Roll Cladding Technology for a 360mm x 760mm Reversing Hot Mill
1. Literature Overview and Technical Context
The paper by Gan Meijun, published in Shanghai Metals (2001, Vol. 23, Issue 1, pp. 39–41), describes the cladding technology for the wear-resistant layer of rolls in a 360mm x 760mm reversing hot mill. The paper covers the selection of cladding materials and fluxes, the determination of welding parameters, and the inspection of cladding quality. The key result is that the cladding hardness reached HRC47, which increased the roll service life by a factor of more than one.
Roll cladding is a critical technology in the steel industry. Rolls in a hot mill are subjected to severe thermal cycling, mechanical stress, and abrasive wear. The surface of the roll must have high hardness and wear resistance, while the core must have sufficient toughness to resist cracking. Cladding provides a way to achieve this combination by applying a hard, wear-resistant layer to a tough, ductile core. The paper focuses on a specific application: the rolls of a reversing hot mill, which are used for rolling steel slabs into plates or strips.
2. Technical Analysis of the Cladding Process
2.1 Selection of Cladding Materials and Flux
The paper emphasizes the importance of selecting the right cladding material and flux. For roll cladding, the typical materials are:
- High-chromium alloys: Provide excellent wear resistance through the formation of hard chromium carbides.
- Tool steels: Provide good hardness and toughness, suitable for hot work applications.
- Nickel-based alloys: Provide good corrosion and wear resistance, but are more expensive.
The flux selection is equally important. For submerged arc cladding, the flux must provide:
- Good arc stability.
- Proper slag formation to protect the weld pool.
- Alloying elements to achieve the desired deposit chemistry.
- Low hydrogen content to prevent cracking.
The paper likely used a submerged arc welding (SAW) process, which is the most common method for roll cladding because it provides high deposition rates and good penetration.
2.2 Welding Parameters
The welding parameters for roll cladding are critical to achieving the desired deposit quality:
| Parameter | Typical Range | Effect |
|---|---|---|
| Welding current | 300–500 A | Determines deposition rate and penetration |
| Arc voltage | 25–35 V | Affects arc stability and bead shape |
| Welding speed | 20–50 cm/min | Affects dilution and heat input |
| Preheat temperature | 150–300°C | Prevents cracking in the hard deposit |
| Interpass temperature | 200–300°C | Controls the cooling rate and microstructure |
The paper reports that the cladding hardness reached HRC47. This is a typical hardness for a high-chromium wear-resistant layer. The hardness is achieved through the formation of chromium carbides in a martensitic or bainitic matrix. The exact hardness depends on the alloy composition and the cooling rate.
2.3 Quality Inspection
The paper emphasizes the importance of quality inspection for roll cladding. The inspection typically includes:
- Visual inspection: The deposit should be smooth, free of cracks, porosity, and slag inclusions.
- Hardness testing: The deposit hardness should be within the specified range.
- Ultrasonic testing: To detect lack of fusion or cracking at the interface.
- Magnetic particle testing: To detect surface cracks.
- Metallographic examination: To verify the microstructure and the bond quality.
In roll cladding, the most common defects are:
- Cracking: Caused by high hardness and high residual stress.
- Porosity: Caused by gas entrapment or contaminated surface.
- Lack of fusion: Caused by insufficient heat input or incorrect welding parameters.
- Slag inclusions: Caused by improper slag removal between passes.
3. Practical Implications and Shop Floor Experience
3.1 The Importance of Preheat and Interpass Temperature
The paper emphasizes the importance of preheat and interpass temperature control. This is critical for roll cladding because the hard deposit is prone to cracking. In my experience, the most common cause of cracking in roll cladding is insufficient preheat. The hard deposit has low ductility, and when it cools rapidly, the residual stress can exceed the fracture strength, causing cracks. The preheat and interpass temperature must be maintained within a narrow range to ensure that the deposit cools at a controlled rate.
3.2 The Role of Dilution
Dilution is a critical parameter in roll cladding. Dilution is the amount of base metal that melts and mixes with the cladding deposit. High dilution reduces the hardness and wear resistance of the deposit because the base metal dilutes the alloying elements. Low dilution can cause lack of fusion. The paper likely optimized the welding parameters to achieve a dilution of 10–20%, which is typical for roll cladding.
3.3 Real Project Experience
I have seen roll cladding projects where the hardness was below specification because the dilution was too high. The welder was using too high a current, which increased the penetration and dilution. By reducing the current and increasing the travel speed, we were able to reduce the dilution and achieve the required hardness. This is a common issue in roll cladding, and it highlights the importance of process control.
4. Study Insights and Recommendations
4.1 The Economic Benefits of Roll Cladding
The paper reports that the cladding increased the roll life by more than one time. This is a significant economic benefit because rolls are expensive and their replacement costs include not just the roll itself but also the downtime of the mill. By cladding the rolls, the mill can extend the service life and reduce the frequency of roll changes.
4.2 The Importance of Process Qualification
Roll cladding is a critical process that must be qualified before production. The qualification should include:
- Procedure qualification: Welding parameters, materials, and preheat/interpass temperatures.
- Performance qualification: The welder's ability to produce a consistent deposit.
- Metallographic examination: To verify the bond quality and microstructure.
- Hardness testing: To verify the deposit hardness.
4.3 The Role of Standards
Roll cladding is not typically governed by a specific standard, but the quality requirements are usually specified by the mill. In some cases, the rolls may be manufactured to ASTM or DIN standards, which specify the material properties. The cladding process must be qualified to meet these requirements.
5. Concluding Remarks
This paper provides a good overview of roll cladding technology for a reversing hot mill. The key technical points are the selection of cladding materials and flux, the determination of welding parameters, and the inspection of cladding quality. The result—a hardness of HRC47 and a service life increase of more than one time—demonstrates the effectiveness of the process. For engineers involved in roll cladding, this paper is a useful reference for understanding the process parameters and quality requirements. In my experience, the most critical factors are preheat and interpass temperature control, dilution control, and the selection of the right cladding material. Roll cladding is a demanding application, but when done correctly, it can significantly extend the service life of expensive mill rolls and reduce downtime. The key is to treat it as a qualified, controlled process, not as a routine welding operation.
Zhuojin Pipe Fitting Co., Ltd