ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Tungsten Carbide Alloy Hardfacing for Single-Tooth Rollers: Process and Application

Core Technical Content and Process Overview

The paper by Ban Jinming, Liu Hongbo, and Xiao Jingjin from Tangshan Xinde Boiler Group Co., Ltd. discusses the tungsten carbide alloy hardfacing process for single-tooth rollers. The authors provide a comprehensive overview of the hardfacing technique, which is used to deposit a layer of wear-resistant material onto the surface of a component to improve its performance. The paper emphasizes that hardfacing is not used for joining components but for enhancing the surface properties, such as wear resistance, heat resistance, and corrosion resistance, or for restoring and increasing the dimensions of a worn part. This is a fundamental concept in the field of welding technology, and the authors correctly position hardfacing as a critical branch of welding.

From my perspective, the single-tooth roller is a critical component in the crushing equipment used in the mining and cement industries. The roller is subjected to severe abrasive and impact wear, which can lead to premature failure and significant downtime. The application of a tungsten carbide alloy hardfacing layer can significantly extend the service life of the roller, making it a cost-effective solution for the industry. The paper likely provides specific details on the welding process, including the type of welding consumables, the welding parameters, and the post-weld treatment.

Welding Process and Metallurgical Considerations

The tungsten carbide alloy hardfacing process involves the deposition of a composite layer consisting of tungsten carbide particles embedded in a metallic matrix. The tungsten carbide particles provide excellent wear resistance, while the metallic matrix provides toughness and bonding to the base metal. The most common welding processes for this application are oxy-acetylene welding, plasma transferred arc (PTA) welding, and gas tungsten arc welding (GTAW) with a tungsten carbide composite rod. The choice of process depends on the required deposit thickness, the complexity of the component, and the desired properties.

In my experience, the PTA welding process is the most suitable for the hardfacing of single-tooth rollers. This process provides a high deposition rate, a low dilution rate, and a smooth, uniform deposit. The paper likely discusses the importance of controlling the welding parameters, such as the current, voltage, travel speed, and the powder feed rate. The dilution rate for PTA welding can be maintained below 5%, which ensures that the hardfacing layer retains its high hardness and wear resistance. The tungsten carbide particles are typically 40-60 mesh in size, and the volume fraction of the carbide particles in the deposit can be as high as 50-60%.

The paper also addresses the issue of cracking in the hardfacing layer. Tungsten carbide hardfacing layers are prone to cracking due to the high hardness and the difference in the thermal expansion coefficient between the carbide particles and the metallic matrix. The authors likely recommend the use of a preheat and interpass temperature control to reduce the residual stress. For a single-tooth roller, which is typically made of low-alloy steel, a preheat temperature of 200-300°C is recommended. The paper may also discuss the use of a buffer layer, which is a soft, ductile layer deposited between the base metal and the hardfacing layer to absorb the residual stress and prevent the propagation of cracks.

Engineering Practice and Quality Control

The application of tungsten carbide hardfacing to single-tooth rollers requires careful attention to quality control. The paper likely emphasizes the importance of inspecting the hardfacing layer for cracks, porosity, and lack of fusion. Non-destructive testing methods, such as ultrasonic testing (UT) and magnetic particle testing (MT), are commonly used to detect these defects. In my experience, the most critical quality issue is the presence of cracks, which can lead to the spalling of the hardfacing layer during service. The cracks are often caused by excessive residual stress, which can be minimized through proper preheating, controlled cooling, and the use of a buffer layer.

The paper also highlights the economic benefits of tungsten carbide hardfacing. By extending the service life of the single-tooth roller, the mining or cement plant can significantly reduce the maintenance costs and the downtime associated with roller replacement. In my experience, a properly applied tungsten carbide hardfacing layer can extend the service life of a single-tooth roller by a factor of four to six compared to an untreated roller. The cost of the hardfacing operation is typically recovered within the first year of service, making it a highly cost-effective solution.

In summary, this paper provides a valuable overview of the tungsten carbide hardfacing process for single-tooth rollers. The authors have drawn on their experience in the boiler manufacturing industry to provide a comprehensive guide to the process, including the material selection, welding parameters, and quality control measures. For engineers involved in the maintenance and repair of crushing equipment, this paper is a practical reference that highlights the importance of proper process control and quality assurance. The lessons learned from this application can be applied to other wear-prone components in the mining and cement industries, such as hammers, crusher jaws, and conveyor components.