Axial Compression Test and Bearing Capacity of Square CFST Columns with Openings

The Problem with Openings in Concrete-Filled Steel Tubes

Concrete-filled steel tube (CFST) columns are widely used in high-rise buildings and bridges because they combine the strength of steel with the stiffness of concrete. However, the need for service openings — for pipes, ducts, or access — creates a discontinuity in the steel tube that weakens the column. The topic of this study is the behavior of square CFST columns with openings under axial compression, and the determination of their bearing capacity.

The Test Program and Key Findings

The study involved axial compression tests on square CFST columns with openings of different sizes and positions. The key parameters were the opening size, the opening position, and the wall thickness of the steel tube. The results showed that the presence of an opening reduces the bearing capacity of the column, and the reduction is more significant for larger openings and for openings located near the mid-height of the column.

Opening Size Position Bearing Capacity Reduction Failure Mode
Small (≤ 10% width) Mid-height 5-10% Local buckling at opening
Medium (10-20% width) Mid-height 15-25% Local buckling + concrete crushing
Large (> 20% width) Mid-height 30-40% Global buckling + concrete crushing
Medium (10-20% width) Near end 10-15% Local buckling at opening

Steel Pipe Fabrication and Welding Considerations for Openings

The fabrication of CFST columns with openings requires careful planning. The opening is typically cut into the steel tube before the concrete is poured, and the edges of the opening must be reinforced to prevent local buckling. The reinforcement can take the form of a stiffener plate, a collar, or a thicker wall section around the opening.

The cutting of the opening must be performed using a method that does not damage the steel, such as plasma cutting or waterjet cutting. The edges must be ground smooth to remove any notches or burrs, which could act as crack initiation sites. If the opening is reinforced, the stiffener must be welded to the tube using a qualified welding procedure, and the weld must be inspected to ensure full fusion.

Practical Design and Fabrication Guidance

From a practical standpoint, the design of CFST columns with openings should be based on a reduced cross-section that accounts for the area of the opening. The bearing capacity can be estimated using a reduction factor that depends on the opening size and position. However, the design should also consider the local effects, such as stress concentration at the opening edges and the potential for local buckling.

The fabrication sequence is critical. The opening should be cut and reinforced before the concrete is poured, and the reinforcement should be designed to be compatible with the concrete pour. The concrete should be placed using a method that ensures complete filling of the tube, including the region around the opening. Self-consolidating concrete is often used for this purpose because it flows easily and fills all the voids.

Key Lessons and Recommendations

  1. The opening size should be limited to a maximum of 20% of the column width, unless the design is specifically verified by testing.
  2. The opening should be reinforced with a stiffener plate that is welded to the tube and designed to carry the local stresses.
  3. The cutting of the opening should be performed using a controlled method, and the edges should be ground smooth.
  4. The welding of the reinforcement should be performed by a qualified welder and inspected using appropriate NDT methods.
  5. The concrete pour should be carefully planned to ensure complete filling of the tube, especially around the opening.

Concluding Reflection

The axial compression behavior of square CFST columns with openings is a practical problem that requires careful attention to both design and fabrication. The study provides valuable data on the reduction in bearing capacity, but the real lesson is that the opening is a discontinuity that must be managed. The industry veteran's role is to ensure that the fabrication quality is such that the design assumptions are met, and that the opening does not become the weak link in the structure.