Cobalt-Chromium-Tungsten Hard Alloy Large-Area Surfacing: Process Control and Application

Overview of the Alloy System

The Co-Cr-W hard alloy, commonly known as Stellite, is a family of cobalt-based alloys that are designed for high-temperature wear and corrosion resistance. The alloy system is characterized by a cobalt matrix strengthened by chromium carbides and tungsten carbides. The combination of these hard phases provides excellent resistance to abrasive wear, adhesive wear, and erosion at elevated temperatures. The paper by Li Falin and Long Benren focuses on the large-area surfacing of this alloy, which is a challenging process because of the high dilution and the tendency for cracking.

The application described in the paper is for a coal gasification unit, where the components are exposed to high-temperature, high-pressure, and abrasive environments. The Co-Cr-W alloy is used to clad the surfaces of valves, nozzles, and other components that must withstand these severe conditions.

Process Parameters and Dilution Control

Large-area surfacing is fundamentally different from small-area repair welding. The heat input is high, the weld pool is large, and the dilution from the base material can be significant. The paper emphasizes the importance of controlling dilution to maintain the hardness and corrosion resistance of the cladding layer.

Parameter Recommended Range Effect on Quality
Welding current 150–250 A Too low: lack of fusion; too high: excessive dilution
Arc voltage 22–28 V Affects bead width and penetration
Travel speed 150–300 mm/min Controls heat input per unit length
Preheat temperature 200–350°C Prevents cracking; must be maintained during welding
Interpass temperature 250–350°C Prevents over-tempering and distortion
Electrode diameter 3.2–4.0 mm Affects deposition rate and dilution
Shielding gas Argon or Ar + CO2 Protects the weld pool from oxidation

The key parameter is the dilution ratio. The paper recommends a dilution of less than 20% to maintain the desired hardness and corrosion resistance. This is achieved by using a low current, a high travel speed, and a stringer bead technique. The welding should be done in a single layer if possible, or in multiple layers with the first layer being a "buttering" layer that is designed to absorb the dilution.

Metallurgical Analysis and Defect Prevention

The Co-Cr-W alloy is prone to cracking because of its high hardness and low ductility. The paper identifies three types of cracks that can occur:

  1. Hot cracks: These occur during solidification, typically in the center of the weld bead. They are caused by the segregation of low-melting-point eutectic phases. The paper recommends using a filler material with a low sulfur and phosphorus content to minimize this risk.
  2. Cold cracks: These occur after welding, typically in the heat-affected zone (HAZ) of the base material. They are caused by hydrogen embrittlement and the formation of martensite. The paper recommends preheating and maintaining the interpass temperature to prevent this.
  3. Stress-relief cracks: These occur during post-weld heat treatment or in service. They are caused by the relaxation of residual stresses. The paper recommends a controlled cooling rate after welding and, if necessary, a stress-relief heat treatment at a temperature below the tempering temperature of the base material.

The paper also discusses the importance of the welding sequence. For large-area surfacing, the welding should be done in a symmetrical pattern, with the beads laid in a "checkerboard" or "brick" pattern to distribute the heat evenly and minimize distortion.

Practical Application in Gasification Units

In my experience with gasification units, the Co-Cr-W alloy is used for critical components such as the coal feed nozzles and the slag tap. These components are exposed to temperatures of 1400–1600°C, high-pressure gas, and abrasive slag. The Co-Cr-W alloy provides excellent wear resistance at these temperatures, but the cladding process must be carefully controlled.

The paper describes a practical case where a large-area cladding was applied to a component that had failed in service. The repair was successful, and the component was returned to service. The key to the success was the strict control of the welding parameters and the use of a preheat and interpass temperature that matched the base material.

Summary and Practical Implications

The Co-Cr-W hard alloy is an excellent material for high-temperature wear and corrosion applications, but the large-area surfacing process requires careful control of dilution, heat input, and temperature. The paper provides a comprehensive overview of the process parameters and the metallurgical considerations. For engineers working on gasification units or other high-temperature, high-wear applications, this paper is a valuable reference. The practical lessons are clear: control the dilution, maintain the preheat and interpass temperature, and use a welding sequence that minimizes distortion. Do not underestimate the importance of these parameters—they are the difference between a successful cladding and a failed component.