Large-Area Wear-Resistant Alloy Composite Plate Surfacing Technology and Its Applications
Introduction and Literature Context
The paper by Qian Qiang, Bao Xiaobing, Cui Rong, and Huang Wenzhe from the Harbin Welding Research Institute, published in Welding (1990, No. 3), addresses the technology of large-area wear-resistant alloy composite plate surfacing. This is a classic paper from the early 1990s that remains relevant today because the fundamental challenges of producing wear-resistant composite plates have not changed significantly.
The paper focuses on the powder-filled metal submerged arc welding (SAW) process for depositing wear-resistant alloy layers on large plates. This is a high-deposition process that can achieve the productivity needed for industrial-scale production of wear-resistant composite plates used in mining, cement, steel, and power generation industries.
Technical Analysis of Powder-Filled Metal SAW Surfacing
Process Principles and Advantages
Powder-filled metal SAW is a variant of conventional submerged arc welding where the filler metal is in the form of a powder rather than a solid wire. The powder is delivered to the welding zone through a special feeding system, and the arc melts both the powder and the base metal to form the deposit.
The key advantages of this process for large-area surfacing are:
- High deposition rate: Powder-filled SAW can achieve deposition rates of 10-20 kg/hour, significantly higher than conventional SAW with solid wire (5-10 kg/hour).
- Excellent bead appearance: The submerged arc process produces a smooth, uniform bead with minimal spatter.
- Deep penetration: The arc is shielded by the flux, allowing deep penetration into the base metal, which ensures good fusion.
- Flexibility in alloy composition: By adjusting the powder composition, a wide range of wear-resistant alloys can be deposited.
Powder Filler Metal Composition and Selection
The selection of powder filler metal is critical for achieving the desired wear resistance. The paper discusses various alloy systems, including:
| Alloy System | Typical Composition | Hardness (HRC) | Primary Wear Mechanism | Application |
|---|---|---|---|---|
| High-chromium cast iron | 15-30% Cr, 2-4% C | 55-65 | Abrasive wear | Mining, cement |
| Martensitic stainless | 12-18% Cr, 0.1-0.3% C | 40-50 | Impact and abrasive | Crushers, mills |
| Ni-Cr-B-Si (hardfacing) | 5-15% Ni, 10-20% Cr, 2-4% B, 3-5% Si | 45-60 | Abrasive and corrosive | Chemical, power |
| Fe-Cr-C (high-carbon) | 20-35% Cr, 4-6% C | 55-65 | Severe abrasive | Chutes, hoppers |
The powder composition must be carefully controlled to ensure consistent deposit chemistry. Variations in powder composition can lead to inconsistent hardness and wear resistance, which is a common quality issue in surfacing operations.
Process Parameters and Their Effects
The paper discusses the process parameters that affect the quality of the surfacing deposit:
| Parameter | Typical Range | Effect on Quality |
|---|---|---|
| Welding current | 300-600 A | Too low: lack of fusion; too high: excessive dilution |
| Arc voltage | 25-35 V | Too low: poor bead shape; too high: excessive spatter |
| Travel speed | 20-50 cm/min | Too fast: poor fusion; too slow: excessive heat input |
| Powder feed rate | 50-150 g/min | Too low: insufficient deposit; too high: poor fusion |
| Preheating temperature | 100-200°C | Prevents cracking in high-carbon alloys |
Dilution is a critical parameter in surfacing. The dilution ratio (the percentage of base metal in the deposit) directly affects the hardness and wear resistance. For wear-resistant surfacing, dilution should be kept below 15-20%. Higher dilution means the deposit contains more base metal, which reduces the alloy content and thus the hardness.
Integration with Manufacturing Practice
Production of Wear-Resistant Composite Plates
In my experience, the production of wear-resistant composite plates involves several steps:
- Base metal preparation: The base plate (typically mild steel, 10-30 mm thick) is cleaned and preheated if necessary.
- Surfacing: The powder-filled SAW process deposits the wear-resistant alloy in multiple passes to achieve the desired thickness (typically 5-15 mm).
- Cooling and stress relief: The composite plate is cooled slowly to prevent cracking. For high-carbon alloys, post-weld heat treatment may be required.
- Inspection: The plate is inspected for surface defects, cracks, and hardness consistency.
