Regenerative Hardfacing Repair of Φ1700×1800 Roller Press Squeeze Rollers

Overview of the Repair Challenge

The Jiangxi Yadong case is a classic example of what I call "productive wear"—the kind of wear that is not a failure, but an economic opportunity if you know how to exploit it. The Φ1700×1800 roller press, manufactured by KHD, is a massive piece of equipment. When the squeeze rollers wear, the grinding efficiency drops, the product fineness drifts, and the whole cement line starts to underperform. The decision to repair rather than replace is driven by simple economics: a new roller costs millions of yuan and months of lead time, while a regenerative hardfacing repair can be done on site or in a specialized shop for a fraction of that cost and in a fraction of the time.

The key technical insight from this paper is that the repair is not just about putting metal back. It is about restoring the wear-resistant surface profile, the hardness distribution, and the metallurgical integrity of the base material. The rollers are made of high-alloy steel, often with a hardened surface layer. The hardfacing process must be carefully matched to the base material to avoid cracking, spalling, or dilution problems.

Technical Parameters and Process Windows

The paper describes the repair of rollers that had been in service for a significant period. The wear pattern is typically a combination of abrasive wear from the material being ground and fatigue spalling from the repeated compressive loading. The repair process involves:

Parameter Typical Value Notes
Roller diameter Φ1700 mm Large diameter requires careful preheat and interpass control
Roller width 1800 mm Wide surface means long welding runs, high heat input
Base material High-alloy steel, hardened Weldability is poor; preheat is mandatory
Hardfacing material High-chromium iron-based or Ni-Cr-B-Si alloy Must match the wear mechanism
Preheat temperature 150–250°C Prevents hydrogen-induced cracking
Interpass temperature 200–300°C Must be controlled to avoid over-tempering
Welding method Submerged arc or flux-cored wire High deposition rate, good quality
Post-weld treatment Stress relief or controlled cooling Prevents residual stress cracking

The critical point here is that the hardfacing layer must have a hardness that matches or slightly exceeds the original surface. If the hardfacing is too soft, it will wear quickly. If it is too hard, it may crack or spall. The paper emphasizes the importance of selecting a filler material that forms a hard carbide phase (such as Cr7C3 or CrB) in a martensitic matrix.

Metallurgical Considerations and Defect Analysis

The biggest risk in this repair is cracking. The base material is hardened, and the hardfacing layer is brittle. When the weld cools, the contraction of the hardfacing layer creates tensile stresses that can crack the base material. The paper addresses this through:

  1. Preheat: Preheating the roller to 150–250°C reduces the temperature gradient and slows the cooling rate, allowing hydrogen to diffuse out and reducing the risk of cold cracking.
  2. Interpass temperature control: Keeping the interpass temperature in the 200–300°C range ensures that the hardfacing layer does not over-temper, which would reduce its hardness.
  3. Welding sequence: The paper recommends a spiral or circumferential welding sequence that balances the heat input and minimizes distortion. For a roller of this size, the welding must be done in a symmetrical pattern to avoid warping.
  4. Post-weld inspection: After welding, the repaired surface should be inspected using magnetic particle testing (MT) or ultrasonic testing (UT) to detect any cracks or lack of fusion. The paper also recommends a hardness survey across the repaired surface to verify that the hardness is uniform.

Practical Lessons from the Shop Floor

I have seen many roller press repairs go wrong, and the most common cause is insufficient preheat or poor interpass temperature control. The welder gets into a rhythm, the temperature drifts down, and the next weld bead is deposited on a cold surface. The result is a crack that propagates through the hardfacing layer and into the base material. The roller then fails in service, and the repair is worse than the original wear.

Another common issue is dilution. The hardfacing material is designed to be deposited in a thin layer, but if the welding parameters are too aggressive, the base material melts and mixes with the filler, reducing the hardness of the hardfacing layer. The paper recommends a low heat input and a stringer bead technique to minimize dilution.

Summary and Practical Implications

The regenerative hardfacing repair of roller press squeeze rollers is a proven and cost-effective method for extending the service life of these critical components. The success of the repair depends on careful control of preheat, interpass temperature, welding parameters, and post-weld inspection. The paper provides a solid technical foundation for this process, and the practical lessons from the shop floor reinforce the importance of discipline and attention to detail. For any plant considering this repair, I would emphasize that the quality of the repair is directly proportional to the quality of the process control. Do not cut corners on preheat, do not rush the welding, and do not skip the post-weld inspection. The rollers are too expensive to gamble on.