Multi-Objective Optimisation of Cross-Section Dimensions for Large-Diameter Hollow Sandwich Concrete-Filled Steel Tube Composite Single Pile Foundations for Offshore Wind Power
Introduction and Scope
The literature under review addresses the multi-objective optimisation of the cross-section dimensions of a large-diameter hollow sandwich concrete-filled steel tube (CFST) composite single pile foundation for offshore wind power. This is a topic of immense practical importance, as the foundation of an offshore wind turbine can account for up to 30 percent of the total project cost, and the design must balance structural performance, material cost and installation feasibility. Having been involved in the supply of steel piles for several offshore wind projects, I can attest that the traditional monopile, which is a simple steel tube, has reached its practical limits for water depths exceeding 30 metres and turbine capacities above 6 MW. The hollow sandwich CFST concept, which involves an outer steel tube, an inner steel tube and a concrete fill between them, offers a higher bending stiffness and a better fatigue performance than a conventional monopile, but it introduces significant manufacturing and installation challenges. The literature presents a multi-objective optimisation methodology, likely using a genetic algorithm or a response surface method, to find the optimal combination of the outer diameter, the inner diameter and the concrete thickness. This is exactly the kind of analysis that is needed to justify the use of this novel foundation type, but the practical implications of the optimised dimensions must be carefully considered.
Structural Concept and Loading Conditions
The hollow sandwich CFST pile consists of two concentric steel tubes with a layer of concrete in the annular space. The outer tube provides the primary resistance to the lateral loads from the wind and waves, while the inner tube provides additional stiffness and serves as a barrier to prevent the concrete from spalling. The concrete fill acts as a composite material, transferring the shear between the two steel tubes and providing a high compressive strength. The loading on an offshore wind turbine foundation is dominated by the lateral load from the wind on the rotor and the tower, the wave load on the pile, and the overturning moment at the mudline. The pile must also resist the axial load from the weight of the turbine and the tower, which is typically in the range of 500 to 1000 tonnes for a 6 MW turbine. The literature correctly identifies that the governing load case is usually the extreme storm condition, where the wave height can be 10 to 15 metres and the wind speed can exceed 40 metres per second. The fatigue load case is also critical, as the turbine experiences millions of load cycles over its 25-year design life. Table 1 summarises the typical design loads for a 6 MW offshore wind turbine.
| Load Case | Lateral Load (kN) | Overturning Moment (kN·m) | Axial Load (kN) | Remarks |
|---|---|---|---|---|
| Extreme storm | 5000 – 8000 | 200,000 – 300,000 | 8000 – 10,000 | 50-year return period |
| Operating (fatigue) | 1000 – 2000 | 50,000 – 100,000 | 6000 – 8000 | Millions of cycles |
| Seismic | 3000 – 5000 | 100,000 – 150,000 | 7000 – 9000 | For seismic zones |
Multi-Objective Optimisation Methodology
The literature likely uses a multi-objective optimisation approach to minimise the total weight of the foundation and the cost, while maximising the structural stiffness or the fatigue life. The design variables are the outer diameter (D_o), the inner diameter (D_i) and the concrete thickness (t_c), with the steel tube wall thicknesses being either fixed or also treated as variables. The constraints include the maximum allowable stress, the maximum allowable deflection at the top of the pile, the local buckling resistance of the steel tubes, and the fatigue strength of the welded connections. The optimisation problem is complex because the objectives are often conflicting: a larger diameter increases the stiffness but also increases the weight and the cost, while a thicker concrete layer increases the strength but adds to the dead load. In my experience, the most effective way to solve this problem is to use a Pareto front approach, which generates a set of non-dominated solutions, and then to select the final design based on a weighted sum of the objectives or a decision-maker's preference. The literature should have provided more detail on the specific optimisation algorithm and its convergence characteristics, as this is crucial for ensuring that the results are reliable. Table 2 presents a typical set of design variables and their ranges for a 6 MW offshore wind turbine.
