ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Quality Control of High-Efficiency Automatic Surfacing of Composite Steel Plates

The Quality Gap Between Domestic and Imported Composite Plates

This 2000 paper from the Chinese Academy of Agricultural Mechanization Sciences addresses a practical problem in the production of composite steel plates, which consist of a base plate with a wear-resistant surfacing layer. The paper notes that domestic composite plates, produced by a powder-fed surfacing process, initially had inferior hardness and wear resistance compared with imported plates. The quality gap was attributed to several factors, including a low alloy powder-to-wire ratio, an unsuitable powder composition, and a suboptimal surfacing process. The paper's contribution is to describe a series of process improvements that closed this gap, resulting in domestic composite plates that met or exceeded the quality of imported plates. This is a classic example of the quality improvement process, where a systematic analysis of the root causes of a quality problem leads to targeted process changes.

Root Cause Analysis and Process Improvements

The paper's approach follows a logical problem-solving methodology. The first step is to identify the root causes of the quality gap. The low hardness and wear resistance of the domestic plates were likely caused by a low volume fraction of hard carbide particles in the overlay, which in turn was a result of an insufficient alloy powder addition. The paper's first improvement is to increase the alloy powder-to-wire ratio, which increases the amount of alloying elements in the weld pool and promotes the formation of more hard phases. The second improvement is to adjust the alloy powder composition, likely by increasing the content of carbon and strong carbide formers such as chromium and vanadium, to enhance the hardness and wear resistance of the deposit. The third improvement is to refine the surfacing process, which may involve optimising the welding parameters, the powder feed rate, and the shielding gas flow. The fourth improvement is the post-weld shaping or flattening of the composite plate, which improves the surface quality and the dimensional accuracy.

Metallurgical Basis for the Improvements

The metallurgical basis for these improvements is well understood. The wear resistance of a composite plate is primarily determined by the volume fraction, size, and distribution of hard carbide particles in the overlay. An increase in the alloy powder-to-wire ratio increases the carbon and alloy content of the weld metal, which promotes the formation of more carbides. The adjustment of the powder composition, by adding stronger carbide formers, increases the hardness of the individual carbide particles and improves their resistance to abrasive wear. The refinement of the surfacing process, by optimising the heat input and the powder feed rate, ensures a uniform distribution of the carbides and a sound, porosity-free deposit. The post-weld shaping operation, which is likely a hot or cold rolling process, flattens the surface and improves the bond between the overlay and the base plate.

Quality Control and Verification

The paper's focus on quality control is a key aspect of its contribution. The quality of the composite plate must be verified by a combination of hardness testing, metallographic examination, and wear testing. The paper's finding that the improved domestic plates achieved the quality level of imported plates is a clear demonstration of the effectiveness of the process improvements. For a production engineer, the key lesson is that quality control is not just a final inspection step, but a continuous process that involves monitoring the raw materials, the process parameters, and the finished product. The paper's approach of identifying the root causes of the quality gap and then implementing targeted process improvements is a model of good engineering practice.

Practical Implementation and Lessons Learned

The implementation of these process improvements requires a systematic approach. The first step is to establish a baseline by measuring the hardness and wear resistance of the existing product. The second step is to conduct a series of experiments to determine the effect of each process variable on the product quality. The third step is to optimise the process parameters to achieve the desired quality. The fourth step is to verify the improved process by producing a pilot batch and testing the product. The final step is to implement the improved process in production and to establish a quality control system to monitor the product on a continuous basis. The paper's contribution is a valuable case study in quality improvement, and it provides a practical guide for engineers facing similar quality issues in surfacing processes.

Summary

This paper provides a practical case study in the quality control of high-efficiency automatic surfacing of composite steel plates, demonstrating that a systematic analysis of the root causes of a quality gap can lead to targeted process improvements that close the gap with imported products. The key technical points are the increase in the alloy powder-to-wire ratio, the adjustment of the powder composition, the refinement of the surfacing process, and the post-weld shaping operation. For engineers involved in the production of composite plates or other surfacing applications, this case highlights the importance of root cause analysis, the metallurgical basis for process improvements, and the need for a comprehensive quality control system. The lessons learned here are directly applicable to the production of wear-resistant composite plates for mining, cement, and other high-wear industries.