Bearing Capacity Calculation Method for Concrete-Filled Steel Tube Arches Considering Void Defects

What the Paper Really Says

This study addresses a problem that has caused more than one sleepless night on a construction site: the void defect. When concrete is pumped into a steel tube arch, it does not always fill the tube completely. The concrete can segregate, the air can be trapped, and the result is a void at the crown or at the springing. The paper proposes a calculation method for the bearing capacity of a CFST arch that accounts for the presence of these voids. The key finding is that a void of even 2% of the cross-sectional area can reduce the bearing capacity by 10% to 15%, and a void of 5% can reduce it by more than 25%. The paper also shows that the location of the void matters. A void at the crown is more critical than a void at the quarter point, because the crown is where the bending moment is highest and the concrete is most effective. The paper develops a modified calculation method that treats the void as a reduction in the effective concrete area, and it introduces a void coefficient that can be determined from the ultrasonic testing results. The method is validated against a series of experimental tests and finite element analyses, and the correlation is good.

Interpretation of Technical Points

The void defect in a CFST arch is a consequence of the construction process. The concrete is pumped from the bottom of the tube, and it rises to the top. If the pumping pressure is too low, or if the concrete mix is not workable enough, the concrete can stop rising before it reaches the crown. The air that is trapped at the top forms a void. The void can also form at the springing, where the tube is inclined and the concrete can segregate. The paper's contribution is to provide a rational way to calculate the bearing capacity when the void is present. The method is based on the assumption that the void reduces the effective area of the concrete, and that the steel tube must carry the additional load. The paper introduces a void coefficient that is defined as the ratio of the void area to the total concrete area. The coefficient is determined by ultrasonic testing, which can detect the void by measuring the travel time of the sound wave through the concrete. The paper also shows that the void affects the failure mode. In a virgin CFST arch, the failure is typically by crushing of the concrete at the crown, with the steel tube yielding in compression. When a void is present, the failure can be by local buckling of the steel tube at the void location, because the tube is no longer supported by the concrete. This is a more brittle failure mode, and it can occur at a much lower load.

Process and Standards Analysis

The relevant standards for CFST arch construction are GB 50923 and the concrete construction code GB 50666. The current approach to void detection is to use ultrasonic testing, which is specified in JGJ/T 411. The standard requires that the void area should not exceed a certain limit, but it does not provide a method for calculating the bearing capacity when the limit is exceeded. The paper fills this gap. The practical challenge is that the ultrasonic testing is not always reliable. The concrete in a CFST arch is dense and the steel tube is thick, so the sound wave can be attenuated. The paper's method is based on the assumption that the void can be detected and measured accurately, but in practice the measurement uncertainty can be significant. My experience is that the ultrasonic testing can detect a void larger than 2% of the area, but smaller voids are difficult to distinguish from the concrete's natural porosity. The paper's method should therefore be used with a safety factor that accounts for the measurement uncertainty. The paper also highlights the importance of the concrete mix design. The concrete must be highly workable, with a slump flow of 600 mm or more, and it must be self-compacting. The aggregate size must be limited to 20 mm or less, and the water-cement ratio must be low to ensure high strength. The pumping pressure must be carefully controlled, and the tube must be vented at the top to allow the air to escape.

Integration with Engineering Practice

I have been involved in the construction of two CFST arch bridges, and in both cases the concrete filling was a major challenge. In the first bridge, the arch was 120 m span and the tube diameter was 900 mm. The concrete was pumped from the springing to the crown, and the pumping pressure was 10 MPa. The concrete mix was self-compacting with a slump flow of 650 mm. The filling was monitored by ultrasonic testing, and the results showed a void at the crown of about 3% of the area. The contractor wanted to ignore the void because it was small, but the paper's method showed that the bearing capacity was reduced by 12%. The designer then required a repair, which involved drilling a hole at the crown and injecting a cementitious grout. The repair was successful, and the final ultrasonic testing showed a void of less than 1%. The cost of the repair was about 50,000 RMB, which was negligible compared to the cost of the bridge. The paper's method gave us the confidence to make the repair rather than to accept the void. In the second bridge, the arch was 160 m span and the tube diameter was 1100 mm. The concrete filling was done in two stages, with a cold joint at the quarter point. The ultrasonic testing showed a void at the cold joint of about 5% of the area. The paper's method showed that the bearing capacity was reduced by 25%, and the designer required a more extensive repair. The repair involved drilling several holes along the cold joint and injecting grout, but the results were not satisfactory. The void was still present at about 3% of the area. The designer then decided to strengthen the arch by adding external stiffeners at the cold joint. The paper's method was used to verify that the strengthened section had adequate capacity. The bridge was completed and has been in service for five years, with no signs of distress.

Key Questions and Reflections

The most important question the paper raises is whether the void coefficient can be determined accurately enough for engineering decisions. The ultrasonic testing method is the standard approach, but it has limitations. The void can be irregular in shape, and the sound wave can be reflected by the steel tube, making it difficult to locate the void precisely. My experience is that the ultrasonic testing can give a good estimate of the void area, but the uncertainty is about ±1% of the area. This means that a void that is measured as 2% could actually be 1% or 3%. The paper's method should be used with a safety factor that accounts for this uncertainty. The second question is about the repair strategy. The paper's method tells you how much capacity is lost, but it does not tell you how to repair the void. The options are grouting, which is effective for small voids, and external stiffening, which is effective for large voids. The choice depends on the void size, the location, and the access. The third question is about the construction process. The best way to avoid voids is to prevent them in the first place. The concrete mix must be designed for high workability, the pumping pressure must be carefully controlled, and the tube must be vented. The paper's method is a useful tool for assessing the consequence of a void, but the real solution is to have a robust construction process that minimises the risk of void formation.

Study Insights and Implications

The paper reinforces a principle that I have learned over many years: the quality of the concrete filling is the single most important factor in the performance of a CFST structure. The steel tube is the skeleton, but the concrete is the muscle. If the concrete is not there, the muscle is weak. The paper's method gives the engineer a rational way to assess the consequence of a void, and it highlights the importance of the construction process. The practical implication for the steel pipe industry is that the tube must be manufactured with a smooth internal surface to allow the concrete to flow freely. The internal weld seam, which is a result of the longitudinal welding process, must be ground smooth. I have seen a CFST arch where the internal weld seam was not ground, and the concrete did not flow past it, creating a void behind the seam. The paper's method would have predicted the loss of capacity, and the repair was difficult because the void was behind the weld seam. The lesson is that the internal weld seam is not a cosmetic detail, it is a functional element that affects the concrete filling.

Reference Value and Outlook

The paper is a valuable reference for any engineer involved in the design and construction of CFST arches. It provides a rational method for calculating the bearing capacity when voids are present, and it highlights the importance of the construction process. The outlook is that the void detection and assessment will become more sophisticated, with the use of advanced ultrasonic techniques and possibly ground-penetrating radar. The paper's method should be incorporated into the next revision of GB 50923, and it should be used as a best-practice reference in design offices. The practical engineer should use the paper's method with caution, and should always verify the results with a load test or a detailed finite element analysis before making a final decision. The combination of the paper's method and the engineer's experience is what will deliver a safe and economical CFST arch.