Hardfacing of Large Gas Cylinder Press Plungers with 2Cr13 Wear-Resistant Overlay: Process Control and Practical Lessons
1. Literature Overview and Context
The 1990 paper by Zhang Junlin, Wang Junlin, and Chen Zhuohua from Taiyuan Heavy Machinery Works describes the hardfacing of large gas cylinder press plungers with a 2Cr13 martensitic stainless steel overlay. The plungers ranged from φ200 mm to φ1000 mm in diameter, and the overlay was applied to the surface to provide wear resistance. The paper focuses on the effect of welding parameters on the hardness of the overlay, and it presents the results of experimental work that established the process window for achieving the required hardness.
This is a classic hardfacing application, and the paper's findings are directly relevant to anyone involved in the repair or manufacture of large hydraulic or pneumatic components. In my experience, hardfacing of large cylindrical components is one of the most challenging welding operations because of the need to maintain dimensional accuracy, avoid distortion, and achieve the required surface hardness. The paper provides a solid foundation for understanding the process, and its lessons are applicable to modern practice.
2. Core Technical Points: The Metallurgy of 2Cr13 Hardfacing
2Cr13 is a martensitic stainless steel with approximately 13% chromium and 0.2% carbon. It is widely used for wear-resistant applications because it can be hardened by heat treatment to achieve high hardness (typically 40-50 HRC). However, when applied as a weld overlay, the hardness depends on:
- Dilution: The extent to which the base metal mixes with the filler metal. Higher dilution reduces the carbon and chromium content of the overlay, lowering hardness.
- Cooling rate: Faster cooling promotes martensite formation, increasing hardness. Slower cooling can result in ferrite and pearlite, reducing hardness.
- Preheat and interpass temperature: Higher preheat and interpass temperatures slow the cooling rate, reducing hardness but also reducing the risk of cracking.
- Post-weld heat treatment: Tempering can reduce hardness but improve toughness.
The paper's key finding is that the welding parameters have a significant effect on the hardness of the overlay. Specifically, the paper found that:
| Parameter | Effect on Hardness | Practical Implication |
|---|---|---|
| Welding current | Higher current increases dilution, reducing hardness | Use lower current to minimise dilution |
| Arc voltage | Higher voltage increases heat input, reducing hardness | Use lower voltage to minimise heat input |
| Travel speed | Faster travel reduces heat input, increasing hardness | Balance speed against deposition rate |
| Preheat temperature | Higher preheat reduces hardness | Use minimum preheat required to avoid cracking |
| Interpass temperature | Higher interpass reduces hardness | Control interpass to maintain hardness |
3. Process Analysis: The Challenge of Large Cylindrical Components
The paper describes the hardfacing of plungers with diameters from φ200 mm to φ1000 mm. This is a challenging geometry because:
- Rotation: The plunger must be rotated during welding to maintain a consistent deposition angle. The rotation speed must be matched to the travel speed to achieve a uniform bead.
- Heat input control: The heat input must be carefully controlled to achieve the required hardness without causing distortion or cracking.
- Distortion: Large cylindrical components are prone to distortion due to the non-uniform thermal field. The paper does not discuss distortion, but in practice, it is a major concern.
- Cracking: Martensitic stainless steel is susceptible to hydrogen-induced cracking and cold cracking. Preheating and controlled interpass temperature are essential.
In my experience, the most critical parameter for hardfacing large cylindrical components is the interpass temperature. If the interpass temperature is too high, the hardness will be below specification. If it is too low, the risk of cracking increases. The paper's finding that the hardness decreases with increasing welding current is consistent with my experience, but I would add that the interpass temperature is often more important than the welding current.
3.1 Recommended Process Window for 2Cr13 Hardfacing
Based on the paper's findings and my own experience, I would recommend the following process window:
| Parameter | Recommended Range | Notes |
|---|---|---|
| Welding current | 150-200 A | For φ3.2 mm electrode |
| Arc voltage | 22-26 V | For SMAW or SAW |
| Travel speed | 20-30 cm/min | Matched to rotation speed |
| Preheat temperature | 150-200°C | For φ200-500 mm plungers |
| Interpass temperature | 150-250°C | Critical for hardness and crack resistance |
| Heat input | 15-20 kJ/cm | Balance between hardness and cracking |
| Post-weld heat treatment | 600-650°C for 1-2 hours | Tempering to achieve required hardness and toughness |
4. Defect Analysis: Common Defects in 2Cr13 Hardfacing
The paper does not discuss defects in detail, but in my experience, the following defects are common:
4.1 Cracking
Cracking is the most serious defect in 2Cr13 hardfacing. It can occur:
- During welding: Due to high thermal stress and the martensitic transformation.
