rolls and pinch rolls: These components see high wear and can benefit from hardfacing.
Process Considerations and Lessons Learned
Preheating and Post-Weld Treatment
The most critical aspect of hardfacing a large cast steel roll is the preheat and post-weld treatment. ZG75CrMo is a high-carbon steel, which is prone to cracking if the cooling rate is too fast. I have seen rolls crack during hardfacing because the preheat was insufficient or the post-weld treatment was not performed correctly.
Dilution Control
The first layer of hardfacing will have significant dilution from the base metal, which reduces the alloy content and the hardness. I typically specify a minimum of two layers, and I check the hardness of the top layer to ensure it meets the specification.
Quality Control
The hardfaced surface must be inspected for cracks, porosity, and lack of fusion. I typically require magnetic particle inspection or ultrasonic testing after hardfacing and after the post-weld heat treatment.
Key Questions and Reflections
The paper does not specify the exact hardfacing alloy or the process parameters. In practice, I would want to know the alloy composition, the preheat temperature, the interpass temperature, and the post-weld heat treatment schedule. These parameters are critical for reproducing the results.
Another question is the economic analysis. The paper mentions significant economic benefits, but does not provide a detailed cost comparison. In practice, the decision to hardface a roll versus replacing it depends on the cost of the hardfacing, the cost of the new roll, and the expected life extension.
Study Insights and Implications
This paper is a good example of how a localized wear problem can be solved by targeted hardfacing. The approach is practical and cost-effective, and it can be applied to many other components in the pipe and fitting industry.
The lesson for my engineers is to always analyze the failure mode before deciding on a repair strategy. If the wear is localized, hardfacing is often the best solution. If the wear is uniform, replacement may be more economical. The key is to understand the economics and the technical feasibility of each option.
Zhuojin Pipe Fitting Co., Ltd