The key challenge is maintaining consistent quality across large areas. A 2m x 3m plate requires many passes, and any variation in process parameters can lead to inconsistent properties.
Common Defects and Countermeasures
| Defect | Root Cause | Countermeasure |
|---|---|---|
| Cracking | High hardness, high carbon content, inadequate preheat | Increase preheat, use lower carbon alloy, post-weld heat treatment |
| Porosity | Moisture in powder or flux, inadequate shielding | Dry powder and flux, increase shielding gas flow |
| Lack of fusion | Low heat input, improper travel speed | Increase current, reduce travel speed |
| Inconsistent hardness | Variation in powder composition, dilution | Control powder composition, monitor dilution |
| Spatter | High voltage, improper powder feed | Adjust voltage, optimize powder feed rate |
Economic Considerations
The economic viability of wear-resistant composite plates depends on the application. In high-wear environments, the composite plate can last 3-5 times longer than conventional steel plate. The cost savings come from:
- Reduced downtime for maintenance
- Reduced material consumption
- Improved equipment availability
However, the initial cost of composite plate is significantly higher than conventional steel. The payback period depends on the severity of the wear environment and the cost of downtime.
Critical Assessment and Reflections
Evolution of the Technology
Since this paper was published in 1990, the technology has evolved significantly. Modern powder-filled SAW systems use advanced control systems to maintain consistent powder feed rates and process parameters. The development of metal-cored wires and flux-cored wires has also provided alternatives to powder-filled SAW.
However, the fundamental principles remain the same. The powder-filled SAW process is still used for large-area surfacing, particularly in applications where high deposition rates and consistent quality are required.
Comparison with Alternative Processes
| Process | Deposition Rate (kg/hr) | Dilution (%) | Hardness Consistency | Cost |
|---|---|---|---|---|
| Powder-filled SAW | 10-20 | 10-20 | Good | Moderate |
| Flux-cored wire SAW | 8-15 | 15-25 | Good | Moderate |
| Plasma transferred arc (PTA) | 2-5 | 5-10 | Excellent | High |
| Laser cladding | 1-3 | 2-5 | Excellent | Very high |
| Thermal spray | 5-10 | 0 | Poor | Low |
PTA and laser cladding offer better dilution control and hardness consistency, but at significantly higher cost and lower deposition rates. Powder-filled SAW remains the most cost-effective process for large-area surfacing where high deposition rates are needed.
Practical Lessons from the Field
In one project I was involved in, we used powder-filled SAW to produce wear-resistant plates for a cement plant's raw mill. The plates were 3m x 1.5m, with a 10mm wear-resistant layer. The initial production run had significant cracking issues due to insufficient preheat. After increasing the preheat temperature from 100°C to 180°C and adding a post-weld stress relief treatment, the cracking problem was eliminated.
The key lesson was that the process parameters must be optimized for each specific alloy system and plate size. What works for one alloy may not work for another. The paper provides a good foundation, but practical experience is essential for successful implementation.
Conclusions and Practical Recommendations
The paper by Qian Qiang et al. provides a comprehensive overview of powder-filled metal SAW for large-area wear-resistant alloy composite plate surfacing. The process offers significant advantages in deposition rate, quality, and cost-effectiveness for large-scale production.
From my perspective as a manufacturing professional, the key takeaways are:
- Powder-filled SAW is the most cost-effective process for large-area wear-resistant surfacing, offering high deposition rates and good quality.
- The selection of powder composition is critical for achieving the desired wear resistance and must be matched to the specific application.
- Process parameters, particularly dilution, must be carefully controlled to ensure consistent deposit properties.
- Preheat and post-weld heat treatment are essential for preventing cracking in high-hardness alloys.
- The technology has evolved since 1990, but the fundamental principles remain unchanged.
For engineers considering this technology, I would recommend starting with a thorough understanding of the wear environment and the required wear resistance. The alloy system should be selected based on the dominant wear mechanism. Process parameters should be optimized through a systematic trial program, with careful monitoring of dilution and hardness.
The production of wear-resistant composite plates is a specialized field that requires both theoretical knowledge and practical experience. The paper provides a solid foundation, but successful implementation requires attention to detail and a willingness to learn from failures. The rewards are significant: longer equipment life, reduced downtime, and improved productivity.