Surfacing Technology for Column Middle Cylinders in Mining Equipment: A Practical Study on 27SiMn Tube

Background and Structure of the Column Middle Cylinder

The paper by Chen Zaiming from Huaibei Mining Group discusses the application of surfacing technology to the middle cylinder of hydraulic support columns. In underground coal mines, these columns are subject to severe wear, corrosion and impact. The middle cylinder is typically made from 27SiMn seamless steel tube, which is a medium carbon, low alloy steel with good hardenability but poor weldability. The column is a critical component; if it fails, the roof support collapses, and that is a life-threatening situation.

The structure of the middle cylinder is such that the outer surface needs a hard, wear-resistant layer, while the core must retain toughness. Surfacing is the natural choice, but the challenge is that 27SiMn is prone to cold cracking due to its carbon equivalent. The author proposes a specific surfacing method and then discusses the welding materials, process parameters and post-weld heat treatment.

Surfacing Method and Welding Material Selection

The paper suggests using a submerged arc surfacing process, likely with a flux-cored wire or a solid wire with an appropriate flux. The key is to select a filler material that produces a deposit with the required hardness and wear resistance, while maintaining a low enough dilution to avoid cracking. For 27SiMn, the carbon equivalent is around 0.55, which is high. The author recommends a low-hydrogen process and controlled preheat.

Parameter Recommended Value Reason
Preheat temperature 200–250 °C Reduces cooling rate, prevents martensite formation in HAZ
Interpass temperature 250–300 °C Maintains uniform heat input, avoids cold cracking
Welding current 300–400 A (for SAW) Ensures good fusion but not excessive dilution
Arc voltage 28–32 V Balances bead shape and penetration
Post-weld heat treatment 550–600 °C, 2 hours, furnace cool Relieves residual stress, tempers martensite

The filler material should be a low-alloy steel wire with a hardness matching the base material after PWHT. In practice, I have seen shops use a 2.5% Ni or a Cr-Mo type wire to achieve a hardness of 300–350 HB. The dilution must be kept below 20% to maintain the deposit chemistry.

Welding Process and Post-Weld Heat Treatment

The author correctly identifies that the welding process must be controlled to minimise heat input while ensuring adequate fusion. For a tube of this diameter, a single or double layer is usually sufficient. The post-weld heat treatment is critical. If you skip it, you will have a hard, brittle HAZ that will crack under load. The PWHT must be done in a furnace with uniform temperature control. I have seen cases where a local PWHT was attempted with induction heating, and the temperature gradient caused distortion.

Practical Experience and Lessons

In my career, I have dealt with many 27SiMn components, mostly for mining equipment and some for heavy machinery. The most common failure mode is cracking at the toe of the surfacing weld, often starting during the cooling phase. The root cause is almost always insufficient preheat or a delay in starting the PWHT. The paper's recommendation of 200–250 °C preheat is sound, but in practice, you must also consider the ambient temperature. In winter, if the shop is cold, the preheat must be increased by 50 °C.

Another lesson is that the surfacing layer must be applied in a balanced manner to avoid distortion. For a cylinder, you should weld in a sequence that alternates around the circumference. If you weld one side continuously, the cylinder will bow, and then you will have to machine it, which removes the hard layer.

The author's outlook on the application prospects is positive, and I agree. With the increasing depth of coal mines, the demand for reliable hydraulic supports is growing. Surfacing is a cost-effective way to extend the life of these components. However, the process must be treated with respect. 27SiMn is not a forgiving material. If you get the preheat or the PWHT wrong, you will have a component that fails in service, and in a mine, that is a catastrophic event.

In summary, this paper is a practical guide for anyone surfacing 27SiMn tubes. The key points are: select a low-hydrogen process, control preheat and interpass temperatures, and always perform the PWHT. The result is a component that can withstand the harsh underground environment, and that is what the industry needs.