ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING  |  NOTES FROM A 30-YEAR INDUSTRY VETERAN

Strip Cladding of Rolls with Domestic Welding Materials

Background and Objectives

This 1999 paper from Dalian Heavy Industry Group and Jinan No. 2 Machine Tool Group addresses a topic that is central to the steel industry: the repair and manufacture of rolls using strip cladding. Rolls are expensive components, and their service life is often limited by surface wear. Strip cladding offers a way to rebuild worn rolls or to manufacture new rolls with a wear-resistant surface.

The paper's objective is straightforward: select domestic welding materials, test the strip cladding process, determine the effect of welding parameters on the cladding layer, and establish the optimal parameters. The authors then successfully clad a roll that meets the technical requirements.

This is a classic example of applied research. The paper is not trying to discover new physics; it is trying to solve a practical problem using available materials and equipment.

Test Methodology and Parameters

The paper describes a systematic test program. The key variables are:

Variable Range Tested Effect on Cladding
Welding current 500–800 A Affects deposition rate and dilution
Arc voltage 20–26 V Affects bead shape and penetration
Travel speed 100–200 mm/min Affects heat input and bead width
Strip width 30–60 mm Affects deposition rate and coverage
Flux type Agglomerated or fused Affects slag removal and bead quality

The paper emphasizes that the flux must be properly baked and dried before use. Moisture in the flux is a common cause of porosity in strip cladding. I have seen this problem many times. A flux that has been exposed to humid air for even a few hours can pick up enough moisture to cause significant porosity.

The paper also notes that the strip must be clean and free of rust, oil, and other contaminants. The strip edges must be smooth and free of burrs, because burrs can cause arc instability and uneven melting.

Results and Optimal Parameters

The paper reports that the optimal parameters were determined through a combination of visual inspection, dimensional measurement, and mechanical testing. The key results are:

Parameter Optimal Value Effect
Welding current 650–750 A High deposition rate with acceptable dilution
Arc voltage 22–24 V Stable arc with good bead shape
Travel speed 150–180 mm/min Good coverage with minimal undercut
Strip width 60 mm Good balance between deposition rate and control
Preheat temperature 150–200 °C Prevents cracking in the HAZ
Interpass temperature ≤ 250 °C Prevents excessive grain growth

The paper reports that the cladding layer had good surface quality, no cracks, and no porosity. The bond between the cladding and the base metal was metallurgically sound, with no lack of fusion.

One important point that the paper makes is that the cladding layer must be deposited in multiple passes. A single pass with a 60 mm strip can deposit 3–4 mm of material, but the dilution is high. By using multiple passes, the dilution is progressively reduced, and the final layer has the desired composition.

Practical Application and Lessons Learned

The paper describes the successful cladding of a roll that met the technical requirements. This is a significant achievement because it demonstrates that domestic materials can produce a roll of acceptable quality.

From my experience, the following practical lessons are important:

  1. The roll must be preheated uniformly. Uneven preheating causes distortion and cracking. The preheat temperature should be measured at multiple points on the roll surface to ensure uniformity.
  2. The strip cladding head must be properly aligned. The strip must be perpendicular to the roll surface, and the angle of the strip relative to the surface must be controlled. A misaligned strip causes uneven melting and poor bead shape.
  3. The flux layer must be uniform. The flux is deposited ahead of the strip, and its thickness must be consistent. A variable flux thickness causes arc instability and uneven penetration.
  4. The roll must be rotated at a constant speed. The rotational speed must be synchronized with the travel speed of the cladding head. Any variation in speed causes the bead width to vary.
  5. The cladding layer must be inspected after each pass. Visual inspection and, where required, UT or PT should be performed to detect defects early.

Key Questions and Reflections

The paper raises an important question: what is the acceptable dilution for a roll cladding layer?

For a roll that is used in a hot rolling mill, the cladding layer must have high wear resistance and good toughness. The dilution must be controlled to ensure that the deposit has the desired composition. If the dilution is too high, the deposit becomes too hard and brittle, increasing the risk of spalling. If it is too low, the deposit may not have sufficient wear resistance.

In my experience, the dilution should be controlled to 10–15% for the final layer. This can be achieved by using multiple passes and by controlling the heat input.

Another question is whether the cladding layer should be stress-relieved after welding. For a roll, the cladding layer is typically not stress-relieved, because the roll is subsequently machined and used in service. However, if the roll is large and the cladding is thick, stress relief may be necessary to prevent distortion.

Study Insights and Implications

This paper is a good example of how applied research can solve a practical problem. The authors did not try to develop a new process; they took an existing process and optimized it for a specific application using domestic materials.

The key insight is that the optimal parameters are not universal. They depend on the specific materials, the equipment, and the application. A parameter set that works for one roll may not work for another.

For a young engineer, this paper is a good introduction to the practical aspects of strip cladding. For a veteran, it is a reminder that the process must be optimized for each application.

Reference Value and Outlook

This paper is from 1999, but its technical content is still relevant. Strip cladding is still widely used for roll repair and manufacture. The fundamental principles have not changed.

Looking forward, I see three trends that will affect strip cladding:

  1. Wider strips — Wider strips (up to 150 mm) are now available, which increase deposition rate and reduce the number of passes.
  2. Improved fluxes — New flux formulations offer better slag removal and improved bead quality.
  3. Automated control — Modern cladding systems use automated control of current, voltage, and travel speed, which improves consistency.

However, the fundamental principles remain the same. The flux must be dry, the strip must be clean, and the parameters must be optimized for the specific application. This paper, despite its age, provides a solid foundation for understanding these principles.

In summary, this is a practical, well-executed paper that demonstrates the value of applied research. It does not offer revolutionary insights, but it offers a clear, honest account of how a real production problem was solved. That is what makes it valuable. The lessons it teaches — control the parameters, manage the dilution, and inspect the cladding layer — are the same lessons I would give to any young engineer on my team today.