Axial Compression Behaviour of Multi-Cavity Hollow Thin-Walled Square Steel Tube Concrete Short Columns: A Practical Review

Literature Overview and Scope

This paper presents an experimental and numerical investigation into the axial compression behaviour of multi-cavity hollow thin-walled square steel tube concrete short columns. The concept is a departure from the conventional concrete-filled steel tube (CFST) column, where the steel tube is filled entirely with concrete. In the multi-cavity design, the tube is divided into several cavities by internal partitions, and only some of the cavities are filled with concrete, leaving others hollow. This results in a column that is lighter than a fully filled CFST column, while retaining a high load-carrying capacity. The paper is a timely contribution to the field, as there is a growing interest in lightweight composite columns for high-rise buildings and long-span structures.

The authors conducted a series of axial compression tests on short columns with varying numbers of cavities, wall thicknesses, and concrete filling patterns. The test results were then used to validate a finite element model, which was employed for a parametric study to investigate the effects of the cavity arrangement, the wall thickness, and the concrete strength on the axial capacity and the failure mode. The key finding is that the multi-cavity column exhibits a higher axial capacity than a conventional CFST column of the same outer dimensions, due to the increased confinement provided by the internal partitions. The failure mode is characterised by local buckling of the steel tube, followed by crushing of the concrete, with the partitions acting as stiffeners that delay the onset of buckling.

Technical Points and Interpretation

Geometry and Cavity Arrangement

The multi-cavity column is fabricated by welding internal partitions to the inner faces of the square steel tube. The partitions can be arranged in a variety of patterns, including a single longitudinal partition, a cross partition, or a more complex grid. The paper focuses on columns with two, three, and four cavities, and the results show that the axial capacity increases with the number of cavities, but the rate of increase diminishes as the number of cavities grows. This is because the partitions are most effective when they are placed at the locations of maximum bending stress, which is at the mid-width of the column faces. The optimal arrangement is one that divides the column into four equal cavities, which provides the highest degree of confinement without adding excessive weight.

Local Buckling and Confinement

The primary failure mode observed in the tests is local buckling of the steel tube wall, which occurs at a load that is significantly higher than that of a conventional CFST column. The partitions act as rigid supports for the tube wall, reducing the effective buckling length and increasing the buckling stress. The concrete in the filled cavities provides lateral support to the tube wall, further delaying the onset of buckling. The result is a column that exhibits a more ductile failure mode, with a gradual loss of load capacity after the peak load, rather than a sudden and brittle failure. This is a desirable characteristic for a structural column, as it provides warning before failure and allows for redistribution of load in a structure.

Comparison with Conventional CFST Columns

The paper compares the performance of the multi-cavity column with that of a conventional CFST column of the same outer dimensions and steel wall thickness. The results show that the multi-cavity column has a higher axial capacity, a higher initial stiffness, and a more ductile failure mode. The improvement in axial capacity is attributed to the increased confinement of the concrete, which is provided by the partitions and the tube wall. The improvement in ductility is attributed to the delay in local buckling, which allows the column to undergo larger deformations before failure. These are significant advantages, but they come at the cost of increased fabrication complexity and a higher risk of welding defects in the partitions.

Integration with Manufacturing and Delivery Practice

Fabrication of the Multi-Cavity Tube

The fabrication of the multi-cavity tube is a challenging task that requires a high degree of precision. The partitions must be welded to the inner faces of the tube, and the welds must be of high quality to ensure that the partitions act as effective stiffeners. In my experience, the most common defect is a lack of fusion at the root of the weld, which can lead to a crack that propagates under load. This is a problem that can be avoided by using a qualified welding procedure and by performing a thorough inspection of the welds, including ultrasonic testing or radiography. The partitions should be cut from plate with a high degree of accuracy, and the edges should be prepared with a bevel to ensure full penetration. The tube itself should be manufactured from a high-quality steel plate, with a flatness tolerance that is tighter than that specified in ASTM A500 or EN 10219.

Concrete Filling and Quality Control

The concrete filling of the cavities is another area where quality control is critical. The concrete must be placed in a manner that ensures complete filling of the cavities, without voids or honeycombing. This is particularly difficult in a multi-cavity column, where the cavities are narrow and the access for the concrete is limited. I would recommend that the concrete be placed using a tremie pipe, and that the column be vibrated thoroughly to ensure that the concrete flows into all corners of the cavities. The strength of the concrete should be verified with test cubes, and the workability should be checked with a slump test. If the concrete is not placed correctly, the column will not achieve its design capacity, and the failure mode may change from a ductile buckling to a brittle crushing.

Delivery and Site Handling

The multi-cavity column is heavier and more complex than a conventional CFST column, and it requires careful handling during transport and installation. The partitions and the tube wall are relatively thin, and they can be damaged by impact or by improper lifting. I would recommend that the columns be lifted using a spreader beam, and that the lifting points be located at the positions of the partitions, to avoid bending the tube wall. The columns should be stored on a flat surface, with the ends protected from damage. The concrete filling should be carried out on site, as the column would be too heavy to transport if it were filled at the factory. This means that the site crew must be trained in the correct placement of the concrete, and the quality control procedures must be followed strictly.

Key Questions and Reflections

One of the questions that the paper does not address is the long-term behaviour of the multi-cavity column under sustained load. The concrete will creep and shrink over time, and this will lead to a redistribution of load between the steel and the concrete. This is a phenomenon that is well understood for conventional CFST columns, but it is not clear how the presence of the partitions affects the creep and shrinkage behaviour. I would encourage the authors to extend their work to include a long-term test, or at least a numerical model that accounts for the time-dependent behaviour of the concrete. Another question is the behaviour of the column under fire, which is not covered in the paper. The concrete in the filled cavities will provide some fire protection to the steel tube, but the hollow cavities will allow the heat to penetrate more deeply into the column. This is a topic that deserves further research, as it is a critical consideration for the design of columns in high-rise buildings.

Study Insights and Implications

The paper provides a valuable contribution to the understanding of multi-cavity hollow thin-walled square steel tube concrete columns. The experimental results are well supported by the finite element model, and the parametric study provides useful design guidance. From a manufacturing and delivery perspective, the key takeaway is that the multi-cavity column is a viable alternative to the conventional CFST column, but it requires a higher level of fabrication quality and a more careful site installation. The partitions are the critical component, and they must be welded with a high degree of quality to ensure that they act as effective stiffeners. The concrete filling must be carried out with care, and the quality control procedures must be followed strictly to avoid voids and honeycombing.

Reference Value and Outlook

The paper is a useful reference for engineers who are designing lightweight composite columns for high-rise buildings and long-span structures. It provides a clear framework for the design of the multi-cavity column, and it offers a numerical model that can be used to verify the performance of a specific column configuration. The findings are also relevant to the broader field of composite structures, where the use of internal partitions is a relatively new concept. I would recommend that the authors extend their work to include a full-scale test of the column under combined axial and bending load, as the behaviour of the column under eccentric loading is not well understood. The next step should be the development of a design formula that accounts for the effects of the cavity arrangement, the wall thickness, and the concrete strength on the axial capacity.

In conclusion, this paper is a welcome addition to the literature on composite columns. It addresses a practical problem with a rigorous experimental and numerical approach, and it offers conclusions that are directly applicable to the design and fabrication of these columns. The insights that I have drawn from the paper, combined with my own experience in the field, lead me to the view that the multi-cavity column is a promising alternative to the conventional CFST column, provided that the fabrication and installation are carried out to a high standard. I would recommend this paper to any engineer who is involved in the design of composite columns, and I would encourage the authors to continue their work with long-term tests and fire tests.