Crevice Corrosion Hardfacing for Steam Turbine Components

The Corrosion Problem in Steam Turbines

The 2000 paper by Wang Changzhu and Zhao Yujiang from Harbin Turbine Works addresses a problem that is often overlooked in the design of steam turbines: crevice corrosion. This is a localized form of corrosion that occurs in narrow gaps or crevices where stagnant water can accumulate. In steam turbines, crevices are found at blade roots, diaphragm joints, and other assembly interfaces. The corrosion can lead to pitting, stress corrosion cracking, and ultimately to component failure.

The paper's contribution is the development of a hardfacing process for steam turbine components that are susceptible to crevice corrosion. The process involves depositing a corrosion-resistant alloy on the component surface, followed by post-weld inspection to verify the integrity of the deposit.

Hardfacing Process Development

The paper discusses the selection of the hardfacing material and the welding process. The key requirement is that the hardfacing material must be resistant to crevice corrosion in the steam environment, which typically contains chlorides and other aggressive species.

The authors selected a nickel-based alloy, which provides excellent corrosion resistance in steam environments. The hardfacing process is summarised below:

Parameter Optimal Value Practical Significance
Hardfacing material Ni-Cr-Mo alloy (e.g., Inconel 625) Excellent crevice corrosion resistance
Process GTAW (TIG) with filler wire Precise control of heat input and dilution
Preheat temperature 100–150°C Prevents cold cracking in the base material
Interpass temperature < 150°C Prevents overheating and distortion
Deposit thickness 3–5 mm Provides sufficient corrosion allowance
Post-weld inspection PT, UT, and hardness testing Verifies integrity and quality of deposit

The use of GTAW is significant. This process provides precise control of heat input, which is essential for welding thin-walled turbine components without distortion. The process also allows the welder to control the dilution rate, ensuring that the hardfacing layer retains its corrosion resistance.

Inspection and Quality Control

The paper emphasises the importance of post-weld inspection. The hardfacing layer must be free of cracks, porosity, and lack of fusion, as these defects can serve as initiation sites for corrosion. The inspection methods include:

  1. Penetrant testing (PT): Detects surface cracks and porosity.
  2. Ultrasonic testing (UT): Detects lack of fusion and internal defects.
  3. Hardness testing: Verifies that the hardfacing layer has the expected hardness and that the HAZ has not been softened excessively.

The paper also discusses the importance of controlling the welding parameters to minimise dilution. If the dilution rate is too high, the nickel-based alloy becomes contaminated with iron from the base material, reducing its corrosion resistance. The authors recommend a dilution rate of less than 15%, which is achieved by using a low current and a controlled travel speed.

Practical Considerations and Lessons

In my experience, the hardfacing of steam turbine components is a delicate operation that requires a high level of skill and attention to detail. The components are often thin-walled and have complex geometries, which makes them susceptible to distortion. The following points are critical:

  1. Surface preparation: The component surface must be clean and free of oil, grease, and oxidation. Grinding should be done with a fine-grit wheel to avoid creating stress concentrations.
  2. Fixture design: The component must be fixtured securely to prevent movement during welding. A rotating fixture is often used to ensure uniform heat distribution.
  3. Welding sequence: A staggered welding sequence should be used to minimise distortion. The welder should deposit short beads, allowing each bead to cool below 150°C before the next is deposited.
  4. Post-weld heat treatment: A stress-relief treatment at 400–500°C may be required for components with high residual stress. However, this treatment must be carefully controlled to avoid softening the base material.

Reflections and Outlook

The paper provides a good overview of the hardfacing process for steam turbine components, but it is a brief communication (two pages) and lacks depth in several areas. The most valuable lesson is the emphasis on inspection and quality control. In my experience, the failure of hardfaced components is often due to inadequate inspection, not to the hardfacing material itself.

The paper also highlights the importance of understanding the corrosion mechanism. Crevice corrosion is a complex phenomenon that depends on the geometry of the crevice, the chemistry of the water, and the temperature. A hardfacing material that is resistant to crevice corrosion in one application may not be suitable for another. The engineer must understand the specific service conditions before selecting the hardfacing material.

For the future, I see the hardfacing of steam turbine components moving towards laser cladding, which offers better control of dilution and heat input. However, GTAW with a nickel-based filler wire remains a reliable and cost-effective option for many applications.