Microstructure and Properties of TiC-Reinforced Wear-Resistant Surfacing Joints Produced by Twin-Electrode Arc Welding
The TiC Reinforcement Concept
This 2020 paper from Qilu University of Technology investigates the microstructure and properties of a TiC-reinforced wear-resistant surfacing layer produced by twin-electrode arc welding, compared with conventional single-electrode arc welding. The concept is to use an in-situ reaction to form titanium carbide (TiC) particles within the weld metal, which act as hard, wear-resistant reinforcement in a tough steel matrix. The TiC particles are formed by the reaction between titanium and carbon in the molten weld pool, and their size, distribution, and volume fraction determine the wear resistance of the overlay. The paper's innovation lies in the use of a twin-electrode arc welding process, which splits the welding current between two electrodes, thereby reducing the heat input per electrode and refining the grain structure of the weld metal. The paper's findings are that the twin-electrode process produces a finer microstructure than the conventional process, and that the hardness of the overlay reaches a maximum at a welding current of 180 A, with a decrease at both 150 A and 210 A.
Effect of Welding Current on Microstructure
The paper's systematic study of the effect of welding current on the microstructure is a key contribution. At a low current of 150 A, the heat input is low, and the cooling rate is fast, which results in a fine grain size but also a high risk of porosity or lack of fusion if the current is too low for the electrode diameter. At a high current of 210 A, the heat input is high, and the cooling rate is slow, which promotes grain growth and a coarser microstructure. The optimum at 180 A represents a balance between sufficient heat input for good fusion and a cooling rate that refines the grain structure. The finding that the hardness increases and then decreases with increasing current is a classic example of the trade-off between grain refinement and the formation of softer phases. The finer grain size at 180 A increases the hardness by the Hall-Petch effect, while the higher heat input at 210 A allows the growth of larger grains and the formation of softer ferrite, which reduces the hardness.
Twin-Electrode vs. Conventional Process
The comparison between the twin-electrode and conventional single-electrode processes is the most valuable aspect of the paper. The twin-electrode process, by splitting the current, reduces the heat input per unit length of the weld, which leads to a finer grain structure in the weld metal and the heat-affected zone. This is a significant advantage for wear-resistant surfacing, where a fine grain size improves both the hardness and the toughness of the overlay. The paper's finding that the twin-electrode process produces a finer microstructure than the conventional process is a clear demonstration of the metallurgical benefits of this approach. For a production engineer, this means that the twin-electrode process can achieve the same hardness with a lower heat input, which reduces the risk of distortion and residual stress in the component. However, the practical implementation of the twin-electrode process is more complex, requiring a special torch and a power source that can split the current, and the process is not as widely used as conventional arc welding.
Practical Implications for Wear-Resistant Overlays
The paper's findings have direct implications for the design and production of wear-resistant overlays. The use of TiC reinforcement is a well-established method for improving wear resistance, but the in-situ formation of TiC particles requires careful control of the weld pool chemistry and the cooling rate. The paper's work shows that the welding current is a critical parameter that affects both the grain size and the hardness of the overlay. The optimum current of 180 A is a practical guide for the production engineer, but the exact value will depend on the electrode diameter, the base material, and the specific application. The twin-electrode process offers a significant advantage in terms of microstructure refinement, but it requires a more sophisticated welding setup. For a veteran, the key lesson is that the welding parameters must be optimised for each specific application, and that the microstructure of the overlay is the primary determinant of its performance. The paper's contribution is a valuable addition to the literature on TiC-reinforced wear-resistant overlays, and it provides a practical basis for the development of new surfacing processes.
Summary
This paper provides a detailed study of the microstructure and properties of TiC-reinforced wear-resistant surfacing joints produced by twin-electrode arc welding, demonstrating that the welding current has a significant effect on the grain size and hardness of the overlay. The key technical points are the in-situ formation of TiC particles, the refinement of the grain structure by the twin-electrode process, and the optimisation of the welding current to achieve the maximum hardness. For engineers involved in wear-resistant surfacing, this case highlights the importance of process parameter control, the metallurgical benefits of the twin-electrode process, and the need for a thorough understanding of the relationship between welding parameters, microstructure, and performance. The lessons learned here are directly applicable to the production of wear-resistant overlays for mining equipment, crushers, and other high-wear components.