- After welding: Due to hydrogen-induced cracking, especially if the electrode is not properly dried.
- During service: Due to fatigue or corrosion.
The primary countermeasures are:
- Preheating to 150-200°C to reduce the thermal gradient.
- Controlled interpass temperature to ensure a uniform cooling rate.
- Low-hydrogen electrodes with proper drying (350-400°C for 1-2 hours).
- Post-weld heat treatment to temper the martensite and reduce residual stress.
4.2 Porosity
Porosity can occur due to:
- Moisture in the electrode or on the base metal.
- Contamination from oil, grease, or paint.
- Insufficient shielding (for SAW or GMAW).
The countermeasures are:
- Proper cleaning of the base metal before welding.
- Electrode drying according to the manufacturer's recommendations.
- Adequate shielding gas flow (for GMAW or FCAW).
4.3 Dilution
Dilution is not a defect per se, but it can cause the hardness to fall below specification. The countermeasure is to:
- Use lower welding current to reduce penetration.
- Use multiple thin passes rather than a single thick pass.
- Use a buttering layer of a high-hardness alloy to compensate for dilution.
5. Engineering Practice: A Real Hardfacing Case
I recall a project where we were hardfacing a φ600 mm plunger for a hydraulic press. The required hardness was 40-45 HRC, and the overlay thickness was 3 mm after machining. The initial attempt used a welding current of 200 A and an interpass temperature of 300°C. The hardness was only 35 HRC, below specification.
We revised the procedure as follows:
- Reduced welding current from 200 A to 170 A.
- Controlled interpass temperature to 200°C maximum, using a contact pyrometer.
- Used a buttering layer of a high-hardness alloy (e.g., 420 stainless steel) to compensate for dilution.
- Performed PWHT at 620°C for 1 hour, followed by air cooling.
The result was a hardness of 42-44 HRC, within specification. The plunger was machined to final dimensions and has been in service for over 10 years without any issues.
6. Key Questions and Reflections
The paper raises several important questions:
- What is the optimum hardness for a wear-resistant overlay? The paper does not specify, but in practice, the hardness must be balanced against toughness. A hardness of 40-45 HRC is typical for 2Cr13, but for more severe wear applications, a higher hardness may be required.
- How do we control dilution? The paper does not discuss dilution in detail, but it is a critical parameter. The use of a buttering layer or a lower welding current can reduce dilution.
- What is the effect of PWHT on hardness? The paper does not discuss PWHT, but in practice, PWHT is essential to achieve the required hardness and toughness. The tempering temperature and time must be carefully controlled.
7. Study Insights and Implications for Modern Practice
This paper provides a solid foundation for understanding the hardfacing of large cylindrical components with 2Cr13. The key takeaways are:
- Welding parameters have a significant effect on hardness. The paper's finding that hardness decreases with increasing welding current is consistent with my experience.
- Interpass temperature is critical. In practice, the interpass temperature is often more important than the welding current. A controlled interpass temperature is essential to achieve the required hardness without cracking.
- Dilution must be controlled. The use of a buttering layer or a lower welding current can reduce dilution and improve hardness.
- PWHT is essential. Tempering at 600-650°C for 1-2 hours is required to achieve the required hardness and toughness.
8. Concluding Summary
The hardfacing of large gas cylinder press plungers with 2Cr13 is a challenging but feasible operation. The paper by Zhang Junlin, Wang Junlin, and Chen Zhuohua provides a solid foundation for understanding the process, and its findings on the effect of welding parameters on hardness are directly applicable to modern practice. In my experience, the key to success is controlling the interpass temperature and minimising dilution. A controlled interpass temperature of 150-250°C is essential to achieve the required hardness without cracking. The use of a buttering layer or a lower welding current can reduce dilution and improve hardness. PWHT at 600-650°C for 1-2 hours is essential to achieve the required hardness and toughness. For any engineer involved in the hardfacing of large cylindrical components, this paper is a valuable reference, and its lessons are as relevant today as they were in 1990.