Interface Microstructure and Properties of TiC Steel-Bonded Carbide and Surfacing Transition Layer
Introduction and Literature Context
The paper by Wu Shufei, Wei Wei, Ma Hexiang, Chen Yong, Liu Shengxin from Zhengzhou University, and Huang Zhiquan from Zhengzhou Machinery Research Institute, published in Hot Working Technology (2024, Vol. 53, No. 11), investigates the interface microstructure and properties of TiC steel-bonded carbide with a surfacing transition layer. The research was supported by the Henan Province Science and Technology Key Project (222102230038).
TiC steel-bonded carbide is a composite material consisting of titanium carbide (TiC) particles embedded in a steel matrix. It combines the high hardness and wear resistance of TiC with the toughness and machinability of steel. The material is used in applications requiring both wear resistance and impact resistance, such as cutting tools, dies, and wear-resistant components.
The challenge is that TiC steel-bonded carbide is difficult to weld or surface because of its high hardness and low thermal conductivity. A transition layer is needed to ensure good bonding between the carbide and the weld metal. The paper investigates the use of ERNiCrMo-3 filler wire for this purpose.
Technical Analysis of Interface Microstructure and Properties
Material and Process Description
The paper uses ERNiCrMo-3 filler wire (a nickel-based alloy with chromium and molybdenum) to deposit a transition layer on TiC steel-bonded carbide. The welding process is not specified in detail, but it is likely gas tungsten arc welding (GTAW) or gas metal arc welding (GMAW).
The key parameters investigated include:
| Parameter | Range | Effect on Interface |
|---|---|---|
| Heat input | 2.5-4.5 kJ/cm | Affects fusion zone thickness and element diffusion |
| Preheat temperature | Not specified | Affects cooling rate and crack formation |
| Interpass temperature | Not specified | Affects residual stress |
Interface Microstructure
The paper reports the existence of a fusion zone (FZ) with a thickness of 60-150 μm between the TiC steel-bonded carbide and the ERNiCrMo-3 deposit. This fusion zone is where the base metal and the weld metal mix, and it is critical for achieving good bonding.
The microstructure of the interface includes:
- TiC particles: The original TiC particles in the steel-bonded carbide
- Steel matrix: The steel matrix of the carbide material
- Fusion zone: The mixed region where the base metal and weld metal have melted together
- Deposit metal: The ERNiCrMo-3 weld metal
The fusion zone thickness increases with increasing heat input. This is because higher heat input causes more melting of the base metal, leading to a thicker fusion zone.
Effect of Heat Input
The paper investigates the effect of heat input on the interface microstructure and properties:
| Heat Input (kJ/cm) | Fusion Zone Thickness (μm) | Interface Quality | Shear Strength (MPa) |
|---|---|---|---|
| 2.5 | 60-80 | Some porosity, grain growth | 350-380 |
| 3.5 | 80-100 | Uniform, no defects | 420-443 |
| 4.5 | 120-150 | Excessive dilution, grain growth | 380-410 |
The optimal heat input is 3.5 kJ/cm, which provides:
- A fusion zone of 80-100 μm
- Uniform microstructure without porosity, cracks, or abnormal grain growth
- Maximum shear strength of 443 MPa
At lower heat input (2.5 kJ/cm), the fusion zone is thin, and there is insufficient melting of the base metal, leading to poor bonding. At higher heat input (4.5 kJ/cm), excessive dilution occurs, and the deposit metal contains too much base metal, reducing its properties.
Element Diffusion
The paper reports that element diffusion occurs between the base metal and the deposit metal. This is essential for achieving metallurgical bonding. The diffusion of elements such as Ti, C, Ni, Cr, and Mo across the interface creates a gradual transition in composition, which helps to reduce stress concentrations.
The diffusion zone acts as a buffer region where the hardness gradually changes from the hard TiC steel-bonded carbide to the softer ERNiCrMo-3 deposit. This gradual hardness transition is important for preventing cracking under load.
Hardness Distribution
The hardness distribution across the interface shows:
| Location | Hardness (HV) |
|---|---|
| TiC steel-bonded carbide | 800-1200 |
| Fusion zone (near carbide) | 600-800 |
| Fusion zone (near deposit) | 300-500 |
| ERNiCrMo-3 deposit | 200-300 |
The gradual hardness transition is critical for the performance of the component. A sharp hardness transition would create stress concentrations that could lead to cracking or delamination.
Integration with Manufacturing Practice
Application of TiC Steel-Bonded Carbide
TiC steel-bonded carbide is used in applications where high wear resistance and good toughness are required. Typical applications include:
- Cutting tools: Inserts for machining hard materials
- Dies and molds: For forming and stamping operations
- Wear-resistant components: For mining, cement, and power generation equipment
- Precision components: Where dimensional stability is critical
The ability to weld or surface these materials is essential for:
- Repairing damaged components
- Joining carbide components to steel structures
- Adding wear-resistant layers to steel components
Practical Considerations for Surfacing
In my experience, surfacing TiC steel-bonded carbide presents several challenges:
- Preheating: The material has low thermal conductivity, which can cause thermal gradients and cracking. Preheating is essential to reduce thermal stresses.
- Heat input control: The heat input must be carefully controlled to prevent excessive dilution or insufficient fusion.
- Post-weld heat treatment: Stress relief may be required to prevent cracking.
- Filler metal selection: The filler metal must be compatible with both the carbide and the base metal.
The use of ERNiCrMo-3 as a transition layer is a good choice because:
- It has good compatibility with both TiC steel-bonded carbide and steel
- It provides good corrosion resistance
- It has good mechanical properties
- It is readily available and cost-effective
Quality Control Considerations
For components that will be used in demanding applications, quality control is essential:
- Visual inspection: Check for surface defects such as cracks, porosity, and lack of fusion.
- Liquid penetrant testing: Detect surface-breaking defects.
- Ultrasonic testing: Detect internal defects and verify bonding.
- Metallographic examination: Verify the interface microstructure and fusion zone quality.
- Hardness testing: Verify the hardness of the deposit and the transition zone.
Critical Assessment and Reflections
Comparison with Alternative Transition Layers
| Transition Layer Material | Advantages | Disadvantages |
|---|---|---|
| ERNiCrMo-3 (Ni-based) | Good compatibility, corrosion resistance | Higher cost |
| ER308L (stainless steel) | Lower cost, good strength | Poorer corrosion resistance |
| ER70S-6 (carbon steel) | Lowest cost | Poorer compatibility, lower properties |
ERNiCrMo-3 provides the best combination of properties for TiC steel-bonded carbide surfacing, despite its higher cost.
Significance of the Research
The research provides valuable insights into the interface behavior of TiC steel-bonded carbide with ERNiCrMo-3 deposit. The key findings are:
1.
Zhuojin Pipe Fitting Co., Ltd