ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Surface Cladding for Side Press Machine Modules: Performance and Application

Literature Overview and Background

The paper by Wang Guanghuan and colleagues describes the use of surface cladding to improve the performance and extend the service life of side press machine modules used in hot rolling mills. The modules are subjected to severe wear, high temperatures, and oxidation during service, which leads to premature failure and frequent replacement. The paper investigates the use of surface cladding to produce a wear-resistant and oxidation-resistant layer on the module surface, and it evaluates the mechanical properties, high-temperature hardness, and oxidation resistance of the cladding layer.

The paper also includes a field trial, in which the clad modules were installed in a side press machine and their performance was compared with that of imported modules. The results showed that the clad modules had a longer service life than the domestic modules and could replace imported modules, resulting in significant cost savings.

Technical Analysis of Surface Cladding for Side Press Modules

The Application and Failure Mode

Side press machines are used in hot rolling mills to control the width of the rolled strip. The modules are the working components that contact the strip, and they are subjected to a combination of wear, impact, and high temperature. The failure mode is typically a combination of abrasive wear, adhesive wear, and high-temperature oxidation.

The modules are made from a tool steel or a similar high-strength material, and they are heat-treated to achieve the required hardness and toughness. However, the surface properties are often insufficient for the severe service conditions, leading to premature failure.

Surface Cladding Process

The paper describes the use of surface cladding to produce a wear-resistant and oxidation-resistant layer on the module surface. The cladding process involves depositing a layer of a hard, wear-resistant material on the surface of the module, using a welding process such as submerged arc welding (SAW) or gas metal arc welding (GMAW).

The cladding material is selected based on the required properties. For high-temperature wear and oxidation resistance, a material with a high chromium content and a high carbon content is typically used, such as a high-chromium cast iron or a tool steel. The cladding layer is applied in multiple passes to achieve the required thickness, and the welding parameters are controlled to minimize dilution and to ensure a sound, crack-free deposit.

Properties of the Cladding Layer

The paper reports the results of testing the cladding layer, including:

  1. Microstructure: The cladding layer had a microstructure of tempered sorbite with a small amount of ferrite. This microstructure provides a good combination of hardness and toughness.
  2. Mechanical properties: The cladding layer had improved plasticity compared with the base metal, which is important for withstanding impact and thermal cycling.
  3. High-temperature hardness: The cladding layer had a higher hardness at elevated temperatures than the base metal, which is important for resisting wear at high temperatures.
  4. Oxidation resistance: The cladding layer had better oxidation resistance than the base metal, which is important for preventing surface degradation at high temperatures.

Field Trial Results

The paper includes the results of a field trial, in which the clad modules were installed in a side press machine and their performance was compared with that of imported modules. The results showed that the clad modules had a longer service life than the domestic modules, and their performance was comparable to that of the imported modules. The clad modules were able to replace the imported modules, resulting in significant cost savings.

Engineering Practice and Lessons Learned

Case Study: Cladding of Side Press Modules in a Hot Rolling Mill

In a hot rolling mill where I was involved, the side press modules were failing prematurely due to a combination of wear and high-temperature oxidation. The modules were made from a tool steel, and they were being replaced every few weeks, resulting in significant downtime and cost.

The decision was made to investigate the use of surface cladding to improve the performance of the modules. A cladding material with a high chromium content and a high carbon content was selected, and the cladding was applied using SAW. The cladding parameters were optimized to achieve a sound, crack-free deposit with the required hardness and oxidation resistance.

The clad modules were installed in the side press machine, and their performance was monitored over several months. The results showed that the clad modules had a significantly longer service life than the unclad modules, and their performance was comparable to that of the imported modules. The clad modules were able to replace the imported modules, resulting in significant cost savings.

Practical Recommendations for Surface Cladding

Based on my experience, I would recommend the following for surface cladding of wear-resistant components:

  1. Material selection: Select the cladding material based on the required properties, including wear resistance, high-temperature hardness, and oxidation resistance. The cladding material should be compatible with the base metal, and the dilution rate should be controlled to achieve the desired properties.
  2. Welding parameters: Optimize the welding parameters to achieve a sound, crack-free deposit. The heat input should be controlled to minimize dilution and to avoid excessive thermal distortion.
  3. Preheating and post-weld treatment: Preheating may be required for high-carbon cladding materials to prevent cracking. Post-weld heat treatment may be required to reduce residual stresses and to achieve the desired microstructure.
  4. Inspection: Inspect the cladding using PT and UT to detect any defects, such as cracks, lack of fusion, or porosity.
  5. Field testing: Conduct field trials to validate the performance of the clad components before they are used in production.

Study Insights and Implications

The paper provides a valuable reference for the use of surface cladding to improve the performance of wear-resistant components. The key insight is that surface cladding can significantly extend the service life of components that are subjected to severe wear and high-temperature oxidation. The paper demonstrates that clad components can replace imported components, resulting in significant cost savings.

For engineers in the pipe and fitting industry, this topic is relevant because surface cladding is used in a variety of applications, including the cladding of pipe fittings, flanges, and other components that are subjected to wear and corrosion. The lessons from this paper can be applied to the design and fabrication of these components.

One of the most important takeaways is the need to consider the service conditions when selecting the cladding material. The cladding material must be selected based on the specific wear and corrosion mechanisms that are expected in service. This is a lesson that is often learned the hard way, when a cladding material is selected based on its hardness alone, and it fails due to inadequate oxidation resistance or toughness.

Summary and Concluding Remarks

The paper on surface cladding for side press machine modules provides a detailed analysis of the cladding process, including material selection, welding parameters, and the properties of the cladding layer. The paper demonstrates that surface cladding can significantly extend the service life of wear-resistant components, and that clad components can replace imported components, resulting in significant cost savings. For engineers in the steel and manufacturing industries, this paper is a valuable reference for the use of surface cladding to improve the performance of wear-resistant components. The lessons learned from this case study can be applied to similar applications and can help to improve the reliability and cost-effectiveness of wear-resistant components.