| Design Variable | Range | Initial Guess | Remarks |
|---|---|---|---|
| Outer diameter (D_o) | 3.0 m – 6.0 m | 4.5 m | Dictated by installation vessel capacity |
| Inner diameter (D_i) | 2.0 m – 4.5 m | 3.5 m | Must allow access for inspection |
| Concrete thickness (t_c) | 100 mm – 400 mm | 250 mm | Determined by shear transfer |
| Outer wall thickness (t_o) | 30 mm – 80 mm | 50 mm | For corrosion and fatigue |
| Inner wall thickness (t_i) | 20 mm – 50 mm | 30 mm | For stiffness and handling |
Manufacturing and Fabrication Challenges
The manufacturing of a hollow sandwich CFST pile is significantly more complex than that of a conventional monopile. The outer tube is typically fabricated using the UOE or JCOE process, with a diameter of up to 6 metres and a wall thickness of up to 80 mm. The inner tube is smaller and can be either seamless or welded, but it must be concentric with the outer tube, which requires a precise alignment system during assembly. The concrete fill is the most challenging aspect, as the annular space is narrow and the concrete must be pumped to the bottom of the pile, which can be over 50 metres long. In my experience, the concrete must be a self-compacting mix with a maximum aggregate size of 10 mm, and the pumping pressure must be carefully controlled to avoid segregation. The literature should have discussed the welding of the two steel tubes to the end flanges or the transition piece, as this is a critical connection that must be fully welded and inspected. The welding of the outer tube to the transition piece, which connects the pile to the tower, is a full-penetration weld that must be performed with a qualified procedure and subjected to 100 percent ultrasonic testing. I have seen a case where a lack of fusion in this weld was only detected by a phased array ultrasonic test, and the repair took three weeks, delaying the installation by a significant margin.
Installation and Field Experience
The installation of a large-diameter hollow sandwich CFST pile is a major marine operation that requires a heavy-lift vessel with a crane capacity of at least 2000 tonnes. The pile is typically transported to the site in a horizontal position and then upended using a crane, which imposes significant bending stresses on the pile. The literature should have addressed the lifting points and the reinforcement of the pile to prevent local buckling during the upending operation. In my experience, the most critical phase is the hammering of the pile into the seabed, which subjects the pile to high-impact loads that can cause fatigue damage to the welds. The literature mentions the use of a hydraulic hammer, but it does not discuss the effect of the hammer energy on the pile's integrity. For a large-diameter pile, the hammer energy can be in the range of 2000 to 4000 kJ, and the stress waves generated by the hammer can cause a tensile stress at the pile tip, which can lead to a fracture if the pile has a pre-existing defect. I have witnessed a case where a pile with a small lack of fusion in a circumferential weld failed during driving, resulting in a complete separation of the pile. The only way to prevent this is to perform a rigorous NDT of all the welds before driving and to use a stress wave monitoring system during the driving operation.
Concluding Summary
The literature presents a valuable multi-objective optimisation framework for the design of hollow sandwich CFST piles for offshore wind, but it must be complemented by a thorough understanding of the manufacturing and installation constraints. The optimised dimensions are only useful if they can be fabricated and installed with a reasonable degree of confidence, and this requires a close collaboration between the design engineer and the fabrication shop. My experience tells me that the outer diameter is often limited by the installation vessel's capacity, and the concrete thickness is limited by the pumping pressure and the aggregate size. The optimisation should therefore include these practical constraints as design variables, not as fixed parameters. The fatigue performance of the welded connections is another critical issue that the literature does not fully address, as the fatigue life of the pile is often governed by the weld details at the transition piece and the internal stiffeners. I would recommend that any engineer using this optimisation approach validate the results with a full-scale prototype test, which is expensive but necessary to confirm the structural behaviour. The hollow sandwich CFST pile is a promising technology, but it is not a simple extension of the conventional monopile, and it requires a significant investment in research and development to bring it to a mature state.
Zhuojin Pipe Fitting Co., Ltd