Hot Rolling Pinch Roll Surfacing Technology
The Pinch Roll Wear Problem
This paper addresses a practical problem in hot rolling mills: the low service life of pinch rolls. Pinch rolls are used to guide and feed the strip through the mill, and they are subjected to severe wear from the hot strip and from the mechanical loads. The conventional material for pinch rolls is a cast iron or a low-alloy steel, and their service life is often too short, leading to frequent roll changes and high maintenance costs.
The authors selected Cr-Mo series welding materials for surfacing the pinch rolls, and they applied the process in production at Baosteel. The results show that the Cr-Mo surfacing material is an ideal choice for this application, significantly improving the quality and service life of the pinch rolls.
Material Selection and Process Parameters
The choice of Cr-Mo series welding materials is based on the service conditions of the pinch roll. The roll surface must have high hardness and wear resistance at elevated temperatures, and it must also have good toughness to resist impact loads. Cr-Mo alloys provide a good combination of these properties.
| Material Property | Cr-Mo Surfacing Layer | Conventional Roll Material |
|---|---|---|
| Hardness | High (typically 40-55 HRC) | Lower (typically 30-40 HRC) |
| Wear resistance | Excellent | Moderate |
| High-temperature strength | Good | Limited |
| Toughness | Adequate | Variable |
| Service life | Significantly improved | Baseline |
The welding process parameters are critical for achieving the desired properties. The authors would have used submerged arc welding or electroslag welding for the large diameter rolls, with preheating and controlled interpass temperature to prevent cracking.
Production Application and Results
The application at Baosteel was successful. The Cr-Mo surfacing material was used to rebuild the pinch rolls, and the results showed a significant improvement in service life compared with the original rolls. This is a practical demonstration of the value of hardfacing in a production environment.
The key to success is the proper selection of the welding material and the careful control of the welding process. The Cr-Mo series provides the right combination of hardness, wear resistance and toughness for the pinch roll service.
Engineering Practice Considerations
In my experience, roll refurbishment by hardfacing is a well-established practice, but the choice of the surfacing material is critical. The material must match the service conditions, and the welding process must be controlled to produce a sound, crack-free layer.
One of the challenges with large rolls is the control of distortion. A roll is a large, relatively thin-walled cylinder, and the heat input from the surfacing can cause it to bow or become out-of-round. The welding sequence must be designed to minimize this, and the roll must be checked for straightness and roundness after surfacing.
Another challenge is the transition zone between the base metal and the surfacing layer. This zone must be free from cracks and other defects, because it is a potential site for failure in service.
Summary and Practical Takeaways
This paper demonstrates the practical value of Cr-Mo series welding materials for surfacing hot rolling pinch rolls. The production application at Baosteel confirms that this material is an ideal choice, significantly improving the service life of the rolls. The key lessons are to select the right material for the service conditions, control the welding process to produce a sound layer, and manage the distortion of the roll during surfacing. This is a good example of how hardfacing can extend the life of expensive components and reduce maintenance costs in a production environment. I would recommend this approach for any application where rolls or similar components are subject to severe wear.
Zhuojin Pipe Fitting Co., Ltd